摘要:
This high-strength steel sheet includes by mass percentage: 0.05 to 0.4% of C; 0.1 to 2.5% of Si; 1.0 to 3.5% of Mn; 0.001 to 0.03% of P; 0.0001 to 0.01% of S; 0.001 to 2.5% of Al; 0.0001 to 0.01% of N; 0.0001 to 0.008% of O; and a remainder composed of iron and inevitable impurities, wherein a steel sheet structure contains by volume fraction 10 to 50% of a ferrite phase, 10 to 50% of a tempered martensite phase, and a remaining hard phase, wherein a 98% hardness is 1.5 or more times as high as a 2% hardness in a range from ⅛ to ⅜ of a thickness of the steel sheet, wherein a kurtosis K* of the hardness distribution between the 2% hardness and the 98% hardness is −1.2 to −0.4, and wherein an average crystal grain size in the steel sheet structure is 10 μm or less.
摘要:
A high-strength cold-rolled steel sheet includes, by mass %, C: 0.10% to 0.40%, Mn: 0.5% to 4.0%, Si: 0.005% to 2.5%, Al: 0.005% to 2.5%, Cr: 0% to 1.0%, and a balance of iron and inevitable impurities, in which an amount of P is limited to 0.05% or less, an amount of S is limited to 0.02% or less, an amount of N is limited to 0.006% or less, the microstructure includes 2% to 30% of retained austenite by area percentage, martensite is limited to 20% or less by area percentage in the microstructure, an average particle size of cementite is 0.01 μm to 1 μm, and 30% to 100% of the cementite has an aspect ratio of 1 to 3.
摘要:
A steel sheet, including: as chemical components, by mass %, 0.05% to 0.35% of C; 0.05% to 2.0% of Si; 0.8% to 3.0% of Mn; 0.01% to 2.0% of Al; equal to or less than 0.1% of P; equal to or less than 0.05% of S; equal to or less than 0.01% of N; and the balance including iron and inevitable impurities, wherein an area ratio of equal to or higher than 50% of a total of a ferrite phase, a bainite phase, and a tempered martensite phase is contained, an area ratio of equal to or higher than 3% of a retained austenite phase is contained, and crystal grains of the retained austenite phase having a number ratio of equal to or higher than 50% satisfy Expression 1, assuming carbon concentration at a position of center of gravity is Cgc and a carbon concentration at a grain boundary is Cgb.
摘要:
A steel sheet, including: as chemical components, by mass %, 0.05% to 0.35% of C; 0.05% to 2.0% of Si; 0.8% to 3.0% of Mn; 0.01% to 2.0% of Al; equal to or less than 0.1% of P; equal to or less than 0.05% of S; equal to or less than 0.01% of N; and the balance including iron and inevitable impurities, wherein the steel sheet comprises 50% or more of a ferrite phase, a bainite phase, and a tempered martensite phase, 3% or more of a retained austenite phase, and 50% or more of the crystal grains of the retained austenite phase satisfy Expression 1, wherein a carbon concentration at a position of center of gravity is Cgc and a carbon concentration at a grain boundary is Cgb.
摘要:
The present invention provides a high-strength steel sheet excellent in impact resistance. The high-strength steel sheet contains predetermined contents of C, Si, Mn, P, S, Al, Ti, N, and O, with the balance being iron and inevitable impurities, and has a steel sheet structure in which, in a ⅛ thickness to ⅜ thickness region across ¼ of a sheet thickness, 1 to 8% retained austenite is contained in volume fraction, an average aspect ratio of the retained austenite is 2.0 or less, an amount of solid-solution Mn in the retained austenite is 1.1 times an average amount of Mn or more, and TiN grains having a 0.5 μm average grain diameter or less are contained, and a density of AlN grains with a 1 μm grain diameter or more is 1.0 pieces/mm2 or less, wherein a maximum tensile strength is 900 MPa or more.
摘要:
[Summary] The present invention provides a high-strength steel sheet excellent in impact resistance. The high-strength steel sheet contains predetermined contents of C, Si, Mn, P, S, Al, Ti, N, and O, with the balance being iron and inevitable impurities, and has a steel sheet structure in which, in a ⅛ thickness to ⅜ thickness region across ¼ of a sheet thickness, 1 to 8% retained austenite is contained in volume fraction, an average aspect ratio of the retained austenite is 2.0 or less, an amount of solid-solution Mn in the retained austenite is 1.1 times an average amount of Mn or more, and TiN grains having a 0.5 μm average grain diameter or less are contained, and a density of AlN grains with a 1 μm grain diameter or more is 1.0 pieces/mm2 or less, wherein a maximum tensile strength is 900 MPa or more.
摘要翻译:发明内容本发明提供耐冲击性优异的高强度钢板。 高强度钢板含有预定含量的C,Si,Mn,P,S,Al,Ti,N和O,余量为铁和不可避免的杂质,并且具有钢板结构,其中在 厚度为⅜厚度区域,1/4的残留奥氏体含量为1〜8%,残留奥氏体的平均纵横比为2.0以下,残留奥氏体中的固溶Mn量为1.1 的平均粒径Mn以上,并且含有0.5μm平均粒径以下的TiN粒子,1μm以上的AlN粒子的密度为1.0个/ mm 2以下,其中,最大拉伸强度 强度为900MPa以上。
摘要:
This high-strength steel sheet includes by mass percentage: 0.05 to 0.4% of C; 0.1 to 2.5% of Si; 1.0 to 3.5% of Mn; 0.001 to 0.03% of P; 0.0001 to 0.01% of S; 0.001 to 2.5% of Al; 0.0001 to 0.01% of N; 0.0001 to 0.008% of O; and a remainder composed of iron and inevitable impurities, wherein a steel sheet structure contains by volume fraction 10 to 50% of a ferrite phase, 10 to 50% of a tempered martensite phase, and a remaining hard phase, wherein a 98% hardness is 1.5 or more times as high as a 2% hardness in a range from ⅛ to ⅜ of a thickness of the steel sheet, wherein a kurtosis K* of the hardness distribution between the 2% hardness and the 98% hardness is −1.2 to −0.4, and wherein an average crystal grain size in the steel sheet structure is 10 μm or less.
摘要:
High strength steel plate with an ultimate tensile strength of 900 MPa or more which is excellent in hydrogen embrittlement resistance characterized in that, in the structure of the steel plate, (a) by volume fraction, ferrite is present in 10 to 50%, bainitic ferrite and/or bainite in 10 to 60%, and tempered martensite in 10 to 50%, and (b) iron-based carbides which contain Si or Si and Al in 0.1% or more are present in 4×108 (particles/mm3) or more.
摘要:
A high-strength cold-rolled steel sheet includes, by mass %, C: 0.10% to 0.40%, Mn: 0.5% to 4.0%, Si: 0.005% to 2.5%, Al: 0.005% to 2.5%, Cr: 0% to 1.0%, and a balance of iron and inevitable impurities, in which an amount of P is limited to 0.05% or less, an amount of S is limited to 0.02% or less, an amount of N is limited to 0.006% or less, the microstructure includes 2% to 30% of retained austenite by area percentage, martensite is limited to 20% or less by area percentage in the microstructure, an average particle size of cementite is 0.01 μm to 1 μm, and 30% to 100% of the cementite has an aspect ratio of 1 to 3.
摘要:
Disclosed is a hot-rolled steel sheet including, by mass %, C:0.02% to 0.5% of C, and the sum of the content of Si and the content of Al is 1.0% to 4.0%. An average pole density of an orientation group from {100} to {223} is 1.0 to 6.5, and a pole density of a crystal orientation {332} is 1.0 to 5.0. A microstructure includes, by of an area ratio, 2% to 30% of retained austenite, 20% to 50% of ferrite, and 10% to 60% of bainite. rC that is a Lankford value in a direction orthogonal to a rolling direction is 0.70 to 1.10, and r30 that is a Lankford value in a direction forming an angle of 30° with the rolling direction is 0.70 to 1.10.