Abstract:
An object of the present invention is to provide an active energy ray-curable composition capable of forming a cured product excellent in damage restoration, adhesion to a plastic base, and transparency after curing. An active energy ray-curable composition for optical components of the present invention essentially includes: a monomer (A) having 2 or more radical-polymerizable reactive groups (x1), a homopolymer of the monomer (A) having a glass transition temperature of higher than 200° C.; a monomer (C) having 2 or more radical-polymerizable reactive groups (x2), a homopolymer of the monomer (C) having a glass transition temperature of lower than −15° C.; and a photopolymerization initiator (E).
Abstract:
The present invention provides an active energy ray-curable resin composition containing: (A) a monofunctional ethylenically unsaturated monomer free of urethane groups; (B) a polyfunctional ethylenically unsaturated monomer free of urethane groups; (C) a urethane group-containing ethylenically unsaturated monomer; (D) a photopolymerization initiator; (E) a polymerization inhibitor; and (F) a surfactant, wherein relative to the total weight of (A), (B), (C), (D), (E), and (F), the weight ratio of (A) is 45 to 90% by weight, the weight ratio of (B) is 3 to 25% by weight, the weight ratio of (C) is 3 to 35% by weight, the weight ratio of (D) is 0.1 to 10% by weight, the weight ratio of (E) is 0.01 to 5% by weight, and the weight ratio of (F) is 0.1 to 10% by weight, and the resin composition has a surface tension of 20 to 30 mN/m.
Abstract:
The present invention aims to provide a viscosity index improver composition and a lubricating oil composition having a low HTHS viscosity at 100° C., an excellent shear stability, and an excellent low temperature viscosity. The present invention relates to, for example, a viscosity index improver composition (C), containing: a copolymer (A) containing a polyolefin-based monomer (a) represented by the following formula (1) as a constituent monomer; a copolymer (B) containing a (meth)acrylic acid alkyl ester (c) having a C12-C15 straight-chain or branched alkyl group and a (meth)acrylic acid alkyl ester (d) having a C16-C20 straight-chain or branched alkyl group as constituent monomers; and a base oil, wherein a weight average molecular weight ratio {(A)/(B)} of the copolymer (A) to the copolymer (B) is 2 to 55, and a weight ratio (A/B) of the copolymer (A) to the copolymer (B) constituting the viscosity index improver composition (C) is 5 to 100: