LITHIUM TITANATE AND PRODUCTION METHOD AND USE FOR SAME
    4.
    发明申请
    LITHIUM TITANATE AND PRODUCTION METHOD AND USE FOR SAME 审中-公开
    钛酸锂和生产方法和用途

    公开(公告)号:US20150044568A1

    公开(公告)日:2015-02-12

    申请号:US14385514

    申请日:2013-03-14

    申请人: TAYCA CORPORATION

    IPC分类号: H01M4/485 C01G23/00

    摘要: A method for manufacturing lithium titanate (Li4Ti5O12) of a substantially single phase, which is excellent in rate performance, and can be easily handled. The lithium titanate (Li4Ti5O12) is prepared from substantially a raw material powder consisting of a lithium compound and a raw material powder consisting of a titanic acid compound which are mixed and the resultant mixture is calcined. A lithium carbonate is used as the lithium compound and metatitanic acid or orthotitanic acid is used as the titanic acid compound. The penetration speed coefficient of the lithium titanate obtained, to a nonaqueous electrolyte is larger than a penetration speed coefficient of lithium titanate, obtained by using a lithium hydroxide as the lithium compound, to the same nonaqueous electrolyte. The specific surface area of the lithium titanate obtained is 10 m2/g or less.

    摘要翻译: 一种制造基本上单相的钛酸锂(Li 4 Ti 5 O 12)的方法,其性能优异,并且可以容易地处理。 钛酸锂(Li 4 Ti 5 O 12)由基本上由锂化合物组成的原料粉末和由混合的钛酸化合物组成的原料粉末制成,并将所得混合物煅烧。 使用碳酸锂作为锂化合物,将偏钛酸或原钛酸用作钛酸化合物。 对于非水电解质,得到的钛酸锂的渗透速度系数大于通过使用氢氧化锂作为锂化合物而获得的钛酸锂的渗透速度系数与相同的非水电解质。 所得钛酸锂的比表面积为10m 2 / g以下。