公开(公告)号:US20240400759A1
公开(公告)日:2024-12-05
申请号:US18239409
申请日:2023-08-29
Applicant: HYUNDAI MOTOR COMPANY , KIA CORPORATION , INDUSTRY-ACADEMIC COOPERATION FOUNDATION GYEONGSANG NATIONAL UNIVERSITY
Inventor: Jung Wook Lee , Jeong Seok Oh , Gyuri Kim , Seongrok Jeong , Sarbaranjan Paria
Abstract: A method of preparing a bio-polyol using coffee by-products, a polyurethane resin composition containing the bio-polyol, and a method of preparing a polyurethane foam using the same are described. The method simplifies the complicated process of extracting polyols from coffee and thus extracts bio-polyols within a short time, thus being advantageous in terms of cost and time.
-
公开(公告)号:US11879036B2
公开(公告)日:2024-01-23
申请号:US17055234
申请日:2019-06-19
Applicant: SOLVAY SPECIALTY POLYMERS USA, LLC , CYTEC INDUSTRIES INC.
Inventor: Chantal Louis , James Pratte
CPC classification number: C08G65/4012 , C08G65/4093 , C08G65/46 , C08J5/042 , C08J5/043 , C08J5/24 , C08G2650/40 , C08J2371/10
Abstract: The present invention relates to poly(ether ketone ketone) (PEKK) polymers, a method for the manufacture thereof, to articles and composites made therefrom, to methods of making the composites, and composite articles including the PEKK composites. It was surprisingly discovered that by synthesizing the PEKK polymers from low-metal monomers and selectively controlling the relative amounts of reactants during the synthesis, PEKK polymers having unexpectedly improved melt stability can be obtained. The PEKK composites including the PEKK polymers are especially well-suited for fabrication of thick composite parts where melt stability of the polymer matrix is important.
-
公开(公告)号:US11518841B2
公开(公告)日:2022-12-06
申请号:US16900728
申请日:2020-06-12
Applicant: John I. Nanos
Inventor: John I. Nanos
IPC: B01D15/00 , C08G18/08 , C08G18/10 , C08G18/32 , C08G18/48 , C08G18/66 , C08G18/73 , C08G18/76 , C08G65/46 , C08L71/00
Abstract: A crosslinked biobased hydrophilic foam comprising a reaction product of: a cleaned biobased polyoxyalkylene glycol polyol with an ethylene oxide content of at least 40 mole percent, constituting 31.80 to 67.95 percent biogenic carbon content by weight, constituting less than 15 ppm combined sodium and potassium metals, and comprising less than 0.5% water by weight; an isocyanate, wherein the isocyanate and the cleaned biobased polyoxyalkylene glycol polyol are premixed to create a prepolymer mixture with the cleaned biobased polyoxyalkylene glycol polyol of the prepolymer mixture; and water, wherein the water is admixed with the prepolymer mixture to yield the crosslinked biobased hydrophilic foam.
-
公开(公告)号:US20220380536A1
公开(公告)日:2022-12-01
申请号:US17618903
申请日:2020-06-11
Applicant: SOLVAY SPECIALTY POLYMERS USA, LLC
Inventor: Chantal LOUIS , Mohammad Jamal EL-HIBRI
Abstract: The present invention generally relates to a powder comprising a PEEK-PEoEK copolymer, wherein the PEEK-PEoEK copolymer having RPEEK and RPEoEK repeat units in a molar ratio RPEEK/RPEoEK ranging from 95/5 to 5/95. The present invention also relates to a method of preparing the powder, as well as to the uses of the powder for coating, compression molding and to prepare a three-dimensional (3D) object.
-
公开(公告)号:US11485821B2
公开(公告)日:2022-11-01
申请号:US16314537
申请日:2018-10-11
Applicant: Kureha Corporation
Inventor: Hiroshi Sakabe , Tasutaka Suzuki , Akiko Wakamatsu , Kenji Suzuki
IPC: C08G65/40 , C08G65/46 , C08K5/3415
Abstract: Provided is a method that can stably produce polyaryletherketone that has a high degree of polymerization and can be easily recovered. The method for producing polyaryletherketone includes: a polycondensation step of carrying out desalting polycondensation in a reaction solvent; and a cooling step of cooling a reaction mixture after desalting polycondensation is completed. When the method is implemented, the polycondensation step is carried out in a hydrophilic solvent under pressurized conditions, and the polymerization temperature in the polycondensation step is at or above the boiling point of the hydrophilic solvent at ambient pressure. In addition, the polymer content in terms of monomers at the time of cooling in the cooling step is from 1 part by mass to 50 parts by mass, per 100 parts by mass of the hydrophilic solvent in the reaction mixture.
-
公开(公告)号:US20210269594A1
公开(公告)日:2021-09-02
申请号:US17323053
申请日:2021-05-18
Applicant: CYTEC INDUSTRIES INC.
Inventor: James Martin GRIFFIN , Kingsley Kin Chee HO , James Francis PRATTE
IPC: C08G65/48 , B32B27/12 , C08J5/04 , C08G65/46 , B32B7/04 , B32B5/16 , B32B5/12 , B32B5/02 , B32B5/26 , B32B5/06 , B29B15/08 , B29C70/34
Abstract: Surface-treated polymeric particles which are dispersible in water or an aqueous solution without the aid of any surfactant. Surface treatment of hydrophobic polymeric particles is carried out to increase the surface energy and to render the surfaces of the particles hydrophilic, thereby eliminating the need for a surfactant to disperse the polymeric particles in water or an aqueous solution. As such, a surfactantless slurry can be formed from the surface-treated particles for the fabrication of fiber-reinforced thermoplastic composite structures.
-
公开(公告)号:US11015071B2
公开(公告)日:2021-05-25
申请号:US16097728
申请日:2017-05-02
Applicant: Arkema France
Inventor: Benoît Brule , Jérôme Amstutz , Guillaume Le , Julien Jouanneau
IPC: C09D11/102 , B33Y10/00 , B33Y70/00 , B29C64/153 , C08G65/40 , C08G65/46 , C08L71/00 , C08G8/02 , B29K71/00
Abstract: Provided is a composition suitable for a process of building a three-dimensional object layer-by-layer by electromagnetic radiation-generated sintering, including at least one poly(aryl-ether-ketone) (PAEK), where the composition has an aromatic ether content of from 0 and 0.4% by mass, based on the total mass of the composition, and an aluminium mass content of lower than 1000 ppm. The composition may be used in process for building an object comprising sintering the composition with electromagnetic radiation. The present invention also includes a three-dimensional object obtained by such a process. A process for preparing the composition is also provided.
-
公开(公告)号:US10899890B2
公开(公告)日:2021-01-26
申请号:US16311239
申请日:2017-06-21
Applicant: Sumitomo Chemical Company, Limited
Inventor: Kazuyuki Ito , Yoshio Shoda
IPC: C08G75/23 , C08L71/10 , C08G65/40 , C08G75/20 , G01N30/26 , C08L81/06 , G01N30/74 , C08G65/46 , G01N30/88 , C09J181/06
Abstract: The invention provides an aromatic polysulfone including an aromatic polysulfone having at least one highly polar functional group at its terminus, wherein in the aromatic polysulfone, an area of a signal attributed to the aromatic polysulfone having a highly polar functional group with respect to a total area of all signals attributed to the aromatic polysulfone in a chromatogram obtained by measurement through a gel permeation chromatography method under the following conditions is 19% or more and 100% or less, wherein sample injection volume is 5 μL, column is “Shodex KF-803” manufactured by Showa Denko K.K., column temperature is 40° C., eluent is N,N-dimethylformamide, eluent flow rate is 0.5 mL/min, and detector is ultraviolet-visible spectrophotometer (UV).
-
9.
公开(公告)号:US10787543B2
公开(公告)日:2020-09-29
申请号:US15598803
申请日:2017-05-18
Applicant: Mitsubishi Chemical Corporation
Inventor: Takanori Taniguchi , Yoko Nakagawa , Ryo Yamashita , Nobuyuki Kobayashi
IPC: C08G65/34 , C09D175/08 , C08G18/48 , D01F6/70 , C08G63/688 , C08G65/30 , C08G65/20 , C08G63/16 , C08G65/46 , D06N3/00
Abstract: The present invention provides a high-molecular-weight polyether polyol ensuring that when used as a polyurethane raw material, a polyurethane having excellent flexibility and elastic recovery can be obtained; and a method for producing, with high productivity, a polyether polyol having a higher number average molecular weight and a narrower molecular weight distribution than those of the raw material polyether polyol, and the polyether polyol of the present invention has a number average molecular weight of 3,500 to 5,500 and a molecular weight distribution of 1.7 to 3.0.
-
10.
公开(公告)号:US20200148822A1
公开(公告)日:2020-05-14
申请号:US16185485
申请日:2018-11-09
Applicant: Arkema France
Inventor: Julien JOUANNEAU , Steven Gabriel SCHON , Andrew Richard GODDARD
Abstract: A method for treating a shear-thinning residue composition deriving from the synthesis of an aryl ether ketone, the residue composition including a liquid fraction and solid residues, the method including the steps of: passing said shear-thinning residue composition through a shear-generating evaporating device, between a rotating part and a stationary part; and recovering a condensed liquid fraction and separately recover concentrated solid residues.
-
-
-
-
-
-
-
-
-