Abstract:
A high-strength galvanized steel sheet has a low YP, good stretch flangeability, and excellent corrosion resistance and contains, on a percent by mass basis, more than 0.015% to less than 0.10% of C, 0.5% or less of Si, 1.0% to 1.9% of Mn, 0.015% to 0.050% of P, 0.03% or less of S, 0.01% to 0.5% of sol. Al, 0.005% or less of N, less than 0.40% of Cr, 0.005% or less of B, less than 0.15% of Mo, 0.4% or less of V, and less than 0.020% of Ti, in which 2.2≦[Mneq]≦3.1 and [% Mn]+3.3[% Mo]≦1.9, and [% Mn]+3.3[% Mo])/(1.3[% Cr]+8[% P]+150B*)
Abstract:
A high strength steel sheet is formed of steel having the composition containing by mass % over 0.015% and less than 0.100% C, less than 0.50% Si, over 1.0% and less than 2.0% Mn, 0.05% or less P, 0.03% or less S, 0.01% or more and 0.3% or less sol. Al, 0.005% or less N, less than 0.35% Cr, 0.0010% or more and 0.0050% or less B, less than 0.15% Mo, less than 0.030% Ti, and iron and unavoidable impurities as a balance, wherein the steel satisfies 2.1≦[Mneq]≦3.1, the microstructure of the steel includes a ferrite and a second phase, a volume fraction of the second phase is set to 2.0 to 12.0%, a total ratio of a volume fraction of martensite and a volume fraction of retained γ to the volume fraction of second phase is 60% or more, and the number of carbides which are present within ferrite particles, have an aspect ratio of 3.0 or less and have a diameter of 0.25 to 0.90 μm is set to 10000 pieces/mm2 or less.
Abstract:
A high tensile-strength galvanized steel sheet includes C: at least 0.05% but less than 0.12%, Si: at least 0.01% but less than 0.35%, Mn: 2.0% to 3.5%, P: 0.001% to 0.020%, S: 0.0001% to 0.0030%, Al: 0.005% to 0.1%, N: 0.0001% to 0.0060%, Cr: more than 0.5% but not more than 2.0%, Mo: 0.01% to 0.50%, Ti: 0.010% to 0.080%, Nb: 0.010% to 0.080%, and B: 0.0001% to 0.0030%, the remainder being Fe and unavoidable impurities, wherein the high tensile-strength galvanized steel sheet has a microstructure that contains 20% to 70% by volume ferrite having an average grain size of 5 μm or less. The high tensile-strength galvanized steel sheet has a tensile strength of at least 980 MPa, and excellent formability and weldability.
Abstract:
A zinciferous coated steel sheet comprises a steel sheet, a zinciferous coating layer formed on the steel sheet, a Fe--Ni--Zn--O film formed on the zinciferous coating layer, and an oxide layer formed on a surface portion of the Fe--Ni--Zn--O film. The method comprises providing an electrolyte of an acidic sulfate aqueous solution, carrying out an electrolysis treatment in the electrolyte under a current density ranging from 1 to 150 A/dm.sup.2, and carrying out an oxidation treatment to a surface of the zinciferous coated steel sheet.
Abstract:
A high strength steel sheet is formed of steel having the composition containing by mass % over 0.015% and less than 0.100% C, less than 0.50% Si, over 1.0% and less than 2.0% Mn, 0.05% or less P, 0.03% or less S, 0.01% or more and 0.3% or less sol. Al, 0.005% or less N, less than 0.35% Cr, 0.0010% or more and 0.0050% or less B, less than 0.15% Mo, less than 0.030% Ti, and iron and unavoidable impurities as a balance, wherein the steel satisfies 2.1≦[Mneq]≦3.1, the microstructure of the steel includes a ferrite and a second phase, a volume fraction of the second phase is set to 2.0 to 12.0%, a total ratio of a volume fraction of martensite and a volume fraction of retained γ to the volume fraction of second phase is 60% or more, and the number of carbides which are present within ferrite particles, have an aspect ratio of 3.0 or less and have a diameter of 0.25 to 0.90 μm is set to 10000 pieces/mm2 or less.
Abstract:
A multiphase steel sheet has a steel composition containing, in percent by mass, more than 0.015% to less than 0.100% of carbon, less than 0.40% of silicon, 1.0% to 1.9% of manganese, more than 0.015% to 0.05% of phosphorus, 0.03% or less of sulfur, 0.01% to 0.3% of soluble aluminum, 0.005% or less of nitrogen, less than 0.30% of chromium, 0.0050% or less of boron, less than 0.15% of molybdenum, 0.4% or less of vanadium, 0.02% or less of titanium, wherein [Mneq] is 2.0 to 2.8, the balance being iron and incidental impurities.
Abstract:
A method produces a high-strength cold-rolled steel sheet includes hot-rolling and cold-rolling steel having a composition which contains, by % by mass, over 0.01% to less than 0.08% of C, 0.2% or less of Si, 0.8% to less than 1.7% of Mn, 0.03% or less of P, 0.02% or less of S, 0.3% or less of sol. Al, 0.01% or less of N, and over 0.4% to 2% of Cr, and which satisfies 1.9
Abstract:
A high tensile-strength galvanized steel sheet includes C: at least 0.05% but less than 0.12%, Si: at least 0.01% but less than 0.35%, Mn: 2.0% to 3.5%, P: 0.001% to 0.020%, S: 0.0001% to 0.0030%, Al: 0.005% to 0.1%, N: 0.0001% to 0.0060%, Cr: more than 0.5% but not more than 2.0%, Mo: 0.01% to 0.50%, Ti: 0.010% to 0.080%, Nb: 0.010% to 0.080%, and B: 0.0001% to 0.0030%, the remainder being Fe and unavoidable impurities, wherein the high tensile-strength galvanized steel sheet has a microstructure that contains 20% to 70% by volume ferrite having an average grain size of 5 μm or less. The high tensile-strength galvanized steel sheet has a tensile strength of at least 980 MPa, and excellent formability and weldability.
Abstract:
A galvannealed steel sheet is manufactured by preparing a hot-dip galvanized steel sheet, alloying the steel sheet, and controlling time and temperature for alloying thereof depending on Si and Al contents. The hot-dip galvanized steel sheet contains 0.05 to 0.30% C, 0.01 to 2.0% Si, 0.08 to 3.0% Mn, 0.003 to 0.1% P, 0 to 0.07% S, 0.01 to 2.5% Al, 0 to 0.007% N, by mass, and the balance being Fe and inevitable impurities. Alloying time and temperature are controlled by the formula [Si+Al≧1.5×10−7×t0.75×(T−465)3+0.117], where t is the total time (sec) of holding the sheet at 465° C. or more on alloying the coating layer thereon, and T is the average temperature (° C.) of the sheet during the total time t (sec) of holding the steel sheet at 465° C. or more on alloying the coating layer thereon.
Abstract:
A zinciferous plated steel sheet which comprises a steel sheet, at least one zinciferous plating layer formed on at least one surface of the steel sheet, and an Fe--Ni--O film as an uppermost layer formed on the zinciferous plating layer. The total quantity of metallic elements in the Fe--Ni--O film is within a range of from 10 to 1,500 mg/m.sup.2, and the oxygen content in the Fe--Ni--O film is within a range of from 0.5 to under 30 wt. %. The ratio of the iron content (g/l) relative to the total quantity of the iron content (g/l) and the nickel content (g/l) in the Fe--Ni--O film is preferably within a range of from over 0 to under 1.0.