Abstract:
An antireflection film is provided and includes at least one layer containing fine pores. When a surface portion of the antireflection film comes into contact with water for 15 minutes and then the water is wiped away, the surface portion has a chromaticity change ΔE of 0.45 or less, the chromaticity change ΔE being a chromaticity change in a CIE1976 L*a*b* color space and measured under a standard light source D65.
Abstract translation:提供防反射膜,并且包括至少一层含有细孔的层。 当防反射膜的表面部分与水接触15分钟,然后水被擦去时,表面部分的色度变化&Dgr; E为0.45以下,色度变化&Dgr; E为色度变化 CIE1976 L * a * b *颜色空间,并在标准光源D65下测量。
Abstract:
A silver halide color photographic light-sensitive material, having at least one each of blue-, green-, and red-sensitive emulsion layers containing yellow, magenta, and cyan couplers, respectively, on a support; wherein said blue-sensitive emulsion layer contains at least one coupler of formula (I); and wherein the light-sensitive material satisfies expression a-1) and/or b-1): wherein, Q forms a 5- to 7-membered ring with the —N═C—N(R1)-; R1 and R2 each are a substituent; m is 0 to 5; and X is a hydrogen atom, or a coupling split-off group; 0.5≦Dmax(UV)/Dmin(UV)≦1.1 a-1) wherein Dmax(UV)/Dmin(UV) is the smallest of the value in a wavelength range of 340 to 450 nm; 1300≦(B−C)/A≦20000 b-1) wherein B is yellow Dmax, C is yellow Dmin; and A is an amount mol/m2 of the coupler of formula (I).
Abstract:
An antireflection film is provided and includes at least one layer containing fine pores. When a surface portion of the antireflection film comes into contact with water for 15 minutes and then the water is wiped away, the surface portion has a chromaticity change ΔE of 0.45 or less, the chromaticity change ΔE being a chromaticity change in a CIE1976 L*a*b* color space and measured under a standard light source D65.
Abstract translation:提供防反射膜,并且包括至少一层含有细孔的层。 当防反射膜的表面部分与水接触15分钟,然后擦去水时,表面部分的色度变化ΔE为0.45以下,色度变化量DeltaE为CIE1976L *的色度变化, a * b *颜色空间,并在标准光源D65下测量。
Abstract:
A silver halide color photographic light-sensitive material, having at least one each of blue-, green-, and red-sensitive emulsion layers containing yellow, magenta, and cyan couplers, respectively, on a support; wherein said blue-sensitive emulsion layer contains at least one coupler of formula (I); and wherein the light-sensitive material satisfies expression a-1) and/or b-1): wherein, Q forms a 5- to 7-membered ring with the —N═C—N(R1)-; R1 and R2 each are a substituent; m is 0 to 5; and X is a hydrogen atom, or a coupling split-off group; 0.5≦Dmax(UV)/Dmin(UV)≦1.1 a-1): wherein Dmax(UV)/Dmin(UV) is the smallest of the value in a wavelength range of 340 to 450 nm; 1300≦(B−C)/A≦20000 b-1): wherein B is yellow Dmax, C is yellow Dmin; and A is an amount mol/m2 of the coupler of formula (I).
Abstract:
A silver halide color photographic light-sensitive material, having at least one each of blue-, green-, and red-sensitive emulsion layers containing yellow, magenta, and cyan couplers, respectively, on a support;wherein said blue-sensitive emulsion layer contains at least one coupler of formula (I); andwherein the light-sensitive material satisfies expression a-1) and/or b-1): wherein, Q forms a 5- to 7-membered ring with the —N═C—N(R1)—; R1 and R2 each are a substituent; m is 0 to 5; and X is a hydrogen atom, or a coupling split-off group; 0.5≦Dmax(UV)/Dmin(UV)≦1.1: a-1) wherein Dmax(UV)/Dmin(UV) is the smallest of the value in a wavelength range of 340 to 450 nm; 1300≦(B−C)/A≦20000: b-1) wherein B is yellow Dmax, C is yellow Dmin; and A is an amount mol/m2 of the coupler of formula (I).
Abstract:
A silver halide color photographic light-sensitive material comprising at least one yellow color developable light-sensitive silver halide emulsion layer, at least one magenta color developable light-sensitive silver halide emulsion layer, and at least one cyan color developable light-sensitive silver halide emulsion layer, each of which is provided on a support: which comprises at least one yellow coupler of formula (I) and at least one cyan coupler of formula (A); wherein Q represents a group of non-metal atoms that form a 5- to 7-membered ring in combination with —N═C—N(R1)-, each of R1 and R2 represents a substituent, m represents an integer of 0 to 5, and X represents a hydrogen atom or a group capable of being split-off upon a coupling reaction; wherein R11 and R12 each represent an alkyl group or an aryl group, J represents an alkylene group, and X represents a hydrogen atom or a group that can split off upon a coupling reaction.
Abstract:
A silver halide color photographic light-sensitive material, having at least one each of blue-, green-, and red-sensitive emulsion layers containing yellow, magenta, and cyan couplers, respectively, on a support; wherein said blue-sensitive emulsion layer contains at least one coupler of formula (I); and wherein the light-sensitive material satisfies expression a-1) and/or b-1): wherein, Q forms a 5- to 7-membered ring with the —N═C—N(R1)—; R1 and R2 each are a substituent; m is 0 to 5; and X is a hydrogen atom, or a coupling split-off group; a-1): 0.5≦Dmax(UV)/Dmin(UV)≦1.1 wherein Dmax(UV)/Dmin(UV) is the smallest of the value in a wavelength range of 340 to 450 nm; b-1): 1300≦(B-C)/A≦20000 wherein B is yellow Dmax, C is yellow Dmin; and A is an amount mol/m2 of the coupler of formula (I).
Abstract:
An object of the present invention is to provide an optical film assured of reflectance low enough to suppress glaring and excellent in the scratch resistance, antifouling property and antistatic property, and another object is to provide a polarizing plate and a display, using such an antireflection film. These objects can be attained by an optical film, particularly, an antireflection film, containing a support and a thin film layer formed by coating a composition containing fine particles and a binder, in which the SP value ((B/A)×100)) which is a ratio of an average particle filling factor (B) in the region of 30% of the film thickness on the upper side opposite the support to an average particle filling factor (A) in the entirety of the thin film layer is 90% or less; and a polarizing plate and an image display, using the optical film.
Abstract:
An object of the present invention is to provide an optical film assured of reflectance low enough to suppress glaring and excellent in the scratch resistance, antifouling property and antistatic property, and another object is to provide a polarizing plate and a display, using such an antireflection film. These objects can be attained by an optical film, particularly, an antireflection film, containing a support and a thin film layer formed by coating a composition containing fine particles and a binder, in which the SP value ((B/A)×100)) which is a ratio of an average particle filling factor (B) in the region of 30% of the film thickness on the upper side opposite the support to an average particle filling factor (A) in the entirety of the thin film layer is 90% or less; and a polarizing plate and an image display, using the optical film.
Abstract:
A silver halide color photographic light-sensitive material comprising at least one yellow color developable light-sensitive silver halide emulsion layer, at least one magenta color developable light-sensitive silver halide emulsion layer, and at least one cyan color developable light-sensitive silver halide emulsion layer, each of which is provided on a support: which comprises at least one yellow coupler of formula (I) and at least one cyan coupler of formula (A); wherein Q represents a group of non-metal atoms that form a 5- to 7-membered ring in combination with —N═C—N(R1)-, each of R1 and R2 represents a substituent, m represents an integer of 0 to 5, and X represents a hydrogen atom or a group capable of being split-off upon a coupling reaction; wherein R11 and R12 each represent an alkyl group or an aryl group, J represents an alkylene group, and X represents a hydrogen atom or a group that can split off upon a coupling reaction.