公开(公告)号:US20210309046A1
公开(公告)日:2021-10-07
申请号:US17343750
申请日:2021-06-10
申请人: FUJIFILM CORPORATION
发明人: Takeshi HAMA , Yuichi HAYATA , Makoto ISHIGURO
摘要: In one embodiment, a method for manufacturing a decorative film for molding and a molding method include, in the following order, forming, on a base material, a liquid crystal layer including a cholesteric liquid crystal compound and a photoisomerization compound, photoisomerizing the liquid crystal layer, and curing the liquid crystal layer. In one embodiment, a decorative film for molding includes, on a base material, a liquid crystal layer including a cholesteric liquid crystal compound and a photoisomerization compound, in which the cured liquid crystal layer has a plurality of regions which are different from each other in terms of a photoisomerization proportion of the photoisomerization compound. A molded product using the decorative film for molding, an automobile exterior plate, and an electronic device are also provided.
-
公开(公告)号:US20190264065A1
公开(公告)日:2019-08-29
申请号:US16406009
申请日:2019-05-08
申请人: FUJIFILM CORPORATION
发明人: Naoki KOITO , Aki NAKAMICHI , Takeshi HAMA , Yusuke HATANAKA
IPC分类号: C09D183/04 , C09D7/61 , C03C17/00 , C03C17/30
摘要: Provided are a laminate including a base material, and an anti-fogging layer provided on at least a part of the base material, in which the anti-fogging layer contains a siloxane binder, silica particles, and a water absorption organic polymer, a water absorption amount of the anti-fogging layer is in a range of 1.5 mg/cm2 to 25.0 mg/cm2, a water contact angle of a surface of the anti-fogging layer is in a range of 1° to 20°, and a film thickness of the anti-fogging layer is more than 1 μm and 10 μm or less; a method of producing the same; and an anti-fogging coating composition which is suitably used for formation of the anti-fogging layer.
-
公开(公告)号:US20240301470A1
公开(公告)日:2024-09-12
申请号:US18673493
申请日:2024-05-24
申请人: FUJIFILM Corporation
发明人: Takeshi HAMA
IPC分类号: C12Q1/6809 , B01L3/00 , C12N15/10 , C12Q1/686
CPC分类号: C12Q1/6809 , B01L3/502753 , C12N15/1017 , C12Q1/686 , B01L2200/16 , B01L2300/042 , B01L2300/047 , B01L2300/0663 , B01L2300/0681 , B01L2300/0816 , B01L2300/0877 , B01L2400/0487
摘要: The nucleic acid examination method includes an extraction step of extracting a nucleic acid from a specimen, a purification step of removing impurities in a liquid of any of a solution containing the specimen or a nucleic acid extraction liquid from which the nucleic acid has been extracted, at any stage before, during, or after the extraction step, an amplification step of amplifying a base sequence in the nucleic acid extraction liquid, a detection step of detecting presence or absence of the base sequence after the amplification step. The extraction step is a step of bringing the specimen into contact with an extraction reagent containing a nonionic surfactant, and the purification step includes an adsorption step of bringing a liquid into contact with a zeolite having any crystal structure of a ferrierite, a mordenite, an L-type, or a Y-type, to adsorb impurities in the liquid to the zeolite.
-
公开(公告)号:US20210170394A1
公开(公告)日:2021-06-10
申请号:US17074009
申请日:2020-10-19
申请人: FUJIFILM Corporation
发明人: Takeshi HAMA , Noboru KOMORI , Yuki INOUE , Aya OUCHI
IPC分类号: B01L3/00 , G01N33/543
摘要: Provided is a liquid feeding device, including: a test container including a first accommodation portion, a second accommodation portion, and a third accommodation portion each accommodating a liquid, a first flow path connecting the first accommodation portion and the second accommodation portion to each other at respective upper end positions thereof, and a second flow path connecting the second accommodation portion and the third accommodation portion to each other at respective upper end positions thereof, in which at least a portion forming an upper wall surface of the second accommodation portion has flexibility; and a pressing machine which includes a first pressing portion and presses the portion forming the upper wall surface of the second accommodation portion at a position closer to the first flow path from a center in a liquid feeding direction towards an inside of the second accommodation portion from an outside by the pressing portion, in which the liquid accommodated in the second accommodation portion is fed to the third accommodation portion by pressing the portion forming the upper wall surface of the second accommodation portion with the pressing machine.
-
公开(公告)号:US20210070022A1
公开(公告)日:2021-03-11
申请号:US16953342
申请日:2020-11-20
申请人: FUJIFILM CORPORATION
发明人: Takashi ARIDOMI , Takeshi HAMA , Shinichi KANNA , Yujiro YANAI , Yuichi HAYATA
IPC分类号: B32B27/08 , B32B27/20 , B32B27/30 , B32B27/36 , B32B27/40 , B32B7/023 , C09J7/38 , C08K3/04 , C08K7/26 , C08K3/36
摘要: Provided are a decorative film including, in the following order, a temporary support, a colored layer, a cholesteric liquid crystal layer, and a protective layer, in which the decorative film is a film for viewing the colored layer through the cholesteric liquid crystal layer; a decoration method or a method for manufacturing a decorative molded article; and a decorative molded film including, in the following order, a base material, a colored layer, a cholesteric liquid crystal layer, and a protective layer, or including, in the following order, a colored layer, a cholesteric liquid crystal layer, a base material, and a protective layer, in which the decorative molded film is a film for viewing the colored layer through the cholesteric liquid crystal layer.
-
6.
公开(公告)号:US20210269563A1
公开(公告)日:2021-09-02
申请号:US17322821
申请日:2021-05-17
申请人: FUJIFILM CORPORATION
发明人: Yuichi HAYATA , Takeshi HAMA , Nobuhiko ICHIHARA , Yujiro YANAI
摘要: Provided are a decorative film for molding including a cholesteric liquid crystal layer on a base material, in which the cholesteric liquid crystal layer is a layer formed by curing a liquid crystal composition which includes, with respect to a total solid content of the liquid crystal composition, 25% by mass or more of a cholesteric liquid crystal compound having one ethylenic unsaturated group or one cyclic ether group; a molded product using the decorative film for molding; and a molding method.
-
公开(公告)号:US20210170404A1
公开(公告)日:2021-06-10
申请号:US16950434
申请日:2020-11-17
申请人: FUJIFILM Corporation
发明人: Takeshi HAMA , Noboru KOMORI , Yuki INOUE , Aya OUCHI
IPC分类号: B01L3/00 , G01N33/543
摘要: A test container including: at least two accommodation portions each accommodating a liquid and internally provided; a flow path connecting the two accommodation portions to each other at respective upper end positions thereof internally provided; and a flexible film deformable inwards of at least one accommodation portion at a portion forming an upper wall surface of the one accommodation portion, in which the liquid accommodated in the one accommodation portion is fed to the other accommodation portion via the flow path due to deformation of the flexible film towards the one accommodation portion, and a breaking elongation of the flexible film is 100% or more and 600% or less.
-
公开(公告)号:US20210170392A1
公开(公告)日:2021-06-10
申请号:US16952198
申请日:2020-11-19
申请人: FUJIFILM Corporation
发明人: Takeshi HAMA , Noboru KOMORI , Yuki INOUE , Aya OUCHI
IPC分类号: B01L3/00
摘要: A test container includes a container main body including a first-accommodation-portion, a second-accommodation-portion, and a third-accommodation-portion each accommodating a liquid and internally provided, a first flow path connecting the first-accommodation-portion and the second-accommodation-portion to each other at respective upper end positions thereof and internally provided, and a second flow path connecting the second-accommodation-portion and the third-accommodation-portion to each other at respective upper end positions thereof and internally provided, in which at least a portion forming an upper wall surface of the second-accommodation-portion has flexibility to be deformable inwards of the second-accommodation-portion; and a liquid return prevention structure which prevents a backflow of the liquid to the first-accommodation-portion, when the liquid accommodated in the second-accommodation-portion is fed to the third-accommodation-portion via the second flow path due to deformation of the portion forming the upper wall surface of the second-accommodation-portion inwards of the second-accommodation-portion.
-
公开(公告)号:US20190100674A1
公开(公告)日:2019-04-04
申请号:US16205249
申请日:2018-11-30
申请人: FUJIFILM CORPORATION
发明人: Takeshi HAMA , Yusuke HATANAKA , Naoki KOITO , AKi NAKAMICHI
IPC分类号: C09D133/02 , C09D175/04 , C09D5/24
摘要: Provided are a film-forming composition containing a hydrolysate of a siloxane compound represented by Formula (1), silica particles, a ketone-based solvent, and water, and a manufacturing method of a laminate. In Formula (1), R1, R2, R3, and R4 each independently represent a monovalent organic group having 1 to 6 carbon atoms. represents an integer of 2 to 20.
-
公开(公告)号:US20160170192A1
公开(公告)日:2016-06-16
申请号:US15052331
申请日:2016-02-24
申请人: FUJIFILM Corporation
发明人: Yuya YAMAMOTO , Takeshi HAMA
CPC分类号: G02B19/0042 , B32B7/02 , B32B15/08 , B32B15/082 , B32B15/09 , B32B15/095 , B32B27/06 , B32B27/18 , B32B27/20 , B32B27/26 , B32B27/30 , B32B27/36 , B32B2255/00 , B32B2255/06 , B32B2255/10 , B32B2255/24 , B32B2255/26 , B32B2307/00 , B32B2307/40 , B32B2307/4026 , B32B2307/416 , B32B2307/536 , B32B2307/554 , B32B2307/584 , B32B2307/71 , B32B2307/712 , B32B2307/728 , B32B2307/754 , B32B2307/762 , B32B2551/00 , B32B2551/08 , B32B2605/006 , C08J7/045 , C08J2367/02 , C08J2405/16 , C08J2433/04 , C08J2475/14 , C09D133/02 , C09D133/14 , G02B1/14 , G02B1/18 , G02B5/08 , G02B5/0808 , G02B5/208 , G02B19/0019 , H02S40/22 , Y02E10/52
摘要: An object of the invention is to provide a composite film and a film mirror for solar light reflection, to which dust and the like is not likely to adhere, of which resistance to scratch due to dust and the like is excellent, and in which cleaning properties of adhered dust and the like are excellent. The composite film according to the invention includes a composite film having a support and a surface covering layer, in which an elastic recovery rate of the surface covering layer is 60% or greater, a surface hardness thereof is 100 N/mm2 or less, and a water contact angle of a surface thereof is 40° or less.