Abstract:
The present invention provides a fiber-reinforced composite film with omnidirectional stretchability on which an auxetic structure 100 is formed integrally with the film on a film, wherein the auxetic structure 100 comprises a plurality of space regions 130 in the form of single closed curves regularly arranged on the film; an island 120 formed surrounded by the space region 130; and a connection portion 110 formed at regular intervals by the space region 130 to connect adjacent islands 120; wherein the film, island 120 and connection portion 110 are plastic materials reinforced with fibers wherein the space region 130 is filled with the elastic auxiliary member 20 and a manufacturing method thereof.
Abstract:
A semiconductor nanocrystal film according to an exemplary embodiment of the present invention includes a glass cloth including a glass fiber having a composition of E glass, S glass, T glass, or E-CR glass, a polymer matrix impregnated in the glass cloth, and a semiconductor nanocrystal dispersed in the polymer matrix, and thus may exhibit uniform light emitting distribution, a low coefficient of thermal expansion, and excellent mechanical strength.
Abstract:
The present application relates to a hard-coating resin composition including a siloxane resin, a preparing method of a siloxane cured hard-coating article using same and an optical film including the siloxane cured hard-coating article.
Abstract:
The present disclosure relates to a hard-coating cured material which contains a siloxane resin component including an epoxy group and a preparing method of the hard-coating cured material. Especially, by using a special polymerization method like a cationic polymerization and a moisture-heat treatment, it is possible to provide a hard-coating film having both superior flexibility and high surface hardness that cannot be obtained from conventional coating compositions.