Electroluminescent ZnS:Mn phosphor and method of making
    1.
    发明授权
    Electroluminescent ZnS:Mn phosphor and method of making 失效
    电致发光ZnS:Mn荧光粉及其制备方法

    公开(公告)号:US08557143B2

    公开(公告)日:2013-10-15

    申请号:US12402019

    申请日:2009-03-11

    CPC classification number: C09K11/574 H05B33/14

    Abstract: An electroluminescent phosphor comprising ZnS:Mn is disclosed. Also disclosed are ZnS:Mn electroluminescent phosphors that are free of or substantially free of copper, and/or wherein the phosphor has a D50 size of less than about 5 μm. In addition, a method for preparing a ZnS:Mn phosphor is disclosed, comprising the steps of contacting at least a portion of each of a first solution comprising a Zn2+ compound, a manganese source, and a second solution comprising a S2− source agent; and then heating the mixture at a temperature and for a time sufficient to form a phosphor.

    Abstract translation: 公开了一种包含ZnS:Mn的电致发光荧光体。 还公开了不含或基本上不含铜的ZnS:Mn电致发光荧光体,和/或其中磷光体具有小于约5μm的D50尺寸。 另外,公开了一种制备ZnS:Mn荧光体的方法,包括使包含Zn 2+化合物,锰源和包含S2-源剂的第二溶液的第一溶液的至少一部分接触的步骤; 然后在足以形成荧光体的温度和时间下加热混合物。

    ELECTROLUMINESCENT ZnS:Mn PHOSPHOR AND METHOD OF MAKING
    2.
    发明申请
    ELECTROLUMINESCENT ZnS:Mn PHOSPHOR AND METHOD OF MAKING 失效
    电致发光ZnS:Mn磷光体及其制备方法

    公开(公告)号:US20090230357A1

    公开(公告)日:2009-09-17

    申请号:US12402019

    申请日:2009-03-11

    CPC classification number: C09K11/574 H05B33/14

    Abstract: An electroluminescent phosphor comprising ZnS:Mn is disclosed. Also disclosed are ZnS:Mn electroluminescent phosphors that are free of or substantially free of copper, and/or wherein the phosphor has a D50 size of less than about 5 μm. In addition, a method for preparing a ZnS:Mn phosphor is disclosed, comprising the steps of contacting at least a portion of each of a first solution comprising a Zn2+ compound, a manganese source, and a second solution comprising a S2− source agent; and then heating the mixture at a temperature and for a time sufficient to form a phosphor.

    Abstract translation: 公开了一种包含ZnS:Mn的电致发光荧光体。 还公开了不含或基本上不含铜的ZnS:Mn电致发光荧光体,和/或其中磷光体具有小于约5μm的D50尺寸。 另外,公开了一种制备ZnS:Mn荧光体的方法,包括使包含Zn 2+化合物,锰源和包含S2-源剂的第二溶液的第一溶液的至少一部分接触的步骤; 然后在足以形成荧光体的温度和时间下加热混合物。

    ELECTROLUMINESCENT PHOSPHOR AND METHOD OF MAKING
    3.
    发明申请
    ELECTROLUMINESCENT PHOSPHOR AND METHOD OF MAKING 审中-公开
    电致发光磷光体及其制备方法

    公开(公告)号:US20090212256A1

    公开(公告)日:2009-08-27

    申请号:US12393690

    申请日:2009-02-26

    CPC classification number: C09K11/584

    Abstract: A copper activated zinc sulfide electroluminescent phosphor is disclosed, wherein the phosphor comprises greater than about 1,000 ppm copper. Also disclosed is a copper activated zinc sulfide electroluminescent phosphor having a y color coordinate of at least about 0.480. A method for preparing the copper activated zinc sulfide electroluminescent phosphor is disclosed, comprising contacting a zinc sulfide, a first copper source, a magnesium source, and a lithium halide to form a first mixture; heating the mixture at a temperature and for a time sufficient to form a fired mixture; subjecting the fired mixture to a shear force capable of inducing a plurality of defects in the zinc sulfide lattice structure; and then contacting the fired mixture with a second copper source and a zinc oxide to form a second mixture; heating the second mixture at a temperature and for a time sufficient to form a second-fired material.

    Abstract translation: 公开了一种铜活化的硫化锌电致发光荧光体,其中磷光体包括大于约1,000ppm的铜。 还公开了具有至少约0.480的y色坐标的铜活化硫化锌电致发光荧光体。 公开了一种制备铜活化硫化锌电致发光荧光体的方法,包括使硫化锌,第一铜源,镁源和卤化锂接触以形成第一混合物; 在足以形成烧制混合物的温度和时间下加热混合物; 使烧制的混合物经受能够引起硫化锌晶格结构中的多个缺陷的剪切力; 然后将烧制的混合物与第二铜源和氧化锌接触以形成第二混合物; 在足以形成二次烧制材料的温度和时间下加热第二混合物。

    Single-Component Yellow-Emitting Electroluminescent Phosphor
    5.
    发明申请
    Single-Component Yellow-Emitting Electroluminescent Phosphor 失效
    单组分黄发光电致发光荧光粉

    公开(公告)号:US20060066208A1

    公开(公告)日:2006-03-30

    申请号:US10711634

    申请日:2004-09-29

    Applicant: Xianzhong Chen

    Inventor: Xianzhong Chen

    CPC classification number: C09K11/752 C09K11/616 H05B33/14

    Abstract: A single-component, yellow-emitting electroluminescent phosphor, a method for making same, and an electroluminescent lamp containing same, are described. The phosphor produces a yellow emission having an x color coordinate from 0.420 and 0.500 and y color coordinate from 0.420 and 0.460 when stimulated by an electric field.

    Abstract translation: 描述了单组分黄色发光电致发光荧光体及其制造方法,以及含有其的电致发光灯。 当由电场刺激时,磷光体产生具有0.420和0.500的x色坐标的黄色发射以及0.420和0.460的y色坐标。

    Single-component white-emitting electroluminescent phosphor and method of making same
    6.
    发明授权
    Single-component white-emitting electroluminescent phosphor and method of making same 失效
    单组分白色发光电致发光荧光体及其制造方法

    公开(公告)号:US06770221B1

    公开(公告)日:2004-08-03

    申请号:US10367036

    申请日:2003-02-14

    CPC classification number: C09K11/584 Y02B20/181

    Abstract: A single-component white-emitting electroluminescent phosphor and its method of making are described. The single-component phosphor exhibits a white emission having an x color coordinate of 0.23 to 0.41 and a y color coordinate of 0.25 to 0.42. The phosphor is comprised of zinc sulfide activated with copper, manganese, chlorine, and, optionally, one or more metals selected from gold and antimony.

    Abstract translation: 描述了单组分白色发光电致发光荧光粉及其制造方法。 单组分荧光体显示x色坐标为0.23至0.41且y色坐标为0.25至0.42的白色发射。 磷光体由用铜,锰,氯和任选的一种或多种选自金和锑的金属活化的硫化锌组成。

    METHOD OF MAKING ELECTROLUMINESCENT PHOSPHORS WITH SMALL PARTICLE SIZES AND POWDER WITH D50 VALUE OF NO MORE THAN 10 MICROMETERS
    7.
    发明申请
    METHOD OF MAKING ELECTROLUMINESCENT PHOSPHORS WITH SMALL PARTICLE SIZES AND POWDER WITH D50 VALUE OF NO MORE THAN 10 MICROMETERS 有权
    用小于10微米的D50值制造具有小颗粒尺寸和粉末的电致发光体磷光体的方法

    公开(公告)号:US20060220546A1

    公开(公告)日:2006-10-05

    申请号:US10907358

    申请日:2005-03-30

    CPC classification number: H05B33/14 C09K11/584

    Abstract: An electroluminescent phosphor powder includes copper-activated zinc sulfide particles that have a size distribution with a D50 value of no more than 10 μm, where no more than 25% of the particles have a size greater than about 15 μm and/or a 24-hr brightness of at least 15 footlamberts. These particles are made by a method that includes first firing copper-doped zinc sulfide mixed with zinc oxide, sulfur and a chloride-containing flux, rapidly cooling the mixture to below 100° C., and then mulling and second firing the mixture to provide a powder. The powder can then be elutriated to provide the electroluminescent powder with a narrow particle size distribution (more than 90% between about 5 and 15 μm). The elutriating step can be avoided (albeit with a slightly wider size distribution) by more tightly controlling the first firing temperature.

    Abstract translation: 电致发光荧光体粉末包括具有D50值不超过10μm的尺寸分布的铜活化的硫化锌颗粒,其中不超过25%的颗粒具有大于约15μm的尺寸和/或24- 小时至少15英尺的亮度。 这些颗粒通过以下方法制造:首先将与氧化锌,硫和含氯化物的助熔剂混合的掺铜的硫化锌,快速冷却到低于100℃,然后研磨和二次烧制该混合物, 一粉 然后可以将粉末淘洗以提供具有窄的粒度分布的电致发光粉末(在约5和15μm之间大于90%)。 通过更紧密地控制第一烧制温度,可以避免淘洗步骤(尽管具有略宽的分布)。

    Method of making electroluminescent phosphors with small particle sizes and powder with D50 value of no more than 10 micrometers
    8.
    发明授权
    Method of making electroluminescent phosphors with small particle sizes and powder with D50 value of no more than 10 micrometers 有权
    制造具有小粒径的电致发光荧光体和D50值不大于10微米的粉末的方法

    公开(公告)号:US07288216B2

    公开(公告)日:2007-10-30

    申请号:US10907358

    申请日:2005-03-30

    CPC classification number: H05B33/14 C09K11/584

    Abstract: An electroluminescent phosphor powder includes copper-activated zinc sulfide particles that have a size distribution with a D50 value of no more than 10 μm, where no more than 25% of the particles have a size greater than about 15 μm and/or a 24-hr brightness of at least 15 footlamberts. These particles are made by a method that includes first firing copper-doped zinc sulfide mixed with zinc oxide, sulfur and a chloride-containing flux, rapidly cooling the mixture to below 100° C., and then mulling and second firing the mixture to provide a powder. The powder can then be elutriated to provide the electroluminescent powder with a narrow particle size distribution (more than 90% between about 5 and 15 μm). The elutriating step can be avoided (albeit with a slightly wider size distribution) by more tightly controlling the first firing temperature.

    Abstract translation: 电致发光荧光体粉末包括具有D50值不超过10μm的尺寸分布的铜活化的硫化锌颗粒,其中不超过25%的颗粒具有大于约15μm的尺寸和/或24- 小时至少15英尺的亮度。 这些颗粒通过以下方法制造:首先将与氧化锌,硫和含氯化物的助熔剂混合的掺铜的硫化锌,快速冷却到低于100℃,然后研磨和二次烧制该混合物, 一粉 然后可以将粉末淘洗以提供具有窄的粒度分布的电致发光粉末(在约5和15μm之间大于90%)。 通过更紧密地控制第一烧制温度,可以避免淘洗步骤(尽管具有略宽的分布)。

    Single-component yellow-emitting electroluminescent phosphor
    9.
    发明授权
    Single-component yellow-emitting electroluminescent phosphor 失效
    单组分黄色发光电致发光荧光粉

    公开(公告)号:US07157845B2

    公开(公告)日:2007-01-02

    申请号:US10711634

    申请日:2004-09-29

    Applicant: Xianzhong Chen

    Inventor: Xianzhong Chen

    CPC classification number: C09K11/752 C09K11/616 H05B33/14

    Abstract: A single-component, yellow-emitting electroluminescent phosphor, a method for making same, and an electroluminescent lamp containing same, are described. The phosphor produces a yellow emission having an x color coordinate from 0.420 to 0.500 and y color coordinate from 0.420 to 0.460 when stimulated by an electric field.

    Abstract translation: 描述了单组分黄色发光电致发光荧光体及其制造方法,以及含有其的电致发光灯。 当由电场刺激时,荧光体产生具有0.420至0.500的x色坐标的黄色发射和0.420至0.460的y色坐标。