Abstract:
An image recording material which has a support and an image recording layer containing a crystalline polymer and an amorphous polymer on at least one surface of the support, wherein the image recording layer has a storage elastic modulus G′ at 100° C. of 1×102 Pa to 1×105 Pa during a temperature increase at 5° C./min, a storage elastic modulus G′ at 60° C. of 1×106 Pa or more during a temperature decrease at 5° C./min and a temperature difference of 18° C. or less between a temperature at which the storage elastic modulus G′ during a temperature increase at 5° C./min reaches 1×105 Pa and a temperature at which the storage elastic modules G′ during a temperature decrease at 5° C./min reaches 1×105 Pa, upon measurement of viscoelasticity by using a rheometer of plate-to-plate distance: 1.5 mm, diameter: 20 mm.
Abstract:
A liquid crystalline composition is disclosed. The composition comprises at least one liquid-crystal compound and at least one fluoroaliphatic group-containing polymer of a formula (1-1). In the formula, i and j each indicate an integer equal to or more than 1; M represents k types of repetitive units each derived from an ethylenic unsaturated monomer (k indicates an integer equal to or more than 1); a, b and c each mean a mass percentage indicating a polymerization ratio; R11 and R12 each represent a hydrogen atom or a methyl group; X1 and X2 each represent an oxygen atom, a sulfur atom or —N(R13)—; R13 represents a hydrogen atom or an alkyl group having from 1 to 4 carbon atoms; m1 and m2 each indicate an integer of from 1 to 6; and n1 indicates an integer of from 0 to 3.
Abstract translation:公开了液晶组合物。 组合物包含至少一种液晶化合物和至少一种式(1-1)的含氟脂族基团的聚合物。 在该式中,i和j分别表示1以上的整数。 M表示各自衍生自烯属不饱和单体的重复单元的k种(k表示1以上的整数)。 a,b和c各自表示表示聚合比的质量百分比; R 11和R 12各自表示氢原子或甲基; X 1和X 2各自表示氧原子,硫原子或-N(R 13) - ; R13表示氢原子或碳原子数为1〜4的烷基; m1和m2各自表示1至6的整数; n1表示0〜3的整数。
Abstract:
The present invention provides an electrophotographic image receiving sheet including a support, and at least two toner image receiving layers formed over at least one surface of the support, wherein a mixture mass ratio M of a crystalline polymer and an amorphous polymer in each of the toner image receiving layers is defined as [A/(A+B)], where A represents a mass of the crystalline polymer (g), and B represents a mass of the amorphous polymer (g), and a mixture mass ratio M1 of the outermost toner image receiving layer which is located farthest from the support, and a mixture mass ratio M2 of the highest inner toner image receiving layer, which has the highest mixture mass ratio among the inner toner image receiving layers located under the outermost toner image receiving layer, satisfy the relation: M1
Abstract:
A liquid crystalline composition is disclosed. The composition comprises at least one liquid-crystal compound and at least one fluoroaliphatic group-containing polymer of a formula (1-1). In the formula, i and j each indicate an integer equal to or more than 1; M represents k types of repetitive units each derived from an ethylenic unsaturated monomer (k indicates an integer equal to or more than 1); a, b and c each mean a mass percentage indicating a polymerization ratio; R11 and R12 each represent a hydrogen atom or a methyl group; X1 and X2 each represent an oxygen atom, a sulfur atom or —N(R13)—; R13 represents a hydrogen atom or an alkyl group having from 1 to 4 carbon atoms; m1 and m2 each indicate an integer of from 1 to 6; and n1 indicates an integer of from 0 to 3.
Abstract translation:公开了液晶组合物。 组合物包含至少一种液晶化合物和至少一种式(1-1)的含氟脂族基团的聚合物。 在该式中,i和j分别表示1以上的整数。 M表示各自衍生自烯属不饱和单体的重复单元的k种(k表示1以上的整数)。 a,b和c各自表示表示聚合比的质量百分比; R 11和R 12各自表示氢原子或甲基; X 1和X 2各自表示氧原子,硫原子或-N(R 13) - ; R 13表示氢原子或具有1至4个碳原子的烷基; m1和m2各自表示1至6的整数; n1表示0〜3的整数。
Abstract:
A luminescent material composed of the polymer of the organic silicon compound represented by the following general formula (1): Chemical Formula 1 [where X is an organic molecule which emits fluorescence or phosphorescence; R1 is a lower alkoxy group, a hydroxyl group, an allyl group, an ester group, or halogen atoms; R2 is a lower alkyl group or a hydrogen atom; n is an integer of 1 to 3; and m is an integer of 1 to 4].
Abstract translation:由以下通式(1)表示的有机硅化合物的聚合物组成的发光材料:化学式1 [其中X是发射荧光或磷光的有机分子; R 1是低级烷氧基,羟基,烯丙基,酯基或卤素原子; R 2是低级烷基或氢原子; n为1〜3的整数。 m为1〜4的整数]。
Abstract:
The invention provides an image forming method, comprising transferring a toner image to an electrophotographic recording sheet, layering the electrophotographic recording sheet on a fixing belt and heating and pressing the sheet, and cooling the electrophotographic recording sheet and separating the sheet from the fixing belt. The electrophotographic recording sheet comprises a support comprising cellulose pulp-containing base paper and a toner image-receiving layer comprising a thermoplastic resin disposed on the support. A shrinkage percentage of the electrophotographic recording sheet in a CD direction in the heating step is 1.3% or less. The support preferably further comprises either a polyolefin-containing layer or a coating that contains at least one selected from the group consisting of kaolin, a pigment, a resin, a rubber latex, or a polymer material and that is provided on one or both surfaces of the base paper.
Abstract:
An electrophotographic image-receiving sheet which includes a support, a toner-receiving layer which contains thermoplastic resin. The fixing belt electrophotographic sheet has an optimized separation force at a surface of the electrophotographic image-receiving sheet from the toner-receiving layer. Having a highly improved long-run properties, the fixing belt electrophotographic sheet realizes a stable paper feed without offset, and provides a good quality image with rich photographic features.
Abstract:
In the image forming process of the present invention wherein a toner is fixed on an electrophotographic image-receiving sheet using a belt fixing and smoothing device, the relationship among the temperature of a heating and fixing roller, the melting point of a toner wax, and the glass transition point of a toner binder, the relationship among the temperature of a heating and fixing roller, the melting point of a wax in the image-receiving layer, and the glass transition point of a binder in the image-receiving layer, and the relationship between the polar components of surface free energy of the toner-image-receiving layer before and after image fixing are optimized. The present invention is to prevent offset in the toner and the toner-image-receiving layer of the electrophotographic image-receiving sheet upon releasing of the belt and to avoid deterioration in image quality especially in operation over the long run.
Abstract:
A method of producing a photographic polyester laminate support having a laminate of layers of at least two kinds of polyesters can provide low formation of scratches in a camera and a curl in the film's width direction. In the support, the glass transition temperature (Tg) of each polyester of the laminate is within the range of from 90.degree. C. to 200.degree. C. and the laminate is subjected to heat-fixing in a temperature range as defined by formula (1):Heat-fixing temperature (.degree.C.)=(Tm(L)-50) to (Tm(H)-10)formula (1)wherein Tm(H)(.degree.C.) means the highest melting temperature of polyesters that constitute the laminate support, and Tm(L)(.degree.C.) means the lowest melting temperature of polyesters that constitute the laminate support.
Abstract:
A polyester film containing a polyester resin having an intrinsic viscosity IV of from 0.73 to 0.9 dL/g in which the polyester film has a specific heat change at 85° C. to 135° C. (ΔCp) of from 0.06 to 0.1 J/g, has an excellent weather resistance, a good planar surface state and a low thermal shrinkage.