Abstract:
A process for dyeing or printing an article comprising a hydrophobic polymer, wherein said polymer is brought into contact with a condensation polymer obtained by condensation of at least one poly-hydroxyl-mono-carboxylic acid, prior to or simultaneously with the treatment of said article with a color imparting compound, with the proviso that the condensation polymer is not terminated with lipophilic groups, provides dyed articles with good fastness properties.
Abstract:
Polyolefin fibers and filaments, and fabrics made therefrom, are rendered dyeable via a combination of dyeability additives. The dyeability additive combination comprises at least one compound selected from the group consisting of the polyamides, copolyamides and polyetherpolyamides and at least one ethylene vinyl acetate. The dyed polyolefin fibers and fabrics are rendered light stable via the use of a combination of stabilizers, which comprises at least one compound selected from the group consisting of the ultraviolet light stabilizers and at least one compound selected from the group consisting of the hindered amine light stabilizers. The ultraviolet light stabilizers are for example hydroxyphenylbenzotriazoles or tris-aryl-s-triazines. The hindered amine light stabilizers are for example of high molecular weight, for instance greater than 1000 g/mol. The dyes are for example anthraquinone blue dyes, anthraquinone red dyes, diazo red dyes or nitro yellow dyes.
Abstract:
The present invention is aimed at a method of providing wettability to polyester fibers or filaments, to woven or nonwoven fabrics made therefrom and to resultant articles of manufacture. The method comprises melt extruding a mixture comprising a polyester and one or more alkyl metal sulfonates where the metal is Na, Li or K and the alkyl is straight or branched chain alkyl of 1 to 24 carbon atoms, or is straight or branched chain alkenyl of 2 to 24 carbon atoms. The alkyl metal sulfonates are present from about 0.1% to about 1.9% by weight based on the weight of the polyester. A post treatment step such as an alkaline treatment step is not included. The melt extrusion mixtures do not include certain additives such as polyoxyalkylene compounds, alkylmonoethonolamide compounds, alkyldiethanolamine compounds and polyetheramide compounds.
Abstract:
The present invention is aimed at a method of providing wettability to polyester fibers or filaments, to woven or nonwoven fabrics made therefrom and to resultant articles of manufacture. The method comprises melt extruding a mixture comprising a polyester and one or more alkyl metal sulfonates where the metal is Na, Li or K and the alkyl is straight or branched chain alkyl of 1 to 24 carbon atoms, or is straight or branched chain alkenyl of 2 to 24 carbon atoms. The alkyl metal sulfonates are present from about 0.1% to about 1.9% by weight based on the weight of the polyester. A post treatment step such as an alkaline treatment step is not included. The melt extrusion mixtures do not include certain additives such as polyoxyalkylene compounds, alkylmonoethonolamide compounds, alkyldiethanolamine compounds and polyetheramide compounds.