公开(公告)号:US20180194907A1
公开(公告)日:2018-07-12
申请号:US15741521
申请日:2016-06-27
Applicant: SABIC Global Technologies B.V.
Inventor: Domenico LA CAMERA , Erik SCHWARTZ , Robert Dirk VAN DE GRAMPEL , Ronald LUIJTEN
IPC: C08J3/24 , C08J3/28 , C08K3/04 , C08K5/101 , C08K5/3492 , C08K7/14 , C08L27/18 , C08L69/00 , C08L71/12 , C08L77/00 , C08L79/08 , C08L83/04
CPC classification number: C08J3/247 , C08J3/24 , C08J3/28 , C08J5/005 , C08J5/042 , C08J5/043 , C08K3/041 , C08K3/042 , C08K5/0025 , C08K5/092 , C08K5/101 , C08K5/20 , C08K5/3417 , C08K5/34924 , C08K5/526 , C08K7/14 , C08L27/18 , C08L67/02 , C08L69/00 , C08L71/123 , C08L77/00 , C08L77/02 , C08L77/06 , C08L79/08 , C08L83/04 , C08L2205/16
Abstract: The disclosure concerns compositions comprising: from about 40 wt. % to about 99.5 wt. % of a polymer base resin; N from 0 wt. % to about 60 wt. % of a reinforcing filler; from 0 wt. % to about 25 wt. % of a lubricant; and from about 0.05 wt. % to about 6 wt. % of a cross-linking agent; wherein the composition is treated to induce cross-linking, wherein the combined weight percent value of all components does not exceed 100 wt % and wherein the composition shows improved tensile fatigue versus a corresponding composition without the cross-linking agent.