摘要:
A baking-type aqueous organic silicon fluorine-containing polymer paint is provided, which includes an aqueous organic silicon fluorine-containing polymer dispersion and a curing agent. The curing agent includes aqueous amino resin, aqueous isocyanate resin, or a combination thereof. In addition, the paint may further include an assist resin such as aqueous polyester resin, aqueous acrylic acid resin, aqueous epoxy resin, aqueous phenoxy resin, or a combination thereof.
摘要:
Polyphenylene ether resin composition includes 100 parts by weight of polyphenylene ether resin, 25 to 40 parts by weight of copolymer, and 0.01 to 0.02 parts by weight of initiator. The copolymer is (A) copolymer polymerized of (a) mono-functional monomer, (b1) bi-functional monomer, and (c) tri-functional monomer through radical polymerization, (B) copolymer polymerized of (a) mono-functional monomer and (b2) bi-functional monomer through radical polymerization, or (C) a combination thereof.
摘要:
A method of manufacturing a coating is provided, which includes applying a primer paint on a substrate, wherein the primer paint includes 100 parts by weight of a first PVF, 30-70 parts by weight of an assistance resin, 5-30 parts by weight of a curing agent, 100-120 parts by weight of a first latent solvent, 3-methoxy-3-methyl-1-butanol, and water. The first latent solvent, 3-methoxy-3-methyl-1-butanol, and water have a weight ratio of 60:10-20:40-60. The method also applies a finish paint on the primer paint, wherein the finish paint includes 100 parts by weight of a second PVF, 100-120 parts by weight of a second latent solvent, 3-methoxy-3-methyl-1-butanol, and water, wherein the second latent solvent, 3-methoxy-3-methyl-1-butanol, and water have a weight ratio of 50:10-20:30-60. The primer paint and the finish paint are baked and dried to form a coating.
摘要:
Disclosed is a method of forming a composite micropowder, including mixing 100 parts by weight of fluorine-containing polymer, 10 to 140 parts by weight of silane, catalyst, and water, such that the silane is in-situ polymerized in the fluorine-containing polymer to form a polysiloxane, and the fluorine-containing polymer and the polysiloxane form a composite. The composite is dried, and then physically crushed to form composite micropowder. The total weight of the fluorine-containing polymer and the silane and the weight of the catalyst have a ratio of 100:1 to 100:0.0001. The silane and the water have a molar ratio of 1:0.5 to 1:3. The composite micropowder has a diameter of 0.1 μm to 15 μm. The fluorine-containing polymer and the polysiloxane in the composite micropowder have a weight ratio of 95:5 to 60:40.
摘要:
Polyphenylene ether resin composition includes 100 parts by weight of polyphenylene ether resin, 25 to 40 parts by weight of copolymer, and 0.01 to 0.02 parts by weight of initiator. The copolymer is (A) copolymer polymerized of (a) mono-functional monomer, (b1) bi-functional monomer, and (c) tri-functional monomer through radical polymerization, (B) copolymer polymerized of (a) mono-functional monomer and (b2) bi-functional monomer through radical polymerization, or (C) a combination thereof.
摘要:
A method of manufacturing a coating is provided, which includes applying a primer paint on a substrate, wherein the primer paint includes 100 parts by weight of a first PVF, 30-70 parts by weight of an assistance resin, 5-30 parts by weight of a curing agent, 100-120 parts by weight of a first latent solvent, 3-methoxy-3-methyl-1-butanol, and water. The first latent solvent, 3-methoxy-3-methyl-1-butanol, and water have a weight ratio of 60:10-20:40-60. The method also applies a finish paint on the primer paint, wherein the finish paint includes 100 parts by weight of a second PVF, 100-120 parts by weight of a second latent solvent, 3-methoxy-3-methyl-1-butanol, and water, wherein the second latent solvent, 3-methoxy-3-methyl-1-butanol, and water have a weight ratio of 50:10-20:30-60. The primer paint and the finish paint are baked and dried to form a coating.
摘要:
A method of manufacturing a bi-layered coating is provided, which includes applying a primer paint on a substrate, wherein the primer paint includes 100 parts by weight of a first polyvinyl fluoride, 20 to 50 parts by weight of an assistance resin, and 150 to 170 parts by weight of a first latent solvent, and wherein the assistance resin is polyester modified epoxy resin, polyester type polyurethane resin, phenoxy resin, or a combination thereof. The primer paint is baked and dried to form a primer coating. A finish paint is then applied onto the primer coating, wherein the finish paint includes 100 parts by weight of a second polyvinyl fluoride and 120 to 150 parts by weight of a second latent solvent. The finish paint is baked and dried to form a finish coating on the primer coating.
摘要:
A method of manufacturing a bi-layered coating is provided, which includes applying a primer paint on a substrate, wherein the primer paint includes 100 parts by weight of a first polyvinyl fluoride, 20 to 50 parts by weight of an assistance resin, and 150 to 170 parts by weight of a first latent solvent, and wherein the assistance resin is polyester modified epoxy resin, polyester type polyurethane resin, phenoxy resin, or a combination thereof. The primer paint is baked and dried to form a primer coating. A finish paint is then applied onto the primer coating, wherein the finish paint includes 100 parts by weight of a second polyvinyl fluoride and 120 to 150 parts by weight of a second latent solvent. The finish paint is baked and dried to form a finish coating on the primer coating.
摘要:
A baking-type aqueous organic silicon fluorine-containing polymer paint is provided, which includes an aqueous organic silicon fluorine-containing polymer dispersion and a curing agent. The curing agent includes aqueous amino resin, aqueous isocyanate resin, or a combination thereof. In addition, the paint may further include an assist resin such as aqueous polyester resin, aqueous acrylic acid resin, aqueous epoxy resin, aqueous phenoxy resin, or a combination thereof.
摘要:
A ceramic paint is provided, which includes a mixture of a silica sol-gel, 20 to 60 parts by weight of filler, and 1 to 50 parts by weight of a fluorine-containing polymer, wherein the silica sol-gel is formed by reacting 100 parts by weight of silica sol, 50 to 100 parts by weight of organic silane, and 0.3 to 1 parts by weight of a catalyst.