MECHANICAL PYROLYSIS IN A SHEAR RETORT
    4.
    发明申请
    MECHANICAL PYROLYSIS IN A SHEAR RETORT 有权
    机械回归中的机械热解

    公开(公告)号:US20120193271A1

    公开(公告)日:2012-08-02

    申请号:US13016328

    申请日:2011-01-28

    IPC分类号: C10C1/04

    摘要: Mechanical visbreaking and pyrolysis between counter-rotating coaxial centrifugal impellers in a continuous radial counterflow process minimizes wastewater discharges. In an embodiment, a cataclastic shear retort comminutes, shear thins, and shear heats an axial feed, such as tar sand, oil shale, coal tailings, distillation bottoms, or lignite. Pyrolyzing the feedstock in this shear retort yields a product stream of gases, naphthas, and oils which first mixes with the feedstock and then is axially extracted, while spent solids are simultaneously extruded from the periphery as coked devolatilized residue, such as char sand for upgrading soil to terra preta. Recirculation of shear-heated solids in long residence time within the shear retort brings heat from the spent solids at the periphery to the feedstock without an external heated sand loop. CO2 emissions from combustion to heat water for oil extraction are eliminated.

    摘要翻译: 反向旋转同轴离心式叶轮在连续径向逆流过程中的机械减粘裂化和热解使废水排放最小化。 在一个实施方案中,破碎剪切破碎物粉碎,剪切变形和剪切加热轴向进料,例如焦油砂,油页岩,煤尾矿,蒸馏塔底或褐煤。 在该剪切蒸馏器中热解原料产生气体,石脑油和油的产物流,其首先与原料混合然后被轴向提取,而废固体同时从周边挤出,作为焦化脱挥发分残余物,例如炭砂,用于升级 土壤到地雷 在剪切蒸馏器内长时间停留的剪切加热固体的再循环将热量从外围的废固体引入原料,而不需要外部加热的砂环。 消除了从燃烧到加热水的CO2排放。

    Coal tar pitch and the preparation and use thereof
    8.
    发明授权
    Coal tar pitch and the preparation and use thereof 失效
    煤焦油沥青及其制备和使用

    公开(公告)号:US5262043A

    公开(公告)日:1993-11-16

    申请号:US869936

    申请日:1992-04-17

    CPC分类号: C10C1/00 C10C1/04 C10C1/19

    摘要: An isotropic coal tar pitch having a low content of carcinogenic compounds is prepared by distilling a coal tar pitch in an evaporator having a specific evaporator surface of from 330 to 10,000 m.sup.2 /m.sup.3, at a temperature in the range of from 300.degree. to 380.degree. C., under a pressure not exceeding 1 mbar, whereby the average stay period is from 2 to 10 minutes. The isotropic pitch thus obtained contains less that 50 ppm of benzo[a]pyrene and is suitable, optionally after adding an oil, resin or other modifying agents having a low benzo[a]pyrene content, for use as binding and impregnating agent and also as protecting agent in construction materials or as varnish (painting agent).

    摘要翻译: 具有低含量致癌化合物的各向同性煤焦油沥青通过在具有330至10,000m 2 / m 3的特定蒸发器表面的蒸发器中蒸馏煤焦油沥青而制备,温度范围为300-380℃ C.在不超过1毫巴的压力下,平均逗留时间为2至10分钟。 由此获得的各向同性沥青包含少于50ppm的苯并[a]芘,并且任选地在加入具有低苯并[a]芘含量的油,树脂或其它改性剂之后,适合用作结合和浸渍剂,并且还 作为建筑材料中的保护剂或清漆(涂漆剂)。