公开(公告)号:US20220018397A1
公开(公告)日:2022-01-20
申请号:US17449491
申请日:2021-09-30
Inventor: Brian MCNAMARA , Ian D. Hutcheson , Gerard T. Buss , David A. Rich
Abstract: The present disclosure relates to a low friction bearing liner for a solenoid that may include a core layer, a first outer layer overlying a first surface of the core layer, a second outer layer overlying the first outer layer, a first inner layer overlying a second surface of the core layer that is opposite of the first surface of the core layer, and a second inner layer overlying the first inner layer. The first outer layer and the first inner layer may include a fluoropolymer material and may have a melt flow rate of at least about 2 g/10 min at 372° C. The second outer layer and the second inner layer may include a fluoropolymer material distinct from the fluoropolymer material of the first outer layer and may have a surface coefficient of friction of not greater than about 0.2.
-
公开(公告)号:US12157292B2
公开(公告)日:2024-12-03
申请号:US17664516
申请日:2022-05-23
Inventor: David A. Rich , Gerard T. Buss , James M. McMartin , Timothy P. Pollock
Abstract: The present disclosure relates to a composite article that may include a structural substrate, a multilayer fluoropolymer film that can include a high-melt fluoropolymer layer and a low-melt fluoropolymer adhesion layer that may contact the structural substrate and the fluoropolymer film. The high-melt fluoropolymer layer may have a melting temperature A1 and the low-melt fluoropolymer adhesive layer may have a melting temperature A2. The melting temperature A2 may be less than the melting temperature A1.
-
公开(公告)号:US11852194B2
公开(公告)日:2023-12-26
申请号:US17643199
申请日:2021-12-08
Inventor: David A. Rich , Nicole M. Dirando
CPC classification number: F16C33/201 , F16C17/02 , F16C33/206 , H01F7/1607 , F16C2202/02 , F16C2202/50 , F16C2208/02 , F16C2208/58 , F16C2240/60 , F16C2380/00
Abstract: The present disclosure relates to a low friction bearing liner for a solenoid may include a low friction layer. The low friction layer may include a first fluoropolymer matrix component and a first thermoplastic filler component distributed throughout the first fluoropolymer matrix component. The content of the first fluoropolymer matrix component may be at least about 1 wt. % and not greater than about 99 wt. % for a total weight of the first low friction layer. The content of the first thermoplastic filler component may be at least about 1 wt. % and not greater than about 99 wt. % for a total weight of the first low friction layer.
-
公开(公告)号:US11708857B2
公开(公告)日:2023-07-25
申请号:US17449491
申请日:2021-09-30
Inventor: Brian McNamara , Ian D. Hutcheson , Gerard T. Buss , David A. Rich
CPC classification number: F16C33/122 , H01F7/081 , H01F7/16 , F16C2380/00 , H01F2007/086
Abstract: The present disclosure relates to a low friction bearing liner for a solenoid that may include a core layer, a first outer layer overlying a first surface of the core layer, a second outer layer overlying the first outer layer, a first inner layer overlying a second surface of the core layer that is opposite of the first surface of the core layer, and a second inner layer overlying the first inner layer. The first outer layer and the first inner layer may include a fluoropolymer material and may have a melt flow rate of at least about 2 g/10 min at 372° C. The second outer layer and the second inner layer may include a fluoropolymer material distinct from the fluoropolymer material of the first outer layer and may have a surface coefficient of friction of not greater than about 0.2.
-
公开(公告)号:US11220120B2
公开(公告)日:2022-01-11
申请号:US16718294
申请日:2019-12-18
Inventor: Brian McNamara , Ian D. Hutcheson , Gerard T. Buss , David A. Rich
IPC: B41J11/057 , B32B27/08 , B32B27/32
Abstract: The present disclosure relates to a low friction roller liner for a printer assembly that may include a core layer, a first outer layer overlying a first surface of the core layer, a second outer layer overlying the first outer layer, a first inner layer overlying a second surface of the core layer that is opposite of the first surface of the core layer, and a second inner layer overlying the first inner layer. The first outer layer and the first inner layer may include a fluoropolymer material and may have a melt flow rate of at least about 2 g/10 min at 372° C. The second outer layer and the second inner layer may include a fluoropolymer material distinct from the fluoropolymer material of the first outer layer and may have a surface coefficient of friction of not greater than about 0.2.
-
公开(公告)号:US11162531B2
公开(公告)日:2021-11-02
申请号:US16718278
申请日:2019-12-18
Inventor: Brian McNamara , Ian D. Hutcheson , Gerard T. Buss , David A. Rich
Abstract: The present disclosure relates to a low friction bearing liner for a solenoid that may include a core layer, a first outer layer overlying a first surface of the core layer, a second outer layer overlying the first outer layer, a first inner layer overlying a second surface of the core layer that is opposite of the first surface of the core layer, and a second inner layer overlying the first inner layer. The first outer layer and the first inner layer may include a fluoropolymer material and may have a melt flow rate of at least about 2 g/10 min at 372° C. The second outer layer and the second inner layer may include a fluoropolymer material distinct from the fluoropolymer material of the first outer layer and may have a surface coefficient of friction of not greater than about 0.2.
-
-
-
-
-