FLUORESCENT LAMP
    1.
    发明申请
    FLUORESCENT LAMP 审中-公开
    日光灯

    公开(公告)号:US20100277057A1

    公开(公告)日:2010-11-04

    申请号:US12835618

    申请日:2010-07-13

    IPC分类号: H01J63/04

    CPC分类号: H01J61/44 H01J61/35

    摘要: The present invention provides a fluorescent lamp, comprising: a glass bulb; mercury that is enclosed within the glass bulb, an amount of the mercury being from 2.2 μg/cm3 to 8.8 μg/cm3; a rare gas that is enclosed within the glass bulb; an electrode that is attached to the glass bulb; a protective layer that is formed on an inside surface of the glass bulb, and includes metal oxide particles and at least 50 wt % of silica, a thickness of the protective layer being from 0.5 μm to 5.0 μm; and a phosphor layer that is formed over the protective layer.

    摘要翻译: 本发明提供一种荧光灯,包括:玻璃灯泡; 封闭在玻璃灯泡内的汞,一定量的汞为2.2μg/ cm3至8.8μg/ cm3; 封闭在玻璃灯泡内的稀有气体; 连接到玻璃灯泡的电极; 保护层,其形成在玻璃泡的内表面上,并且包括金属氧化物颗粒和至少50重量%的二氧化硅,所述保护层的厚度为0.5μm至5.0μm; 以及形成在保护层上的荧光体层。

    Fluorescent lamp
    2.
    发明申请
    Fluorescent lamp 审中-公开
    日光灯

    公开(公告)号:US20050285537A1

    公开(公告)日:2005-12-29

    申请号:US11165396

    申请日:2005-06-23

    IPC分类号: H01J61/35 H01J61/44 H01J65/04

    CPC分类号: H01J61/44 H01J61/35

    摘要: The present invention provides a fluorescent lamp, comprising: a glass bulb; mercury that is enclosed within the glass bulb, an amount of the mercury being from 2.2 μg/cm3 to 8.8 μg/cm3; a rare gas that is enclosed within the glass bulb; an electrode that is attached to the glass bulb; a protective layer that is formed on an inside surface of the glass bulb, and includes metal oxide particles and at least 50 wt % of silica, a thickness of the protective layer being from 0.5 μm to 5.0 μm; and a phosphor layer that is formed over the protective layer.

    摘要翻译: 本发明提供一种荧光灯,包括:玻璃灯泡; 封闭在玻璃灯泡内的汞,一定量的汞为2.2mug / cm 3至8.8mug / cm 3; 封闭在玻璃灯泡内的稀有气体; 连接到玻璃灯泡的电极; 形成在玻璃管的内表面上的保护层,包括金属氧化物粒子和至少50重量%的二氧化硅,保护层的厚度为0.5〜5.0μm; 以及形成在保护层上的荧光体层。

    Fluorescent lamp with glass tube and protective layer, method for producing the same, and lighting system
    3.
    发明授权
    Fluorescent lamp with glass tube and protective layer, method for producing the same, and lighting system 有权
    具有玻璃管和保护层的荧光灯,其制造方法和照明系统

    公开(公告)号:US07986082B2

    公开(公告)日:2011-07-26

    申请号:US11914635

    申请日:2006-05-29

    IPC分类号: H01J1/62

    CPC分类号: H01J61/35 H01J9/20

    摘要: A fluorescent lamp according to the present invention includes: a glass tube 1 in which mercury and a rare gas are enclosed; a protective film 3 that is attached so as to cover an inner face of the glass tube 1; and a phosphor layer 4 that is laminated on the protective film 3. The protective film 3 has a thickness of 0.5 μm to 3 μm. Further, the protective film 3 is formed of inorganic particles and has a volume ratio of 0.1 to 0.5. Preferably, the inorganic particles are of at least one selected from the group consisting of aluminum oxide, silicon dioxide, magnesium oxide, zinc oxide, titanium oxide, cerium oxide, yttrium oxide, and calcium halophosphate.

    摘要翻译: 根据本发明的荧光灯包括:包围汞和稀有气体的玻璃管1; 安装以覆盖玻璃管1的内表面的保护膜3; 以及层叠在保护膜3上的荧光体层4.保护膜3的厚度为0.5μm〜3μm。 此外,保护膜3由无机粒子形成,体积比为0.1〜0.5。 优选地,无机颗粒是选自氧化铝,二氧化硅,氧化镁,氧化锌,氧化钛,氧化铈,氧化钇和卤代磷酸钙中的至少一种。

    FLUORESCENT LAMP AND PROCESS FOR PRODUCING THE SAME, AND ILLUMINATOR
    4.
    发明申请
    FLUORESCENT LAMP AND PROCESS FOR PRODUCING THE SAME, AND ILLUMINATOR 有权
    荧光灯及其制造方法和照明器

    公开(公告)号:US20090079325A1

    公开(公告)日:2009-03-26

    申请号:US11914635

    申请日:2006-05-29

    IPC分类号: H01J61/35 H01J9/20

    CPC分类号: H01J61/35 H01J9/20

    摘要: A fluorescent lamp according to the present invention includes: a glass tube 1 in which mercury and a rare gas are enclosed; a protective film 3 that is attached so as to cover an inner face of the glass tube 1; and a phosphor layer 4 that is laminated on the protective film 3. The protective film 3 has a thickness of 0.5 μm to 3 μm. Further, the protective film 3 is formed of inorganic particles and has a volume ratio of 0.1 to 0.5. Preferably, the inorganic particles are of at least one selected from the group consisting of aluminum oxide, silicon dioxide, magnesium oxide, zinc oxide, titanium oxide, cerium oxide, yttrium oxide, and calcium halophosphate.

    摘要翻译: 根据本发明的荧光灯包括:包围汞和稀有气体的玻璃管1; 安装以覆盖玻璃管1的内表面的保护膜3; 以及层叠在保护膜3上的荧光体层4.保护膜3的厚度为0.5μm〜3μm。 此外,保护膜3由无机粒子形成,体积比为0.1〜0.5。 优选地,无机颗粒是选自氧化铝,二氧化硅,氧化镁,氧化锌,氧化钛,氧化铈,氧化钇和卤代磷酸钙中的至少一种。

    Tractor transmission
    6.
    发明授权
    Tractor transmission 有权
    拖拉机传动

    公开(公告)号:US06446521B1

    公开(公告)日:2002-09-10

    申请号:US09652988

    申请日:2000-08-31

    IPC分类号: F16H5904

    摘要: A tractor transmission includes a change speed mechanism, a shift lever (30) for shifting the change speed mechanism, a super-reduction mechanism (16) for decelerating and outputting power inputted thereto, the super-reduction mechanism having a larger reduction ratio than the change speed mechanism, and an overdrive mechanism (45) for accelerating and outputting power inputted thereto. A single switching device (29) is provided for operating both the super-reduction mechanism and overdrive mechanism. The switching device is shiftable, when the super-reduction mechanism is in neutral, from a state of operating the super-reduction mechanism to a state of operating the overdrive mechanism.

    摘要翻译: 拖拉机变速器包括变速机构,用于换档机构的变速杆(30),用于减速输出输入动力的超减速机构(16),该超减速机构的减速比大于 变速机构,以及用于加速输出输入功率的过驱动机构45。 提供单个开关装置(29),用于操作超减速机构和过驱动机构。 当超级减速机构处于中立状态时,从超级减速机构的运转状态到运转超速机构的状态,切换装置可以移动。

    Method for producing .alpha.-form silicon nitride fine powders
    7.
    发明授权
    Method for producing .alpha.-form silicon nitride fine powders 失效
    生产α型氮化硅细粉的方法

    公开(公告)号:US4590053A

    公开(公告)日:1986-05-20

    申请号:US747851

    申请日:1985-06-24

    IPC分类号: C01B21/068 C04B35/584

    摘要: A method for producing a high-grade fine powder of .alpha.-form silicon nitride (.alpha.-Si.sub.3 N.sub.4) for use as sintered bodies excellent in heat-stability and mechanical strength which comprises heat-treating, in an atmosphere containing nitrogen, a mixture prepared by adding additive:a mixture of at least one of Mg, Ca, and compounds thereof with 0.01-1 part by weight of silicon nitride powder,in a total amount of 0.001-0.1 part by weight calculated in terms of elemental weight(s) of Mg or/and Ca, and 1 part or less by weight of silicon nitride powder, to 1 part by weight of silicon oxide powder and 0.4-4 parts by weight of carbon powder.

    摘要翻译: 一种制造用作热稳定性和机械强度优异的烧结体的α型氮化硅(α-Si 3 N 4)的高级细粉末的方法,包括在含氮气氛中热处理由 添加添加剂:Mg,Ca及其化合物中的至少一种与0.01-1重量份氮化硅粉末的混合物,其总量为0.001-0.1重量份,以元素重量 Mg或/和Ca,1重量份或更少的氮化硅粉末,至1重量份氧化硅粉末和0.4-4重量份碳粉末。