Abstract:
An analysis system 10 includes: an operational data acquisition unit 11 that acquires operational data including an operational state of a production line 20; a product information acquisition unit 13 that acquires a state of a product manufactured in the production line and outputs the state of the product as product information; a production state analyzer 12 that obtains a predetermined physical quantity of the product on a basis of the operational data acquired by the operational data acquisition unit 11 and outputs the predetermined physical quantity as information on the physical quantity; and a correlation analyzer 14 that performs analysis of a correlation between the information on the physical quantity and the product information.
Abstract:
A non-oriented electrical steel sheet having a high magnetic flux density and a low iron loss includes C: not more than 0.01 mass %, Si: 1.3-5.0 mass %, Mn: 0.001-3 mass %, sol. Al: not more than 0.004 mass %, P: 0.03-0.20 mass %, S: not more than 0.005 mass %, N: not more than 0.005 mass %, Ti: more than 0.0020 mass % but not more than 0.1 mass %, and further contains one or more selected from Sn: 0.001-0.1 mass %, Sb: 0.001-0.1 mass %, Ca: 0.001-0.02 mass % and Mg: 0.001-0.02 mass % as required.
Abstract:
A batch annealing furnace includes a coil support base on which an end face of a coil is mounted and that supports the coil with an axis of the coil being upright, an inner cover that covers an entire body of the coil mounted on the coil support base, and a cooling pipe that extends downward from the upper part of the inner cover to a cavity of the inner peripheral part of the coil mounted on the coil support base and cools the coil from the inner surface side by passing a coolant through the inside of the cooling pipe.
Abstract:
A non-oriented electrical steel sheet has a high magnetic flux density and a low iron loss contains in terms of mass %, C: not more than 0.010%, Si: 1-4%, Mn: 0.05-3%, Al: not more than 0.004%, N: not more than 0.005%, P: 0.03-0.20%, S: not more than 0.01% and Se: not more than 0.002% or contains in terms of mass, C: not more than 0.01%, Si: 1-4%, Mn: 0.05-3%, Al: not more than 0.004%, N: not more than 0.005%, P: 0.03-0.20%, S: not more than 0.01%, Se: not more than 0.003% and further contains one or two selected from Sn: 0.001-0.1 mass % and Sb: 0.001-0.1 mass %.
Abstract:
A top-blowing lance nozzle is configured to freely switch an adequate expansion condition so as to control an oxygen-blowing amount and a jetting velocity independently of each other without requiring a plurality of lance nozzles or a mechanically movable part. A lance nozzle is configured to blow refining oxygen to molten iron charged in a reaction vessel while a gas is blown from a top-blowing lance to the molten iron. One or more blowing holes for blowing a working gas are on an inner wall side surface of the nozzle, at a site where the lance nozzle has a minimum cross-sectional area in a nozzle axis direction or at a neighboring site of the site.
Abstract:
A non-oriented electrical steel sheet having a high magnetic flux density and a low anisotropy contains C: not more than 0.01 mass %, Si: 1-4 mass %, Mn: 0.05-3 mass %, P: 0.03-0.2 mass %, S: not more than 0.01 mass %, Al: not more than 0.004 mass %, N: not more than 0.005 mass %, As: not more than 0.003 mass %, and preferably further contains one or two of Sb: 0.001-0.1 mass % and Sn: 0.001-0.1 mass % or further contains one or two of Ca: 0.001-0.005 mass % and Mg: 0.001-0.005 mass %.
Abstract:
A non-oriented electrical steel sheet has a chemical composition that includes C: not more than 0.005%, Si: 1.5-4%, Mn: 1.0-5%, P: not more than 0.1%, S: not more than 0.005%, Al: not more than 3 mass %, N: not more than 0.005 mass %, Bi: not more than 0.0030% as mass % and the remainder being Fe and inevitable impurities or a chemical composition containing C: not more than 0.005%, Si: 1.5-4%, Mn: 1.0-5%, P: not more than 0.1%, S: not more than 0.005%, Al: not more than 3 mass %, N: not more than 0.005 mass %, Bi: not more than 0.0030% and further one or two of Ca: 0.0005-0.005% and Mg: 0.0002-0.005%, and is stably excellent in the high-frequency iron loss property even if a great amount of Mn is included.
Abstract:
A non-oriented electrical steel sheet is obtained by subjecting a slab containing C: not more than 0.005 mass %, Si: 1.0-5.0 mass %, Mn: 0.04-3.0 mass %, sol. Al: not more than 0.005 mass %, P: 0.03-0.2 mass %, S: not more than 0.005 mass %, N: not more than 0.005 mass %, B: not more than 0.001 mass %, and Se: not more than 0.001 mass % and satisfying sol. Al+C+5B+5Se≤0.005 mass % to hot rolling, cold rolling and finish annealing. A sheet temperature at the outlet side of the rolling machine in at least one pass of the final cold rolling is set to a range of 100-300° C. to provide S/2M of not less than 1.0 and S/5C of not less than 1.0 when X-ray intensity ratios of {001} , {111} and {001} in a central layer in a thickness direction are S, M and C, respectively.
Abstract:
A non-oriented electrical steel sheet having a high magnetic flux density and a low iron loss at not only a commercial frequency but also a high frequency zone, which has a chemical composition including C: not more than 0.0050 mass %, Si: more than 1.5 mass % but not more than 5.0 mass %, Mn: not more than 0.10 mass %, sol. Al: not more than 0.0050 mass, P: more than 0.040 mass % but not more than 0.2 mass %, S: not more than 0.0050 mass %, N: not more than 0.0040 mass % and Ca: 0.001-0.01 mass % and the remainder being Fe and inevitable impurities and a compositional ratio of CaO in oxide-based inclusions existing in a steel sheet of not less than 0.4 and/or a compositional ratio of Al2O3 of not less than 0.3, and a hot rolled steel sheet used as a raw steel material thereof.
Abstract:
A non-oriented electrical steel sheet has a chemical composition including C: not more than 0.005 mass %, Si: 1.5-4 mass %, Mn: 1-5 mass %, P: not more than 0.1 mass %, S: not more than 0.005 mass %, Al: not more than 3 mass %, N: not more than 0.005 mass %, Pb: not more than 0.001 mass % and the remainder being Fe and inevitable impurities or a chemical composition including C: not more than 0.005 mass %, Si: 1.5-4 mass %, Mn: 1-5 mass %, P: not more than 0.1 mass %, S: not more than 0.005 mass %, Al: not more than 3 mass %, N: not more than 0.005 mass %, Pb: not more than 0.0020 mass % and further one or two of Ca: 0.0005-0.007 mass % and Mg: 0.0002-0.005 mass %, and has a stable and excellent high-frequency iron loss property even when Mn content is high.