USE OF A STEREOISOMER MIXTURE OF DIAMINOMETHYLCYCLOHEXANE AS A HARDENER FOR EPOXY RESINS
    1.
    发明申请
    USE OF A STEREOISOMER MIXTURE OF DIAMINOMETHYLCYCLOHEXANE AS A HARDENER FOR EPOXY RESINS 有权
    使用作为环氧树脂硬化剂的二氨基甲酰氯的立体异构体混合物

    公开(公告)号:US20120226017A1

    公开(公告)日:2012-09-06

    申请号:US13496993

    申请日:2010-09-20

    IPC分类号: C08G59/02 C09K3/00

    CPC分类号: C08G59/5026 C08L63/00

    摘要: The present invention provides a composition which comprises at least one epoxy resin and a mixture comprising the 7 stereoisomers of diaminomethylcyclohexane in very specific ratios relative to one another, a process for preparing the composition, the use of the composition for producing hardened epoxides, adhesives, composite materials and moldings, a mixture comprising the 7 stereoisomers of diaminomethylcyclohexane in the specific ratios, and the use of this mixture for producing the composition.

    摘要翻译: 本发明提供一种组合物,其包含至少一种环氧树脂和包含二氨基甲基环己烷的7种立体异构体的混合物,其相对于彼此具有非常特定的比例,制备该组合物的方法,该组合物用于生产硬化环氧化物,粘合剂, 复合材料和模制品,以特定比例包含二氨基甲基环己烷的7种立体异构体的混合物,以及该混合物用于制备组合物的用途。

    Use of a stereoisomer mixture of diaminomethylcyclohexane as a hardener for epoxy resins
    3.
    发明授权
    Use of a stereoisomer mixture of diaminomethylcyclohexane as a hardener for epoxy resins 有权
    使用二氨基甲基环己烷的立体异构体混合物作为环氧树脂的硬化剂

    公开(公告)号:US08828267B2

    公开(公告)日:2014-09-09

    申请号:US13496993

    申请日:2010-09-20

    CPC分类号: C08G59/5026 C08L63/00

    摘要: The present invention provides a composition which comprises at least one epoxy resin and a mixture comprising the 7 stereoisomers of diaminomethylcyclohexane in very specific ratios relative to one another, a process for preparing the composition, the use of the composition for producing hardened epoxides, adhesives, composite materials and moldings, a mixture comprising the 7 stereoisomers of diaminomethylcyclohexane in the specific ratios, and the use of this mixture for producing the composition.

    摘要翻译: 本发明提供一种组合物,其包含至少一种环氧树脂和包含二氨基甲基环己烷的7种立体异构体的混合物,其相对于彼此具有非常特定的比例,制备该组合物的方法,该组合物用于生产硬化环氧化物,粘合剂, 复合材料和模制品,以特定比例包含二氨基甲基环己烷的7种立体异构体的混合物,以及该混合物用于制备组合物的用途。

    PROCESS FOR PRODUCING VISCOELASTIC FLEXIBLE POLYURETHANE FOAMS
    5.
    发明申请
    PROCESS FOR PRODUCING VISCOELASTIC FLEXIBLE POLYURETHANE FOAMS 有权
    生产粘弹性柔性聚氨酯泡沫的方法

    公开(公告)号:US20120115970A1

    公开(公告)日:2012-05-10

    申请号:US13383238

    申请日:2010-07-14

    IPC分类号: C08G18/67

    摘要: The invention relates to a process for producing viscoelastic flexible polyurethane foams by reacting a) polyisocyanates with b) compounds having at least two hydrogen atoms which are reactive toward isocyanate groups, c) blowing agents, wherein the compounds having at least two hydrogen atoms which are reactive toward isocyanate groups b) comprise b1) from 0 to 90 parts by weight of at least one polyether alcohol consisting of exclusively propylene oxide units or propylene oxide units and not more than 50% by weight, based on the total weight of the alkylene oxides used, of ethylene oxide units in the polyether chain and having a nominal functionality of from 3 to 8 and a hydroxyl number in the range from 100 to 350 mg KOH/g, and b2) from 10 to 100 parts by weight of at least one graft polyol which can be prepared by in-situ polymerization of olefinically unsaturated monomers in at least one polyether alcohol which has exclusively propylene oxide units or propylene oxide units and not more than 50% by weight, based on the total amount of alkylene oxides used, of ethylene oxide units in the polyether chain, a nominal functionality of from 2 to 8 and a hydroxyl number in the range from 100 to 350 mg KOH/g, having a solids content of not more than 60% by weight, based on the total amount of polyols and solids used, where the sum of the parts by weight of b1) and b2) is 100.

    摘要翻译: 本发明涉及通过使a)多异氰酸酯与b)具有至少两个对异氰酸酯基团具有反应性的氢原子的化合物反应来制备粘弹性柔性聚氨酯泡沫体的方法,c)发泡剂,其中具有至少两个氢原子的化合物是 对于异氰酸酯基团具有反应性b)包括:b1)0至90重量份的至少一种由专门环氧丙烷单元或环氧丙烷单元组成的聚醚醇,且不大于50重量%,基于环氧烷烃的总重量 使用聚醚链中的环氧乙烷单元,其标称官能度为3至8,羟基数为100至350mg KOH / g,和b2)10至100重量份的至少一种 接枝多元醇,其可以通过在至少一种仅具有环氧丙烷单元或环氧丙烷单元的聚醚醇中将烯属不饱和单体原位聚合而不是 大于50重量%,基于所使用的环氧烷烃的总量,聚醚链中的环氧乙烷单元,标称官能度为2至8,羟基数为100至350mg KOH / g, 基于所使用的多元醇和固体的总量,固体含量不超过60重量%,其中b1)和b2)的重量份之和为100。

    Process for producing viscoelastic polyurethane foams
    6.
    发明授权
    Process for producing viscoelastic polyurethane foams 有权
    生产粘弹性聚氨酯泡沫的方法

    公开(公告)号:US08362098B2

    公开(公告)日:2013-01-29

    申请号:US12095754

    申请日:2006-11-30

    摘要: A process for producing viscoelastic flexible polyurethane foams by reacting a) polyisocyanates with b) compounds having at least two hydrogen atoms which are reactive toward isocyanate groups, c) blowing agents, wherein b) comprise b1) from 70 to 10 parts by weight of at least one polyether alcohol having polyoxypropylene units, a nominal functionality of from 3 to 6 and a hydroxyl number of 100 to 300 mg KOH/g, b2) from 10 to 70 parts by weight of at least one polyetherol having polyoxypropylene units, a nominal functionality of 2 and a hydroxyl number of 50 to 350 mg KOH/g, b3) from 10 to 30 parts by weight of at least one polyether alcohol having ethylene oxide units, a nominal functionality of from 2 to 3 and a hydroxyl number of 50 to 550 mg KOH/g, b4) from 0 to 20 parts by weight of at least one graft polyetherol having a nominal functionality of from 2 to 3 and a hydroxyl number of 20 to 40 mg KOH/g.

    摘要翻译: 一种制备粘弹性柔性聚氨酯泡沫的方法,通过使a)多异氰酸酯与b)具有至少两个对异氰酸酯基团具有反应性的氢原子的化合物,c)发泡剂,其中b)包含:b1)70至10重量份的 至少一种具有聚氧丙烯单元的聚醚醇,标称官能度为3至6,羟基数为100至300mg KOH / g,b2)10至70重量份的至少一种具有聚氧丙烯单元的聚醚,标称官能度 的2,羟值为50〜350mg KOH / g,b3)10〜30重量份的至少一种具有环氧乙烷单元的聚醚醇,2〜3的标称官能度和50〜 550mg KOH / g,b4)0至20重量份的标称官能度为2至3,羟值为20至40mg KOH / g的至少一种接枝聚乙烯醇。

    Polyurethane Article With Increased Comfort
    7.
    发明申请
    Polyurethane Article With Increased Comfort 有权
    聚氨酯文章舒适度增加

    公开(公告)号:US20100196690A1

    公开(公告)日:2010-08-05

    申请号:US12758656

    申请日:2010-04-12

    IPC分类号: B32B27/40 C08L75/04

    摘要: A unique combination of a hydrophilic polyol (A) and a hydrophobic polyol (B) having a terminal ethylene oxide cap are used in a resin composition and a polyurethane system, and are used to form a polyurethane article, such as a polyurethane foam. The hydrophilic polyol (A) is ethylene oxide (EO) rich and the hydrophobic polyol (B) is propylene oxide (PO) rich. The hydrophilic polyol (A) and the hydrophobic polyol (B) are present in the resin composition and the polyurethane system in a weight ratio (A:B) of from 1.5:1 to 20:1. The polyurethane article exhibits excellent comfort for use in vehicle applications, such as automotive and motorcycle seating, due to reduced resonance frequency and reduced peak vibration transmissivity relative to previous polyurethane articles.

    摘要翻译: 在树脂组合物和聚氨酯体系中使用具有末端环氧乙烷盖的亲水性多元醇(A)和疏水性多元醇(B)的独特组合,并且用于形成聚氨酯制品如聚氨酯泡沫。 亲水性多元醇(A)为环氧乙烷(EO),疏水性多元醇(B)为环氧丙烷(PO)浓。 亲水性多元醇(A)和疏水性多元醇(B)以重量比(A:B)为1.5:1〜20:1存在于树脂组合物和聚氨酯体系中。 由于相对于以前的聚氨酯制品的共振频率降低和峰值振动透过率降低,聚氨酯制品在汽车和摩托车座椅等车辆用途中表现出极好的舒适性。

    Process for producing viscoelastic flexible polyurethane foams
    9.
    发明授权
    Process for producing viscoelastic flexible polyurethane foams 有权
    生产粘弹性柔性聚氨酯泡沫的方法

    公开(公告)号:US09193821B2

    公开(公告)日:2015-11-24

    申请号:US13383238

    申请日:2010-07-14

    摘要: The invention relates to a process for producing viscoelastic flexible polyurethane foams by reacting a) polyisocyanates with b) compounds having at least two hydrogen atoms which are reactive toward isocyanate groups, c) blowing agents, wherein the compounds having at least two hydrogen atoms which are reactive toward isocyanate groups b) comprise b1) from 0 to 90 parts by weight of at least one polyether alcohol consisting of exclusively propylene oxide units or propylene oxide units and not more than 50% by weight, based on the total weight of the alkylene oxides used, of ethylene oxide units in the polyether chain and having a nominal functionality of from 3 to 8 and a hydroxyl number in the range from 100 to 350 mg KOH/g, and b2) from 10 to 100 parts by weight of at least one graft polyol which can be prepared by in-situ polymerization of olefinically unsaturated monomers in at least one polyether alcohol which has exclusively propylene oxide units or propylene oxide units and not more than 50% by weight, based on the total amount of alkylene oxides used, of ethylene oxide units in the polyether chain, a nominal functionality of from 2 to 8 and a hydroxyl number in the range from 100 to 350 mg KOH/g, having a solids content of not more than 60% by weight, based on the total amount of polyols and solids used, where the sum of the parts by weight of b1) and b2) is 100.

    摘要翻译: 本发明涉及通过使a)多异氰酸酯与b)具有至少两个对异氰酸酯基团具有反应性的氢原子的化合物反应来制备粘弹性柔性聚氨酯泡沫体的方法,c)发泡剂,其中具有至少两个氢原子的化合物是 对于异氰酸酯基团具有反应性b)包括:b1)0至90重量份的至少一种由专门环氧丙烷单元或环氧丙烷单元组成的聚醚醇,且不大于50重量%,基于环氧烷烃的总重量 使用聚醚链中的环氧乙烷单元,其标称官能度为3至8,羟基数为100至350mg KOH / g,和b2)10至100重量份的至少一种 接枝多元醇,其可以通过在至少一种仅具有环氧丙烷单元或环氧丙烷单元的聚醚醇中将烯属不饱和单体原位聚合而不是 大于50重量%,基于所使用的环氧烷烃的总量,聚醚链中的环氧乙烷单元,标称官能度为2至8,羟基数为100至350mg KOH / g, 基于所使用的多元醇和固体的总量,固体含量不超过60重量%,其中b1)和b2)的重量份之和为100。

    Process for producing flexible polyurethane foams
    10.
    发明授权
    Process for producing flexible polyurethane foams 有权
    生产柔性聚氨酯泡沫的方法

    公开(公告)号:US08247467B2

    公开(公告)日:2012-08-21

    申请号:US12513506

    申请日:2007-11-09

    IPC分类号: C08G18/28

    摘要: The invention relates to a process for producing flexible polyurethane foams by reacting a) polyisocyanates with b) compounds having at least two hydrogen atoms which are reactive toward isocyanate groups in the presence of c) blowing agents, wherein the component b) comprises at least one polyether carbonate polyol bi) which can be prepared by addition of carbon dioxide and alkylene oxides onto H-functional starter substances using DMC catalysts and has a functionality of at least 2, a hydroxyl number in the range from 10 to 500 mg KOH/g and a content of incorporated carbon dioxide in the form of carbonate units of at least 2% by weight.

    摘要翻译: 本发明涉及通过使a)多异氰酸酯与b)在c)发泡剂存在下具有至少两个对异氰酸酯基团具有反应性的氢原子的化合物反应来生产柔性聚氨酯泡沫体的方法,其中组分b)包含至少一种 聚醚碳酸酯多元醇bi),其可以通过使用DMC催化剂将二氧化碳和环氧烷加成到H官能起始物质上并具有至少2的官能度,羟值在10至500mg KOH / g范围内的官能度和 碳酸酯单元形式的并入二氧化碳的含量为至少2重量%。