Composite foamed polypropylene resin molding and method of producing same
    2.
    发明授权
    Composite foamed polypropylene resin molding and method of producing same 有权
    复合发泡聚丙烯树脂成型及其制造方法

    公开(公告)号:US07182896B2

    公开(公告)日:2007-02-27

    申请号:US10502934

    申请日:2003-03-19

    IPC分类号: B29C44/04

    摘要: A composite foamed polypropylene resin molding including a plurality of sections which are fuse-bonded to each other, at least two of which differ from each other in color, apparent density, composition and/or mechanical strengths, each of which is formed from expanded polypropylene resin beads, and each of which shows a high temperature endothermic peak in a DSC curve thereof. At least one of the sections satisfies conditions (d) to (f) at the same time: (d) to be formed from specific expanded polypropylene resin beads of a base resin having a tensile modulus of at least 1,200 MPa, (e) to have an apparent density D2 of 10–500 g/L, and (f) to have such a high temperature endothermic peak with a calorific of E2 J/g, wherein D2 and E2 have the relationship 20−0.020×D2≦E2≦65−0.100×D2. The composite molding may be prepared by filling expanded polypropylene resin beads in each of a plurality of contiguous spaces defined in a mold cavity and heating the expanded beads to fuse-bond respective expanded beads together into a unitary body. At least one of the spaces is filled with the specific expanded polypropylene resin beads.

    摘要翻译: 一种复合发泡聚丙烯树脂模制品,其包括彼此熔合键合的多个部分,其中至少两个在颜色,表观密度,组成和/或机械强度方面彼此不同,每个部分由发泡聚丙烯 树脂珠,其DSC曲线中都显示高温吸热峰。 至少一个部分同时满足条件(d)至(f):(d)由具有至少1200MPa的拉伸模量的基础树脂的特定发泡聚丙烯树脂珠粒形成,(e)至 具有10-500g / L的表观密度D 2,和(f)具有发热量为E 2 J / g的高温吸热峰,其中D 2和E 2具有20-0.020xD 2的关系 <= E 2 <= 65-0.100xD 2.复合成型可以通过在模腔中限定的多个连续空间中的每一个中填充发泡聚丙烯树脂珠并加热发泡珠以将相应的发泡珠熔合在一起来制备 进入一个单一的身体。 至少一个空间用特定的发泡聚丙烯树脂珠填充。

    Foamed molding of expanded polypropylene resin beads
    4.
    发明申请
    Foamed molding of expanded polypropylene resin beads 审中-公开
    发泡聚丙烯树脂珠发泡成型

    公开(公告)号:US20070197673A1

    公开(公告)日:2007-08-23

    申请号:US11790316

    申请日:2007-04-25

    IPC分类号: B29C44/34

    摘要: A process for the production of expanded beads, including kneading a base resin containing a polypropylene resin and having a tensile modulus of at least 1,200 MPa together with a mixture of a coloring agent and a thermoplastic polymer having a tensile modulus lower than that of the base resin to form a kneaded mixture including a matrix of the base resin and a multiplicity of domains dispersed in the matrix and each containing the thermoplastic polymer and the coloring agent. The kneaded mixture is formed into resin particles, then treated with an organic peroxide to modify surfaces of the resin particles therewith. Foaming and expanding of the surface-modified resin particles gives expanded beads having an inside region surrounded by a surface region. The heat of fusion of a high temperature peak of the surface region is lower than that of the inside region.

    摘要翻译: 一种生产发泡珠粒的方法,包括捏合含有聚丙烯树脂的基础树脂和拉伸模量至少为1200MPa的着色剂和热塑性聚合物的混合物,其拉伸模量低于基体的拉伸模量 树脂以形成包含基体树脂的基体和分散在基体中的多个畴并且各自包含热塑性聚合物和着色剂的捏合混合物。 捏合的混合物形成树脂颗粒,然后用有机过氧化物处理以改性树脂颗粒的表面。 表面改性树脂颗粒的发泡和膨胀产生具有由表面区域包围的内部区域的发泡珠粒。 表面区域的高温峰的熔化热低于内部区域的熔融热。

    Composite foamed polypropylene resin molding and method of producing same
    5.
    发明申请
    Composite foamed polypropylene resin molding and method of producing same 审中-公开
    复合发泡聚丙烯树脂成型及其制造方法

    公开(公告)号:US20070026218A1

    公开(公告)日:2007-02-01

    申请号:US11529209

    申请日:2006-09-29

    IPC分类号: B32B7/02 B32B3/00 B32B3/26

    摘要: A composite foamed polypropylene resin molding including a plurality of sections which are fuse-bonded to each other, at least two of which differ from each other in color, apparent density, composition and/or mechanical strengths, each of which is formed from expanded polypropylene resin beads, and each of which shows a high temperature endothermic peak in a DSC curve thereof. At least one of the sections satisfies conditions (d) to (f) at the same time: (d) to be formed from specific expanded polypropylene resin beads of a base resin having a tensile modulus of at least 1,200 MPa, (e) to have an apparent density D2 of 10-500 g/L, and (f) to have such a high temperature endothermic peak with a calorific of E2 J/g, wherein D2 and E2 have the relationship 20−0.020×D2≦E2≦65−0.100×D2. The composite molding may be prepared by filling expanded polypropylene resin beads in each of a plurality of contiguous spaces defined in a mold cavity and heating the expanded beads to fuse-bond respective expanded beads together into a unitary body. At least one of the spaces is filled with the specific expanded polypropylene resin beads.

    摘要翻译: 一种复合发泡聚丙烯树脂模制品,其包括彼此熔合键合的多个部分,其中至少两个在颜色,表观密度,组成和/或机械强度方面彼此不同,每个部分由发泡聚丙烯 树脂珠,其DSC曲线中都显示高温吸热峰。 至少一个部分同时满足条件(d)至(f):(d)由具有至少1200MPa的拉伸模量的基础树脂的特定发泡聚丙烯树脂珠粒形成,(e)至 具有10-500g / L的表观密度D2和(f)具有发热量为E2J / g的这样的高温吸热峰,其中D2和E2具有20-0.020xD2 <= E2 <= 65-0.100xD2。 可以通过将限定在模腔中的多个连续空间中的每一个中填充发泡聚丙烯树脂珠并加热发泡珠以将相应的发泡珠熔合到一体中来制备复合模制品。 至少一个空间用特定的发泡聚丙烯树脂珠填充。

    Composite foamed polypropylene resin molding and method of producing same
    7.
    发明申请
    Composite foamed polypropylene resin molding and method of producing same 有权
    复合发泡聚丙烯树脂成型及其制造方法

    公开(公告)号:US20050056957A1

    公开(公告)日:2005-03-17

    申请号:US10502934

    申请日:2003-03-19

    摘要: A composite foamed polypropylene resin molding including a plurality of sections which are fuse-bonded to each other, at least two of which differ from each other in color, apparent density, composition and/or mechanical strengths, each of which is formed from expanded polypropylene resin beads, and each of which shows a high temperature endothermic peak in a DSC curve thereof. At least one of the sections satisfies conditions (d) to (f) at the same time: (d) to be formed from specific expanded polypropylene resin beads of a base resin having a tensile modulus of at least 1,200 MPa, (e) to have an apparent density D2 of 10-500 g/L, and (f) to have such a high temperature endothermic peak with a calorific of E2 J/g, wherein D2 and E2 have the relationship 20−0.020×D2≦E2. ≦65−0.100×D2. The composite molding may be prepared by filling expanded polypropylene resin beads in each of a plurality of contiguous spaces defined in a mold cavity and heating the expanded beads to fuse-bond respective expanded beads together into a unitary body. At least one of the spaces is filled with the specific expanded polypropylene resin beads.

    摘要翻译: 一种复合发泡聚丙烯树脂模制品,其包括彼此熔合键合的多个部分,其中至少两个在颜色,表观密度,组成和/或机械强度方面彼此不同,每个部分由发泡聚丙烯 树脂珠,其DSC曲线中都显示高温吸热峰。 至少一个部分同时满足条件(d)至(f):(d)由具有至少1200MPa的拉伸模量的基础树脂的特定发泡聚丙烯树脂珠粒形成,(e)至 具有10-500g / L的表观密度D2,(f)具有发热量为E2J / g的高温吸热峰,其中D2和E2的关系为20-0.020xD2 <= E2。 <= 65-0.100xD2。 可以通过将限定在模腔中的多个连续空间中的每一个中填充发泡聚丙烯树脂珠并加热发泡珠以将相应的发泡珠熔合到一体中来制备复合模制品。 至少一个空间用特定的发泡聚丙烯树脂珠填充。

    Expanded polypropylene resin beads and process for the production thereof
    9.
    发明授权
    Expanded polypropylene resin beads and process for the production thereof 失效
    膨胀聚丙烯树脂珠及其制备方法

    公开(公告)号:US07259189B2

    公开(公告)日:2007-08-21

    申请号:US10855633

    申请日:2004-05-28

    IPC分类号: C08J9/16 C08J9/22

    摘要: A process for the production of expanded beads, including kneading a base resin containing a polypropylene resin and having a tensile modulus of at least 1,200 MPa together with a mixture of a coloring agent and a thermoplastic polymer having a tensile modulus lower than that of the base resin to form a kneaded mixture including a matrix of the base resin and a multiplicity of domains dispersed in the matrix and each containing the thermoplastic polymer and the coloring agent. The kneaded mixture is formed into resin particles, then treated with an organic peroxide to modify surfaces of the resin particles therewith. Foaming and expanding of the surface-modified resin particles gives expanded beads having an inside region surrounded by a surface region. The heat of fusion of a high temperature peak of the surface region is lower than that of the inside region.

    摘要翻译: 一种生产发泡珠粒的方法,包括捏合含有聚丙烯树脂的基础树脂和拉伸模量至少为1200MPa的着色剂和热塑性聚合物的混合物,其拉伸模量低于基体的拉伸模量 树脂以形成包含基体树脂的基体和分散在基体中的多个畴并且各自包含热塑性聚合物和着色剂的捏合混合物。 捏合的混合物形成树脂颗粒,然后用有机过氧化物处理以改性树脂颗粒的表面。 表面改性树脂颗粒的发泡和膨胀产生具有由表面区域包围的内部区域的发泡珠粒。 表面区域的高温峰的熔化热低于内部区域的熔融热。

    Expanded polypropylene resin bead and process of producing same
    10.
    发明授权
    Expanded polypropylene resin bead and process of producing same 失效
    膨胀聚丙烯树脂珠及其生产方法

    公开(公告)号:US06956067B2

    公开(公告)日:2005-10-18

    申请号:US10379569

    申请日:2003-03-06

    IPC分类号: C08J9/224 C08L23/10 C08J9/16

    摘要: Expanded, substantially non-crosslinked polypropylene resin beads capable of producing a high rigidity foamed molding at a relatively low temperature. The beads are produced by a process including a step of dispersing substantially non-crosslinked polypropylene resin particles in a dispersing medium containing an organic peroxide to obtain a dispersion, a step of heating the dispersion to decompose the organic peroxide and to modify the surface of the surface-modified polypropylene resin particles, and a step of expanding the non-crosslinked, surface-modified polypropylene resin particles using a blowing agent.