摘要:
A dehydrogenation processing method for a turbine blade of a steam turbine. The method includes a step of heating the turbine blade by suppling heating steam into a casing of the steam turbine after a steam turbine plant is stopped. The heating steam supplied to the casing has a temperature that is higher than steam passing through the turbine blade during operation of the steam turbine plant. The method further includes repeating the process of supplying the heating steam into the casing a multiple of times.
摘要:
An R-T-B based permanent magnet includes main phase grains composed of R2T14B type compound. R is a rare earth element. T is iron group element(s) essentially including Fe or Fe and Co. B is boron. An average grain size of the main phase grains is 0.8 μm or more and 2.8 μm or less. The R-T-B based permanent magnet contains at least C and Zr in addition to R, T, and B. B is contained at 0.75 mass % or more and 0.88 mass % or less. Zr is contained at 0.65 mass % or more and 5.00 mass % or less. A formula (1) of 5.0≤[B]+[C]−[Zr]≤5.6 is satisfied, where [B] is a B content represented by atom %, [C] is a C content represented by atom %, and [Zr] is a Zr content represented by atom %.
摘要:
A method of producing an article selected from a titanium article and a titanium alloy article comprises melting feed materials with a source of hydrogen to form a molten heat of titanium or a titanium alloy, and casting at least a portion of the molten heat to form a hydrogenated titanium or titanium alloy ingot. The hydrogenated ingot is deformed at an elevated temperature to form a worked article comprising a cross-sectional area smaller than a cross-sectional area of the hydrogenated ingot. The worked article is dehydrogenated to reduce a hydrogen content of the worked article. In certain non-limiting embodiments of the method, the dehydrogenated article comprises an average α-phase particle size of less than 10 microns in the longest dimension.
摘要:
A dehydrogenation processing method for a turbine blade of a steam turbine includes: a step of heating the turbine blade by supplying heating steam into a casing of the steam turbine when a steam turbine plant is started or stopped.
摘要:
A method for improvement of magnetic performance of sintered NdFeB magnet includes the following steps. Firstly, material containing element R, H and X is to be covered on a surface of the sintered NdFeB magnet to form a finish coat. After that, proceed with a diffusion treatment and an aging treatment to the sintered NdFeB magnet with the finish coat in the environment of vacuum or inert gas. R is at least one of such elements as Sc, Y, La, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb and Lu. H is hydrogen. X is at least one of such elements as C, O, N, S, B, Cl and Si.
摘要:
An R-T-B based permanent magnet includes main phase grains composed of R2T14B type compound. R is a rare earth element. T is iron group element(s) essentially including Fe or Fe and Co. B is boron. An average grain size of the main phase grains is 0.8 μm to 2.8 μm. The R-T-B based permanent magnet contains at least C and Ga in addition to R, T, and B. B is contained at 0.71 mass % to 0.86 mass %. C is contained at 0.13 mass % to 0.34 mass %. Ga is contained at 0.40 mass % to 1.80 mass %. A formula (1) of 0.14≦[C]/([B]+[C])≦0.30 is satisfied, where [B] is a B content represented by atom %, and [C] is a C content represented by atom %.
摘要:
A method of producing an article selected from a titanium article and a titanium alloy article comprises melting feed materials with a source of hydrogen to form a molten heat of titanium or a titanium alloy, and casting at least a portion of the molten heat to form a hydrogenated titanium or titanium alloy ingot. The hydrogenated ingot is deformed at an elevated temperature to form a worked article comprising a cross-sectional area smaller than a cross-sectional area of the hydrogenated ingot. The worked article is dehydrogenated to reduce a hydrogen content of the worked article. In certain non-limiting embodiments of the method, the dehydrogenated article comprises an average α-phase particle size of less than 10 microns in the longest dimension.
摘要:
Steel is carburized at a temperature within the austenitic range and in an atmosphere which comprises nitrogen, hydrogen and carbon monoxide, by lowering the hydrogen concentration in the treatment atmosphere prior to cooling steel in oil, salt or water, so as to reduce the hydrogen concentration in the carburization layer of the steel, by outward diffusion of hydrogen from the carburization layer.
摘要:
A clad steel plate having tensile strength (TS) of 780 MPa or more, excellent bendability, collision resistance, and LME resistance. The clad steel plate having a base metal and a cladding metal on front and back surfaces of the base metal, and the chemical composition and microstructure of the base metal and the cladding metal being appropriately controlled so that the average Vickers hardness (HVL) of the cladding metal is 260 or less, the average Vickers hardness (HVL) of the cladding metal divided by the average Vickers hardness (HVB) of the base metal is 0.80 or less, the boundary roughness between the base metal and the cladding metal is 50 μm or less at the maximum height Ry, and the number of voids at the boundary between the base metal and the cladding metal is controlled to 20 or fewer per 10 mm length of the boundary.