摘要:
The present invention relates to an equipment and method for producing polymer pellets which comprise one or more polymer components and one or more further components, wherein in said process at least one of said one or more further components is incorporated into pellets by applying a liquid, which comprises said at least one component, onto said pellets.
摘要:
The present invention relates to a structure comprising (i) a layer or profile (A) composed of a first material, and (ii) a polyolefin layer or profile (B) adjacent to layer or profile (A) which is composed of a composition comprising a base resin comprising a polyolefin, characterized in that the surface of any or both of layer or profile (A) and layer or profile (B) has/have been treated with a composition comprising an organosilicon compound before (A) and (B) are brought adjacent to each other, to a process for the production of such a structure, to an article, in particular a coated pipe, comprising such a structure and to the use of a composition comprising an organosilicon compound as an adhesion promoter in such a structure.
摘要:
The present invention relates to crosslinkable polymer composition, comprising an unsaturated polyolefin having a total amount of carbon-carbon double bonds/1000 carbon atoms of at least 0.1, at least one scorch retarder, and at least one crosslinking agent.
摘要:
The present invention relates to a polyolefin composition comprising a polyolefin base resin and an antioxidant, characterized in that said polyolefin composition has a lifetime of at least 200 h in a test measuring the resistance against ClO2-containing water at 90° C. and at a concentration of ClO2 of 4 ppm wherein the equipment used is according to ASTM F2263-03.The present invention further relates to a pipe comprising the polyolefin composition according to the invention, to the use of the polyolefin composition for the production of a pipe, and to the use of a particularly selected antioxidant for increasing the resistance of a polyolefin composition against degradation caused by contact with ClO2-containing water.
摘要:
The invention is directed to a process for the treatment of plastic material comprising a) providing a liquid; b) contacting the plastic material with the liquid; c) keeping the plastic material in the liquid at Tb−25° C. to Tb of the liquid, wherein Tb is the boiling point of the liquid at the applied pressure; and d) removing the plastic material from the liquid. Furthermore, the invention is directed to the use of a liquid for the treatment of plastic material and to a plant for treating plastic material with a liquid.
摘要:
The present invention relates to an equipment and method for producing polymer pellets which comprise one or more polymer components and one or more further components, wherein in said process at least one of said one or more further components is incorporated into pellets by applying a liquid, which comprises said at least one component, onto said pellets.
摘要:
The present invention relates to a polymer composition, comprising: (i) a polypropylene matrix; (ii) a first elastomeric phase dispersed within the matrix and having a glass transition temperature Tg1, measured with dynamical mechanical thermal analysis according to ISO 6721-2, wherein the first elastomeric phase comprises an ethylene copolymer having comonomer units derived from C3 to C8 olefins; (iii) a second elastomeric phase dispersed within the matrix, wherein the second elastomeric phase is crosslinked and has a glass transition temperature Tg2, measured with dynamical mechanical thermal analysis according to ISO 6721-2, within the range of −70° C. to −90° C., wherein the difference between Tg1 and Tg2 is at least 15° C. and Tg1 is higher than Tg2.
摘要:
The invention relates to propylene polymer compositions comprising 50-70 wt % of a propylene homo- or copolymer, 5-20 wt % of a first elastomeric ethylene-propylene copolymer, 5-25 wt % of a second elastomeric ethylene-propylene copolymer and 5-30 wt % of an ethylene polymer. The propylene polymer compositions are suitable for molding and they have low haze and a good impact strength/stiffness balance with good impact strengths at low temperatures.
摘要:
The present invention relates to a process for the preparation of an article, comprising the following steps: (a) providing a component (i) which comprises a blend of (a1) an unsaturated first polyolefin having a certain total amount m1 of carbon-carbon double bonds/1000 carbon atoms, (a2) a crosslinking agent, (a3) optionally an unsaturated low molecular weight compound having a certain total amount m2 carbon-carbon double bonds/1000 carbon atoms, (b) providing a component (ii) which comprises a second polymer having a certain total amount m3 of carbon-carbon double bonds/1000 carbon atoms, wherein m1, m2 and m3 satisfy a certain relationship, (c) forming a blend of component (i) and component (ii) wherein the weight ratio of the component (i) to the component (ii) is within the range of 10:90 to 99:1, (d) applying one or more layers of the blend onto a substrate.
摘要:
The application relates to a polyethylene composition having a base resin, the base resin comprising (A) a first polyethylene fraction, and (B) a second polyethylene fraction, wherein the melt flow rate MFR5/190° c. of the first fraction is higher than the melt flow rate MFR5/190° c. of the second fraction, the flow rate ratio FRR21/5 of the polyethylene composition, defined as the ratio of melt flow rate MFR21-6/190° c. to melt flow rate MFR5/190° c., is within the range of 15-28, and 10 the melt flow rate MFR5/190° c. of the polyethylene composition is within the range of 0.5-1.1 g/10 min.