COATINGS FOR USE IN HIGH HUMIDITY CONDITIONS
    1.
    发明申请
    COATINGS FOR USE IN HIGH HUMIDITY CONDITIONS 有权
    涂料在高湿度条件下使用

    公开(公告)号:US20140179859A1

    公开(公告)日:2014-06-26

    申请号:US13721973

    申请日:2012-12-20

    IPC分类号: C09D133/04

    摘要: The present invention is directed to a coating composition comprising a vinyl acrylic copolymer latex wherein said copolymer latex has a water contact angle of about 60° or higher on the dried latex film surface, wherein said copolymer latex further has a specific water vapor permeability of about 0.5 mg/cm2/mm/24 hr. The invention is also directed to the copolymer latex itself. Further, the invention is a method of improving a coating's ability to withstand a high humidity environment comprising adding a vinyl acrylic copolymer latex to the coating composition wherein said copolymer latex has a water contact angle of about 60° or higher on the dried latex film surface, and wherein said copolymer latex further has a specific water vapor permeability of about 0.5 mg/cm2/mm/24 hr.

    摘要翻译: 本发明涉及包含乙烯基丙烯酸共聚物胶乳的涂料组合物,其中所述共聚物胶乳在干燥的胶乳膜表面上具有约60°或更高的水接触角,其中所述共聚物胶乳进一步具有约为 0.5mg / cm 2 / mm 2/24小时。 本发明还涉及共聚物胶乳本身。 此外,本发明是一种提高涂层承受高湿度环境的能力的方法,包括向涂料组合物中加入乙烯基丙烯酸共聚物胶乳,其中所述共聚物胶乳在干燥的胶乳膜表面上具有约60°或更高的水接触角 ,并且其中所述共聚物胶乳的特定水蒸气透过率为约0.5mg / cm 2 / mm / 24小时。

    Coatings for use in high humidity conditions
    3.
    发明授权
    Coatings for use in high humidity conditions 有权
    用于高湿度条件下的涂料

    公开(公告)号:US08907002B2

    公开(公告)日:2014-12-09

    申请号:US13721973

    申请日:2012-12-20

    IPC分类号: C08K3/34 C08F8/30 C09D133/04

    摘要: The present invention is directed to a coating composition comprising a vinyl acrylic copolymer latex wherein said copolymer latex has a water contact angle of about 60° or higher on the dried latex film surface, wherein said copolymer latex further has a specific water vapor permeability of about 0.5 mg/cm2/mm/24 hr. The invention is also directed to the copolymer latex itself. Further, the invention is a method of improving a coating's ability to withstand a high humidity environment comprising adding a vinyl acrylic copolymer latex to the coating composition wherein said copolymer latex has a water contact angle of about 60° or higher on the dried latex film surface, and wherein said copolymer latex further has a specific water vapor permeability of about 0.5 mg/cm2/mm/24 hr.

    摘要翻译: 本发明涉及包含乙烯基丙烯酸共聚物胶乳的涂料组合物,其中所述共聚物胶乳在干燥的胶乳膜表面上具有约60°或更高的水接触角,其中所述共聚物胶乳进一步具有约为 0.5mg / cm 2 / mm 2/24小时。 本发明还涉及共聚物胶乳本身。 此外,本发明是一种提高涂层承受高湿度环境的能力的方法,包括向涂料组合物中加入乙烯基丙烯酸共聚物胶乳,其中所述共聚物胶乳在干燥的胶乳膜表面上具有约60°或更高的水接触角 ,并且其中所述共聚物胶乳的特定水蒸气透过率为约0.5mg / cm 2 / mm / 24小时。

    Latex Based Open-Time Extenders for Low VOC Paints
    5.
    发明申请
    Latex Based Open-Time Extenders for Low VOC Paints 有权
    基于乳胶的低挥发性有机油涂料的开放式增量剂

    公开(公告)号:US20090227705A1

    公开(公告)日:2009-09-10

    申请号:US12042841

    申请日:2008-03-05

    IPC分类号: C09D5/16 C08L25/10

    摘要: The present invention relates to paint extenders or open-time extenders, which are mixed with an architectural coating, such as aqueous latex paints, to increase the coating's open time. The open-time extender comprises acrylic or vinyl latex particles having a mean diameter of less than about 150 nm, and at least one crosslinkable monomer that can crosslink the latex particles in the open-time extender to the latex particles in the architectural coating at ambient conditions. The open-time extender also comprises water and the total solid content of the open-time extender is less than about 15% by weight.

    摘要翻译: 本发明涉及涂料增量剂或开放式增量剂,其与建筑涂料如水性乳胶漆混合,以增加涂料的开放时间。 开放时间延长剂包括平均直径小于约150nm的丙烯酸或乙烯基胶乳颗粒,以及至​​少一种可交联单体,其可将开放时间延长剂中的胶乳颗粒与环境中的建筑涂料中的胶乳颗粒交联 条件。 开放式增量剂还包含水,而开放时间增量剂的总固体含量小于约15重量%。

    Latex based open-time extenders for low VOC paints
    7.
    发明授权
    Latex based open-time extenders for low VOC paints 有权
    乳胶为基础的低VOC涂料的开放时间延长剂

    公开(公告)号:US08034871B2

    公开(公告)日:2011-10-11

    申请号:US12042841

    申请日:2008-03-05

    IPC分类号: C08L31/00 C08L25/10 C09D5/16

    摘要: The present invention relates to paint extenders or open-time extenders, which are mixed with an architectural coating, such as aqueous latex paints, to increase the coating's open time. The open-time extender comprises acrylic or vinyl latex particles having a mean diameter of less than about 150 nm, and at least one crosslinkable monomer that can crosslink the latex particles in the open-time extender to the latex particles in the architectural coating at ambient conditions. The open-time extender also comprises water and the total solid content of the open-time extender is less than about 15% by weight.

    摘要翻译: 本发明涉及涂料增量剂或开放式增量剂,其与建筑涂料如水性乳胶漆混合,以增加涂料的开放时间。 开放时间延长剂包括平均直径小于约150nm的丙烯酸或乙烯基胶乳颗粒,以及至​​少一种可交联单体,其可将开放时间延长剂中的胶乳颗粒与环境中的建筑涂料中的胶乳颗粒交联 条件。 开放式增量剂还包含水,而开放时间增量剂的总固体含量小于约15重量%。

    Latex for low VOC paint having improved block resistance, open time and water-softening resistance
    8.
    发明申请
    Latex for low VOC paint having improved block resistance, open time and water-softening resistance 审中-公开
    具有改善阻块性,开放时间和耐水软化性的低VOC涂料的乳胶

    公开(公告)号:US20080058473A1

    公开(公告)日:2008-03-06

    申请号:US11513859

    申请日:2006-08-31

    IPC分类号: C08F8/00

    摘要: The invention is directed to latex compositions comprising sequentially designed polymer having a first stage, a second stage and a third stage corresponding to a seed, a core and a shell. The latex polymer is suitable for aqueous low volatile organic compounds (“VOC”) paint (less than 50 g/L) with good block resistance, improved open time and increased water softening resistance. To attain good block resistance, the seed and the core contain monomers that form polymers with relatively harder characteristics and higher glass transition temperature (“Tg”) while the shell contains monomers that form polymers with softer characteristics and lower Tg. To gain improved open time, the latex polymer contains suitable level of hydrophilic monomers necessary to hold water. To achieve water softening resistance, hydrophobic monomers are grafted on hydrophilic portions of the shell or the core layers. The invention is also directed to the process of making the latex by a sequential emulsion polymerization.

    摘要翻译: 本发明涉及包含依次设计的聚合物的胶乳组合物,其具有对应于种子,核和壳的第一阶段,第二阶段和第三阶段。 胶乳聚合物适用于低挥发性有机化合物(“VOC”)油漆(小于50g / L),具有良好的耐粘连性,改善的开放时间和增加的耐水软化性。 为了获得良好的耐阻断性,种子和芯包含形成具有较硬特性和较高玻璃化转变温度(“T”g“)的聚合物的单体,而壳包含形成具有较软特性的聚合物的单体, 较低的T 。 为了获得改善的开放时间,胶乳聚合物含有合适水平的保持水所需的亲水单体。 为了获得耐水软化性,将疏水性单体接枝在壳或芯层的亲水部分上。 本发明还涉及通过连续乳液聚合制备胶乳的方法。