JOINING METHOD
    1.
    发明申请

    公开(公告)号:US20230042870A1

    公开(公告)日:2023-02-09

    申请号:US17788668

    申请日:2020-12-02

    IPC分类号: B23K26/348 B23K9/16

    摘要: A joining method includes: an overlapping step of overlapping a front surface of a first metal member with a back surface of a second metal member; and a welding step of welding the first metal member with the second metal member by hybrid welding, using a hybrid welding machine including a leading laser welding unit and a trailing arc welding unit. In the welding step, laser welding, by irradiating with a laser beam, and arc welding are performed from a front surface of the second metal member, along a preset travel route which is set on an overlapped part formed by the first metal member and the second metal member overlapped with each other, to the overlapped part, and the laser beam is oscillated to cross the preset travel route.

    Method for manufacturing heat transfer plate

    公开(公告)号:US11413700B2

    公开(公告)日:2022-08-16

    申请号:US17058601

    申请日:2019-05-07

    IPC分类号: B23K20/00 B23K20/12

    摘要: The present invention is characterized by including a heat medium pipe insertion process to insert a heat medium pipe into a concave groove; a lid plate insertion process to insert a lid plate into a lid groove; and a joining process to perform friction stirring while a primary joining rotary tool provided with a base side pin and a tip side pin is moved along a butted portion of a side wall of the lid groove and a side face of the lid plate, wherein in the joining process, friction stirring is performed while the tip side pin of the primary rotary tool which is rotating is inserted into the butted portion and an outer circumferential face of the base side pin is in contact with the base member and the lid plate, and plastically fluidized material fluidized by frictional heat is flowed into a void portion formed adjacent to the heat medium pipe.

    Joining method
    6.
    发明授权

    公开(公告)号:US11241756B2

    公开(公告)日:2022-02-08

    申请号:US16607055

    申请日:2017-11-02

    IPC分类号: B23K20/12

    摘要: An edge of each of a first metal member and a second metal member is formed to have a U-shaped cross section with a first horizontal plate projecting from a base edge of a vertical plate, and with a second horizontal plate projecting from a top edge of the vertical plate. The second metal member includes a projecting part. The joining method includes: an abutting step of forming an abutted part by abutting a front surface of the first horizontal plate the first metal member against a second side surface of the second metal member; and a joining step of performing friction stir welding of the first metal member and the second metal member by inserting a stirring pin from the projecting part and moving a joining rotating tool along an inner corner at the top edge of the vertical plate of the second metal member while making only the stirring pin in contact with the first metal member and the second metal member.

    ALUMINUM ALLOY SHEET FOR BATTERY LID USE FOR FORMING INTEGRATED EXPLOSION-PROOF VALVE AND METHOD OF PRODUCTION OF SAME

    公开(公告)号:US20210238720A1

    公开(公告)日:2021-08-05

    申请号:US16644861

    申请日:2019-07-12

    IPC分类号: C22F1/04 C22C21/00 H01M50/159

    摘要: Aluminum alloy sheet for battery lid use having suitable strength and excellent in deformation resistance and formability, which aluminum alloy sheet for battery lid use enabling formation of an integrated explosion-proof valve with little variation in operating pressure and excellent in cyclic fatigue resistance, and a method of production of the same are provided, the aluminum alloy sheet for battery lid use for forming an integrated explosion-proof valve having a component composition containing Fe: 0.85 to 1.50 mass %, Mn: 0.30 to 0.70 mass %, Ti: 0.002 to 0.15 mass %, and B: less than 0.05 mass %, having a balance of Al and impurities, having an Fe/Mn ratio restricted to 1.8 to 3.5, restricting, as impurities, Si to less than 0.40 mass %, Cu to less than 0.03 mass %, Mg to less than 0.05 mass %, and V to less than 0.03 mass %, having a tensile strength of 95 MPa or more, having a 0.2% yield strength of 40 MPa or more, having a value of elongation of 40% or more, having a recrystallized structure, and having a value of elongation after cold rolling by a rolling reduction of 80% of 6.5% or more. Furthermore, an average grain size of the recrystallized grains of the recrystallized structure is preferably 15 to 25 μm.

    PRODUCTION METHOD OF HEAT TRANSMITTING PLATE

    公开(公告)号:US20210170521A1

    公开(公告)日:2021-06-10

    申请号:US16772038

    申请日:2019-01-17

    IPC分类号: B23K20/12

    摘要: A primary joining rotary tool F comprises a stirring pin F2including a circumferential face tapers to become thinner toward a tip portion of the stirring pin, a flat face F3 at the tip portion of the stirring pin F2 and a projecting portion F4 projecting from the flat face F3. Friction-stirring is performed in the primary joining process by inserting the stirring pin F2 that is rotating into an abutted portion J1 in a manner that only the stirring pin F2 is in contact with the base member 2 and the lid plate 5 with the flat face F3 being in contact with the base member 2 and the lid plate 5 and with a tip face F5 of the projecting portion F4 being in contact only with the base member 2.

    JOINING METHOD
    9.
    发明申请

    公开(公告)号:US20210146472A1

    公开(公告)日:2021-05-20

    申请号:US16622559

    申请日:2018-01-25

    IPC分类号: B23K20/12

    摘要: A first metal member (1) and a second metal member (2) are joined together using a rotary tool (F1D) comprising a base side pin (F3) and a tip side pin (F4), comprising an overlapping and abutting process of forming an overlapped portion (J1a), a top side abutted portion (J1b) and a back side abutted portion (J1c), and a friction stirring process of inserting the tip side pin (F4) that is rotating into the top side abutted portion (J1b) to join the top side abutted portion (J1b) and the overlapped portion (J1a) with a flat face (F5) vertical to a rotation axis of the rotary tool (F1D) being in contact with both the first metal member (1) and the second metal member (2) and with a tip face (f7) of a protruding portion (F6) protruding from the flat face (F5) being inserted deep over the overlapped portion (J1a).

    Pellicle frame and pellicle
    10.
    发明授权

    公开(公告)号:US10955740B2

    公开(公告)日:2021-03-23

    申请号:US16316501

    申请日:2017-06-30

    IPC分类号: G03F1/64

    摘要: The present invention provides; a pellicle frame which can effectively inhibit distortion of the photo mask (8) caused by mounting the pellicle (1), and which does not have a complex shape, and a pellicle which uses said pellicle frame are provided, and a manufacturing method of a blackened pellicle frame is also provided which can reduce the defect of the surface flickering under concentrated light and which facilitates inspection of the foreign matter adhesion prior to use. The present invention relates to a pellicle frame with an anodized film on a surface of an aluminum alloy frame, characterized in that: the aluminum alloy frame comprises an aluminum alloy which contains Ca: 5.0 to 10.0% by mass with the remainder aluminum and unavoidable impurities are contained, and has an area (volume) ratio of an Al4Ca phase, which is a dispersed phase, is greater than or equal to 25%, and a crystal structure of a part of the Al4Ca phase is monoclinic; wherein the Al4Ca phase dispersed in the anodized film is anodized, and the anodized film is stained with a black dye.