Oxide ore smelting method
    3.
    发明授权

    公开(公告)号:US11608543B2

    公开(公告)日:2023-03-21

    申请号:US16094493

    申请日:2017-04-26

    摘要: The present invention addresses the problem, in methods for producing a metal or alloy by reducing a mixture that contains an oxide ore, of providing an oxide ore smelting method with good productivity and efficiency. The present invention is an oxide ore smelting method for producing a metal or alloy by reducing a mixture that contains an oxide ore, the method comprising at least: a mixing step S1 for mixing an oxide ore with a carbonaceous reducing agent; a mixture-molding step S2 for molding the mixture obtained to obtain a mixture-molded body; and a reducing step S3 for heating the mixture-molded body obtained at a specified reducing temperature in a reducing furnace.

    Method for preparing a leach feed matertial

    公开(公告)号:US11535910B2

    公开(公告)日:2022-12-27

    申请号:US16494567

    申请日:2018-04-04

    申请人: TNG LIMITED

    IPC分类号: C22B5/10 C22B3/10 C22B34/22

    摘要: A method (10) for preparing a leach feed material, the method (10) comprising the steps of: passing an ore or concentrate containing vanadium and iron to a reduction step (12) to form a reduced ore or concentrate; and passing the reduced ore or concentrate to a ferric leach step (14) to produce a ferric leachate containing iron and a ferric leach residue containing vanadium, wherein the ferric leach residue is suitable for use as the leach feed material for extracting and recovering vanadium.

    METHOD FOR SMELTING SAPROLITE ORE
    9.
    发明申请

    公开(公告)号:US20180030574A1

    公开(公告)日:2018-02-01

    申请号:US15552031

    申请日:2015-12-01

    摘要: Provided is a smelting method whereby a reaction for reducing pellets, said pellet being formed by using a saprolite ore as a starting material, can be effectively conducted and thus an iron/nickel alloy having a nickel grade of, for example, 16% or greater can be obtained. The method comprises: a pellet production step (S1) for producing the pellets from the saprolite ore; and a reduction step (S2) for heating and reducing the obtained pellets in a smelting furnace. In the pellet production step (S1), at least the saprolite ore and a preset amount of a carbonaceous reducing agent are mixed together to produce the pellets. In the reduction step (S2), a hearth carbonaceous reducing agent is preliminarily spread on the hearth of the smelting furnace and the pellets produced above are placed on the hearth carbonaceous reducing agent and then subjected to a heat reduction treatment.