摘要:
The present invention provides compositions of phosphorus acid group and methacrylic anhydride group containing telomeric copolymers of methacrylic acid having an as yet never achieved amount of more than 70 wt. %, or, preferably, 72 wt. % or more, and up to 99 wt. %, of methacrylic anhydride groups based on the total weight of polymerized methacrylic acid and/or salt units. The compositions enjoy higher thermal stability than was previously achieved and enable easer processing that does not require the removal of liquids or solvents.
摘要:
The present invention provides compositions comprising particles or agglomerates of one or more phosphorus oxide telomer or cotelomer ((co)telomer) of one or more unsaturated carboxylic acids or anhydrides having a mean average particle size of from 2 μm to 1 mm, preferably from 5 to 500 μm, preferably, comprising at least one carboxylic acid anhydride group. In addition, the present invention provides methods comprising aqueous solution addition polymerizing a monomer mixture of one or more unsaturated carboxylic acid in the presence of a phosphorus oxide acid or salt compound, drying the resulting copolymer at a temperature of from 120 to 230° C. and reducing its particle size to make a phosphorus oxide (co)telomer particle or agglomerate; the methods may further comprise reacting the (co)telomer particle or agglomerate with one or more polyether polyol, alkyl polyether polyol, polyether amine or alkyl polyether amine, with heating, to form a comb polymer useful, e.g. as a superplasticizer or dispersant.
摘要:
The present invention provides hypophosphite (co)telomers of methacrylic anhydride having a weight average molecular weight of from 1,000 to 20,000, and having, on average, at least one phosphorus atom bound to two carbon atoms, and at least one carboxylic acid or salt group.
摘要:
The present invention provides telomeric copolymers of acrylic and methacrylic acid which further comprise an olefin polymerization residue and have one or more phosphorus acid groups wherein the phosphorus acid group comprises one or more phosphorus atom in the +1 oxidation state or in the +3 oxidation state, or both. In addition the present invention provides methods of making the telomeric copolymers comprising aqueous solution copolymerizing a monomer mixture comprising acrylic acid and methacrylic acid in the presence of a phosphorus acid group containing reactant having a phosphorus atom in the +1 oxidation state, and thermally treating the resulting telomeric copolymer at 175° C. or higher for a sufficient time to decarboxylate the copolymer.
摘要:
The present invention provides hypophosphite (co)telomers of methacrylic anhydride having a weight average molecular weight of from 1,000 to 20,000, and having, on average, at least one phosphorus atom bound to two carbon atoms, and at least one carboxylic acid or salt group.
摘要:
A method for producing a nitrone of formula (I) wherein R is a branched alkyl group having from four to thirty carbon atoms; R1, R2, R3 and R4 independently are hydrogen or alkyl groups having from one to six carbon atoms from an imine having formula (II)
摘要:
The present invention provides telomeric copolymers of acrylic and methacrylic acid which further comprise an olefin polymerization residue and have one or more phosphorus acid groups wherein the phosphorus acid group comprises one or more phosphorus atom in the +1 oxidation state or in the +3 oxidation state, or both. In addition the present invention provides methods of making the telomeric copolymers comprising aqueous solution copolymerizing a monomer mixture comprising acrylic acid and methacrylic acid in the presence of a phosphorus acid group containing reactant having a phosphorus atom in the +1 oxidation state, and thermally treating the resulting telomeric copolymer at 175° C. or higher for a sufficient time to decarboxylate the copolymer.
摘要:
The present invention provides compositions of phosphorus acid group and methacrylic anhydride group containing telomeric copolymers of methacrylic acid having an as yet never achieved amount of more than 70 wt. %, or, preferably, 72 wt. % or more, and up to 99 wt. %, of methacrylic anhydride groups based on the total weight of polymerized methacrylic acid and/or salt units. The compositions enjoy higher thermal stability than was previously achieved and enable easer processing that does not require the removal of liquids or solvents.
摘要:
The invention provides aqueous thermosetting binder compositions exhibiting both of improved flame retardation and wet tensile strength comprising a reducing sugar, a diprimary diamine or a polyprimary diamine, a phosphorus acid salt and from 3 to 20 wt. %, based on total solids, of an aqueous polymeric polyacid solution polymer containing phosphorus or its salt, wherein the aqueous thermosetting binder composition comprises from 0.7% P (s/s) to 5% P (s/s).
摘要:
The invention provides aqueous thermosetting binder compositions exhibiting both of improved flame retardation and wet tensile strength comprising a reducing sugar, a diprimary diamine or a polyprimary diamine, a phosphorus acid salt and from 3 to 20 wt. %, based on total solids, of an aqueous polymeric polyacid solution polymer containing phosphorus or its salt, wherein the aqueous thermosetting binder composition comprises from 0.7% P (s/s) to 5% P (s/s).