摘要:
A method of fabricating a turbine engine part, the method including fabricating an ingot out of ceramic material of eutectic composition by performing the Czochralski process including putting a seed of the ingot that is to be obtained into contact with a molten bath of a mixture of eutectic composition in order to initiate the formation of the ingot on the seed, the mixture including at least two ceramic compounds; drawing the ingot from the molten bath while imposing on the ingot that is being formed a drawing speed less than or equal to 10 mm/h together with rotation at a speed of rotation less than or equal to 50 rpm; and machining the ingot as fabricated in this way in order to obtain the turbine engine part.
摘要:
The invention relates to a fused cast refractory material based on aluminium oxide, zirconium dioxide and silicon dioxide, and a use of such a material.
摘要:
This invention provides an electrolyte sheet for solid oxide fuel cells, characterized in: being formed by a doctor blade method or an extrusion molding method; being a scandia partially stabilized zirconia sheet, wherein 4 mol % to 6 mol % scandia is doped in a solid zirconia; a crystal structure thereof has a polycrystalline structure having a main body of tetragonal and including monoclinic phase, wherein a ratio of monoclinic phase (M), calculated by below described formula (1) from a diffraction peak intensity using X-ray diffraction, is 1% to 80%; and a Weibull modulus (m) thereof is not less than 10: a ratio of monoclinic phase(M:%)=[{monoclinic(1,1,1)+monoclinic(−1,1,1)}/{tetragonal and cubic(1,1,1)+monoclinic(1,1,1)+monoclinic(−1,1,1)}]×100 (1).
摘要:
A fusion-cast refractory is provided. The refractory comprises 0.8% to 2.5% Al2O3, 4.0% to 10.0% SiO2, 86% to 95% ZrO2, 0.1% to 1.2% B2O3, up to 0.04% Na2O, up to 0.4% CaO, up to 0.1% Fe2O3 and up to 0.25% TiO2.
摘要翻译:提供熔融耐火材料。 耐火材料包含0.8%至2.5%的Al 2 O 3,4.0%至10.0%的SiO 2,86%至95%的ZrO 2,0.1%至1.2%的B 2 O 3,至多0.04%的Na 2 O,至多0.4%的CaO,至多0.1%的Fe 2 O 3及以上 至0.25%的TiO 2。
摘要:
The invention relates to a refractory ceramic product which comprises: a) ≧93% by weight of at least one refractory basic component and b) ≦7% by weight of at least one anticorrosive component from the group including: b1) transition metals, b2) compounds of transition metals with each other, b3) non-oxidic compounds of transition metals, b4) oxidic compounds of transition metals, b5) compounds of the transition metals with Ca, Ba, Sr.
摘要:
Slip containing at least one aluminium oxide powder and at least one unstabilized zirconium dioxide powder, wherein a) the zirconium dioxide powder i) has a mean particle diameter of less than 300 nm, ii) shows only the monoclinic phase and the tetragonal phase in the X-ray diffraction pattern, with the proportion of tetragonal phase at room temperature being from 20 to 70%, and iii) is present in a proportion of from 2 to 20% by weight, based on the total amount of the slip, b) the aluminium oxide powder i) has a mean particle diameter of more than 300 nm and ii) is present in a proportion of from 80 to 98% by weight, based on the total amount of the slip, and c) the solids content, as the sum of aluminium oxide and zirconium dioxide, is from 50 to 85% by weight, based on the total amount of the slip.
摘要:
A fused-cast-alumina-zirconia-silica refractory consisting essentially of corundum crystals, baddeleyite crystals and a matrix glass phase and having a chemical composition comprising (a) from 30 to 70 wt % of Al.sub.2 O.sub.3, (b) from 20 to 59 wt % of ZrO.sub.2, (c) from 5 to 12 wt % of SiO.sub.2, (d) from 0.15 to 0.60 wt % of Na.sub.2 O, (e) from 0 to 0.50 wt % of K.sub.2 O, (f) from 0 to 0.40 wt % of Li.sub.2 O, (g) from 0.05 to 0.80 wt % of B.sub.2 O.sub.3, (h) from 0.05 to 0.80 wt % of P.sub.2 O.sub.5, and (i) from 0.05 to 0.50 wt % in total of at least one member selected from the group consisting of SnO.sub.2, ZnO, CuO and MnO.sub.2.
摘要翻译:基本上由刚玉晶体,方解石晶体和基体玻璃相组成的熔融 - 铸造 - 氧化铝 - 氧化锆 - 二氧化硅耐火材料,其化学组成包含(a)30至70重量%的Al 2 O 3,(b)20至59重量% %的ZrO 2,(c)5〜12重量%的SiO 2,(d)0.15〜0.60重量%的Na 2 O,(e)0〜0.50重量%的K 2 O,(f)0〜0.40重量% Li 2 O,(g)0.05〜0.80重量%的B 2 O 3,(h)0.05〜0.80重量%的P 2 O 5,(i)0.05〜0.50重量%的至少一种选自SnO 2 ,ZnO,CuO和MnO 2。
摘要:
Disclosed is a fused grain having the following chemical composition, expressed in percentages by mass on the basis of the oxides: ZrO2+HfO2: 2% to 13%; elements other than ZrO2, HfO2, Y2O; and Al2O3: ≤2%. Y2O3+Al2O3: made up to 100%; with 0.0065≤Y2O;/(ZrO2+HfO2)≤0.1300.
摘要:
Disclosed is a method for preparing an alumina-based solid solution ceramic powder by using an aluminum oxygen combustion synthesis water mist process, which comprises: drying raw materials and then mixing same until uniform to obtain a mixed material; loading the mixed material into a high-pressure reactor, igniting same in an oxygen-containing atmosphere, carrying out a high-temperature combustion synthesis reaction to form a high-temperature melt and then carrying out heat preservation for 1-60 s; and then opening a nozzle, ejecting the high-temperature melt through the nozzle and rapidly cooling same through a liquid phase, thus obtaining the alumina-based solid solution ceramic powder.