摘要:
The invention provides a stock oil composition for needle coke for a graphite electrode, the stock oil composition having a 10 vol % distillation temperature of 280° C. or higher as the distillation property, and when separated into the aromatic component and non-aromatic component by elution chromatography, having an aromatic component content of 30-80 wt % with respect to the total weight of the stock oil composition and an aromatic component molecular weight of 255-1300, as well as a non-aromatic component normal paraffin content of at least 5 parts by weight with respect to 100 parts by weight of the aromatic component.
摘要:
The present invention provides feedstock compositions for use of the production of an activated carbon for electric double layer capacitor electrodes or the production of needle coke, comprising a first heavy oil with an initial boiling point of 300° C. or higher, an asphalten content of 12 percent by mass or less, a saturate content of 50 percent by mass or more and a sulfur content of 0.3 percent by mass or less, produced as a residue resulting from vacuum-distillation of a petroleum-based oil and a second heavy oil with an initial boiling point of 150° C. or higher and a sulfur content of 0.5 percent by mass or less, produced by subjecting a hydrocarbon oil to fluidized catalytic cracking.
摘要:
The present invention provides a raw coke having such a structure that the graphitized product resulting from graphitization of the raw coke at a temperature of 2800° C. under an inactive gas atmosphere will have ratios of the crystallite size to the lattice constant of 360 or less in the (002) plane and 1500 or less in the (110) plane, as a raw coke providing active carbon produced by alkali-activating the raw coke, which is reduced in remaining alkali content and can simplify washing operation because washing liquid can easily pass through the activated carbon, or as a raw coke for the production of needle coke.
摘要:
The present invention provides a method of regenerating an oil adsorbent, wherein an oil adsorbent even if containing a large amount of oil can be regenerated without taking it out from the facility. The method of regenerating an oil adsorbent comprises washing a carbonaceous oil adsorbent made from calcined coke, with oil adsorbed thereon, with warm water of 40° C. or higher or gas-bubbled warm water of 40° C. or higher.
摘要:
A raw material composite 10 for a carbon material used in an electric double layer capacitor contains microcrystalline carbon having a layered crystal structure similar to graphite, and is formed a carbon material for an electric double layer capacitor by undergoing an activation treatment. Here, the raw material composite is characterized in that a Hardgrove grindability index HGI defined by ASTMD-409-71 is 50 or above, an interlayer distance d002 of the microcrystalline carbon determined by an X-ray diffraction method is 0.343 NM or below, and a crystallite size Lc002 of the microcrystalline carbon determined by the X-ray diffraction method is 3.0 nm or below.
摘要:
In the raw coke composition of the invention, as the starting material for a negative electrode material of a lithium ion secondary battery, the ratio of the crystallite size Lc(002) and lattice constant co(002) (Lc(002)/co(002)) on the 002 plane is no greater than 180, and the ratio of the crystallite size La(110) and the lattice constant ao(110) (La(110)/ao(110)) on the 110 plane is no greater than 1500, as determined by X-ray diffraction upon graphitizing in an inert gas atmosphere at a temperature of 2800° C.
摘要:
The present invention provides a raw coke having such a structure that the graphitized product resulting from graphitization of the raw coke at a temperature of 2800° C. under an inactive gas atmosphere will have ratios of the crystallite size to the lattice constant of 360 or less in the (002) plane and 1500 or less in the (110) plane, as a raw coke providing active carbon produced by alkali-activating the raw coke, which is reduced in remaining alkali content and can simplify washing operation because washing liquid can easily pass through the activated carbon, or as a raw coke for the production of needle coke.
摘要:
The amorphous carbon material for the negative electrode of a lithium ion secondary battery of the invention has a true density of 1.800-2.165 g/cm3, but has a true density of 2.255 g/cm3 or greater when subjected to graphitizing in an inert gas atmosphere at a temperature of 3000° C.
摘要翻译:本发明的锂离子二次电池用负极的无定形碳材料的真密度为1.800-2.165g / cm 3,当在惰性气体气氛中进行石墨化时,其真密度为2.255g / cm 3以上 在3000℃的温度下
摘要:
A process is provided for producing petroleum coke that is high in strength and sufficiently small in thermal expansion coefficient and sufficiently suppressed from puffing. The process includes coking a feedstock containing a first heavy oil having a sulfur content of 1.0 percent by mass or less, a nitrogen content of 0.5 percent by mass or less, and an aromatic index of 0.1 or greater, produced by hydrodesulfurizing a heavy oil with a sulfur content of 1 percent by mass or more under conditions (1) where the total pressure is 10 MPa or greater and less than 16 MPa and the hydrogen partial pressure is 5 MPa or greater and 16 MPa or less or conditions (2) where the total pressure is 20 MPa or greater and 25 MPa or less and the hydrogen partial pressure is greater than 20 MPa and 25 MPa or less, and a second heavy oil with an aromatic index of 0.3 or greater and an initial boiling point of 150° C. or higher.
摘要:
In the raw coke composition of the invention, as the starting material for a negative electrode material of a lithium ion secondary battery, the ratio of the crystallite size Lc(002) and lattice constant co(002) (Lc(002)/co(002)) on the 002 face is no greater than 180, and the ratio of the crystallite size La(110) and the lattice constant ao(110) (La(110)/ao(110)) on the 110 face is no greater than 1500, as determined by X-ray diffraction upon graphitizing in an inert gas atmosphere at a temperature of 2800° C.