摘要:
A squeegee blade made of a compound having a methyl vinyl silicone polymer, a filler, and a friction-reducing additive is provided. The friction-reducing additive is present in an amount from between about 5 and 42 weight percent. The average particle size of the friction-reducing additive is preferably less than about 25 microns, thereby permitting extrusion of the compound into the shape of a squeegee blade. Polytetrafluoroethylene is preferred as a friction-reducing additive, but other substances, such as boron nitride or graphite could be used.
摘要:
A wiper blade made of a compound having a methyl vinyl silicone polymer, a filler, and a friction-reducing additive is provided. The friction-reducing additive is present in an amount from between about 5–42 weight percent, preferably 11 percent. The average particle size of the friction-reducing additive is preferably less than 6 microns, thereby permitting extrusion of the compound into the shape of a wiper blade. Polytetrafluoroethylene is preferred as a friction-reducing additive, but other substances, such as boron nitride or graphite could be used.
摘要:
A wiper blade made of a compound having a methyl vinyl silicone polymer, a filler, and a friction-reducing additive is provided. The friction-reducing additive is present in an amount from between about 5 and 42 weight percent. The average particle size of the friction-reducing additive is preferably less than about 25 microns, thereby permitting extrusion of the compound into the shape of a wiper blade. Polytetrafluoroethylene is preferred as a friction-reducing additive, but other substances, such as boron nitride or graphite could be used.
摘要:
A wiper blade made of a compound having a methyl vinyl silicone polymer, a filler, and a friction-reducing additive is provided. The friction-reducing additive is present in an amount from between about 5 and 42 weight percent. The average particle size of the friction-reducing additive is preferably less than about 25 microns, thereby permitting extrusion of the compound into the shape of a wiper blade. Polytetrafluoroethylene is preferred as a friction-reducing additive, but other substances, such as boron nitride or graphite could be used.
摘要:
A wiper blade made of a compound having a methyl vinyl silicone polymer, a filler, and a friction-reducing additive is provided. The friction-reducing additive is present in an amount from between about 5 and 42 weight percent, preferably 11 percent. The average particle size of the friction-reducing additive is preferably less than about 25 microns, thereby permitting extrusion of the compound into the shape of a wiper blade. Polytetrafluoroethylene is preferred as a friction-reducing additive, but other substances, such as boron nitride or graphite could be used.
摘要:
A wiper blade made of a compound having a methyl vinyl silicone polymer, a filler, and a friction-reducing additive is provided. The friction-reducing additive is present in an amount from between about 5 and 42 weight percent, preferably 11 percent. The average particle size of the friction-reducing additive is preferably less than about 25 microns, thereby permitting extrusion of the compound into the shape of a wiper blade. Polytetrafluoroethyiene is preferred as a friction-reducing additive, but other substances, such as boron nitride or graphite could be used.
摘要:
A coherent material is formed on a substrate (10) by providing a precursor suspension (14) in which particulates are suspended in a carrier fluid, and directing the precursor suspension (14) at the substrate (10) from a first source (12). Generally contemporaneously with application of the deposited precursor suspension (14) to the surface, hot gases, e.g. hot gases produced by a flame (16), are directed at the substrate (10) from a remote second source (18) to fuse the particulates into the coherent material.
摘要:
Flame produced vapors for combustion chemical vapor deposition are redirected from the direction of the flame by differential atmospheric pressure, such as positive pressure provided by a blower or negative pressure provided by a vacuum. This allows, for example, lower surface temperatures of substrates being coated with flame-produced vapors and coating of interior surfaces.
摘要:
An improved chemical vapor deposition apparatus and procedure is disclosed. The technique provides improved shielding of the reaction and deposition zones involved in providing CVD coatings, whereby coatings can be produced, at atmospheric pressure, of materials which are sensitive to components in the atmosphere on substrates which are sensitive to high temperatures and which are too large, or inconvenient, to process in vacuum or similar chambers. The improved technique can be used with various energy sources and is particularly compatible with Combustion Chemical Vapor Deposition (CCVD) techniques.
摘要:
An apparatus for connecting a wiper blade to a wiper arm (202), comprising a wiper blade adapter (2) and a locking tab (102) wherein the locking tab is releasably engageable with the wiper blade adapter such that when the locking tab releasably engages the wiper blade adapter at least a portion of the wiper arm is retained between the wiper blade adapter and the locking tab. A process for connecting a wiper blade to a wiper arm, comprising releasably engaging a locking tab with a wiper blade adapter such that when the locking tab releasably engages the wiper blade adapter at least a portion of the wiper arm is retained between the wiper blade adapter and the locking tab.