Abstract:
A porous polybenzimidazole (PBI) particulate resin is disclosed. This resin is easily dissolved at ambient temperatures and pressures. The resin is made by: dissolving a virgin PBI resin in a highly polar solvent; precipitating the dissolved PBI in a bath; and drying the precipitated PBI, the dried precipitated PBI being porous. The porous PBI resin may be dissolved by: mixing a porous PBI resin with a highly polar solvent at ambient temperatures and pressures to form a solution.
Abstract:
A porous polybenzimidazole (PBI) particulate resin is disclosed. This resin is easily dissolved at ambient temperatures and pressures. The resin is made by: dissolving a virgin PBI resin in a highly polar solvent; precipitating the dissolved PBI in a bath; and drying the precipitated PBI, the dried precipitated PBI being porous. The porous PBI resin may be dissolved by: mixing a porous PBI resin with a highly polar solvent at ambient temperatures and pressures to form a solution.
Abstract:
A process for producing a solution blend of a polybenzimidazole (PBI) and a polyetherketoneketone (PEKK). The PBI is mixed with sulfuric acid at a temperature between 40° C. and 80° C. for 30 minutes to 2 hours to produce a PBI solution then cooled to room temperature to form a cooled PBI solution. Then PEKK is added to the cooled PBI solution to form a mixture and that mixture is stirred from 30 minutes to 2 hours at room temperature to form a stirred mixture. The stirred mixture is poured into an excess of water being stirred swiftly to form an aqueous mixture. The aqueous mixture is filtered to produce a blend. The blend is washed with water and dried. The resulting blend can yield a blend in all proportion from 1/99 PBI/PEKK to 99/1 PBI/PEKK.
Abstract:
A pervaporation membrane may be an acid-resistant polybenzidimazole (PBI) membrane. The acid-resistant PBI membrane may be a PBI membrane chemically modified by a process selected from the group consisting of sulfonation, phosphonation, cross-linking, N-substitution, and/or combinations thereof. The membrane may be thermally stabilized. A method for the dehydration of an acid material may include the steps of: contacting an acidic aqueous solution with a membrane of an acid-resistant polybenzidimazole; taking away a permeate stream rich in water; and taking away a concentrate steam rich in the acid material. The acidic aqueous solution may be acetic acid.
Abstract:
A pervaporation membrane may be an acid-resistant polybenzidimazole (PBI) membrane. The acid-resistant PBI membrane may be a PBI membrane chemically modified by a process selected from the group consisting of sulfonation, phosphonation, cross-linking, N-substitution, and/or combinations thereof. The membrane may be thermally stabilized. A method for the dehydration of an acid material may include the steps of: contacting an acidic aqueous solution with a membrane of an acid-resistant polybenzidimazole; taking away a permeate stream rich in water; and taking away a concentrate steam rich in the acid material. The acidic aqueous solution may be acetic acid.
Abstract:
A pervaporation membrane may be an acid-resistant polybenzidimazole (PBI) membrane. The acid-resistant PBI membrane may be a PBI membrane chemically modified by a process selected from the group consisting of sulfonation, phosphonation, cross-linking, N-substitution, and/or combinations thereof. The membrane may be thermally stabilized. A method for the dehydration of an acid material may include the steps of: contacting an acidic aqueous solution with a membrane of an acid-resistant polybenzidimazole; taking away a permeate stream rich in water; and taking away a concentrate steam rich in the acid material. The acidic aqueous solution may be acetic acid.
Abstract:
A porous polybenzimidazole (PBI) particulate resin is disclosed. This resin is easily dissolved at ambient temperatures and pressures. The resin is made by: dissolving a virgin PBI resin in a highly polar solvent; precipitating the dissolved PBI in a bath; and drying the precipitated PBI, the dried precipitated PBI being porous. The porous PBI resin may be dissolved by: mixing a porous PBI resin with a highly polar solvent at ambient temperatures and pressures to form a solution.
Abstract:
A process for producing a solution blend of a polybenzimidazole (PBI) and a polyetherketoneketone (PEKK). The PBI is mixed with sulfuric acid at a temperature between 40° C. and 80° C. for 30 minutes to 2 hours to produce a PBI solution then cooled to room temperature to form a cooled PBI solution. Then PEKK is added to the cooled PBI solution to form a mixture and that mixture is stirred from 30 minutes to 2 hours at room temperature to form a stirred mixture. The stirred mixture is poured into an excess of water being stirred swiftly to form an aqueous mixture. The aqueous mixture is filtered to produce a blend. The blend is washed with water and dried. The resulting blend can yield a blend in all proportion from 1/99 PBI/PEKK to 99/1 PBI/PEKK.
Abstract:
A porous polybenzimidazole (PBI) particulate resin is disclosed. This resin is easily dissolved at ambient temperatures and pressures. The resin is made by: dissolving a virgin PBI resin in a highly polar solvent; precipitating the dissolved PBI in a bath; and drying the precipitated PBI, the dried precipitated PBI being porous. The porous PBI resin may be dissolved by: mixing a porous PBI resin with a highly polar solvent at ambient temperatures and pressures to form a solution.