Abstract:
A precursor mixture for producing a porous body, wherein the precursor mixture comprises: (i) milled alpha alumina powder having a particle size of 0.1 to 6 microns, (ii) boehmite powder that functions as a binder of the alpha alumina powders, and (iii) burnout materials having a particle sizes of 1-10 microns. In some embodiments, an unmilled alpha alumina powder having a particle size of 10 to 100 microns is also included in said precursor mixture. Also described herein is a method for producing a porous body in which the above-described precursor mixture is formed to a given shape, and subjected to a heat treatment step in which the formed shape is sintered to produce the porous body.
Abstract:
A silver-based ethylene epoxidation catalyst is provided that exhibits improved performance, i.e., selectivity and activity decline. The catalyst that exhibits the improved performance includes greater than about 20% by weight of silver disposed on an alpha-alumina carrier, and a promoting amount of one or more promoters disposed on the alpha-alumina carrier. The silver is present on the alpha-alumina carrier as silver particles having a diameter of greater than about 150 nm and a distribution density of about 20 particles per 1 square micron or less.
Abstract:
A precursor mixture for producing a porous body, wherein the precursor mixture comprises: (i) milled alpha alumina powder having a particle size of 0.1 to 6 microns, (ii) boehmite powder that functions as a binder of the alpha alumina powders, and (iii) burnout materials having a particle sizes of 1-10 microns. In some embodiments, an unmilled alpha alumina powder having a particle size of 10 to 100 microns is also included in said precursor mixture. Also described herein is a method for producing a porous body in which the above-described precursor mixture is formed to a given shape, and subjected to a heat treatment step in which the formed shape is sintered to produce the porous body.
Abstract:
A precursor mixture for producing a porous body, wherein the precursor mixture comprises: (i) at least one milled alpha alumina powder having a particle size of 0.1 to 6 microns, (ii) non-silicate powder that functions as a binder of the alpha alumina powders, and (iii) at least one burnout material having a particle size of 1-10 microns and a decomposition temperature of less than 550° C., with the proviso that a burnout material having a decomposition temperature of 550° C. or greater is excluded from the precursor mixture.
Abstract:
A method is provided for improving the performance of a silver-based epoxidation catalyst comprising a carrier. The carrier includes at least 80 percent alpha alumina and has a pore volume from 0.3 mL/g to 1.2 mL/g, a surface area from 0.3 m2/g to 3.0 m2/g, and a pore architecture that provides at least one of a tortuosity of 7 or less, a constriction of 4 or less and a permeability of 30 mdarcys or greater. A catalytic amount of silver and a promoting amount of one or more promoters is disposed on and/or in said carrier. The method further includes the steps of initiating an epoxidation reaction by reacting a feed gas composition containing ethylene and oxygen present in a ratio of from about 3.5:1 to about 12:1, in the presence of the silver-based epoxidation catalyst at a temperature of about 200° C. to about 230° C., and subsequently increasing the temperature either stepwise or continuously.
Abstract:
A porous body is provided with enhanced fluid transport properties that is capable of performing or facilitating separations, or performing reactions and/or providing areas for such separations or reactions to take place. The porous body includes at least 80 percent alpha alumina and has a pore volume from 0.3 mL/g to 1.2 mL/g and a surface area from 0.3 m2/g to 3.0 m2/g. The porous body further includes a pore architecture that provides at least one of a tortuosity of 7.0 or less, a constriction of 4.0 or less and a permeability of 30 mdarcys or greater. The porous body can be used in a wide variety of applications such as, for example, as a filter, as a membrane or as a catalyst carrier.
Abstract:
A precursor mixture for producing a porous body, wherein the precursor mixture comprises: (i) at least one milled alpha alumina powder having a particle size of 0.1 to 6 microns, (ii) non-silicate powder that functions as a binder of the alpha alumina powders, and (iii) at least one burnout material having a particle size of 1-10 microns and a decomposition temperature of less than 550° C., with the proviso that a burnout material having a decomposition temperature of 550° C. or greater is excluded from the precursor mixture.
Abstract:
A precursor mixture for producing a porous body, wherein the precursor mixture comprises: (i) milled alpha alumina powder having a particle size of 0.1 to 6 microns, (ii) boehmite powder that functions as a binder of the alpha alumina powders, and (iii) burnout materials having a particle sizes of 1-10 microns. In some embodiments, an unmilled alpha alumina powder having a particle size of 10 to 100 microns is also included in said precursor mixture. Also described herein is a method for producing a porous body in which the above-described precursor mixture is formed to a given shape, and subjected to a heat treatment step in which the formed shape is sintered to produce the porous body.
Abstract:
A porous body is provided with enhanced fluid transport properties that is capable of performing or facilitating separations, or performing reactions and/or providing areas for such separations or reactions to take place. The porous body includes at least 80 percent alpha alumina and has a pore volume from 0.3 mL/g to 1.2 mL/g and a surface area from 0.3 m2/g to 3.0 m2/g. The porous body further includes a pore architecture that provides at least one of a tortuosity of 7.0 or less, a constriction of 4.0 or less and a permeability of 30 mdarcys or greater. The porous body can be used in a wide variety of applications such as, for example, as a filter, as a membrane or as a catalyst carrier.
Abstract:
Oxalic acid is employed in a precursor mixture containing at least one milled alpha alumina powder having a particle size of 0.1 to 6 microns, boehmite powder that functions as a binder of the alpha alumina powders, and at least one burnout material having a particle size of 1-10 microns to provide a porous body having enhanced pore architecture in which extrusion cracks can be reduced. The presence of oxalic acid in such as precursor mixture can reduce and even eliminate NOx emission during a high temperature heat treatment process.