摘要: Chlorinated vinyl chloride resin may be produced through a heat chlorination reaction of an aqueous suspension of vinyl chloride resin in a hermetically sealable reaction vessel, the method including carrying out a first heat chlorination reaction while raising the temperature of an aqueous suspension of a vinyl chloride resin powder to a predetermined temperature within the range of 85° C. to 95° C., and subsequently carrying out a second heat chlorination reaction at the predetermined temperature.
摘要翻译: 氯化氯乙烯树脂可以通过氯乙烯树脂的水性悬浮液在可密封的反应容器中的热氯化反应来制备,该方法包括进行第一热氯化反应同时提高氯乙烯树脂的水悬浮液的温度 粉末至85℃至95℃范围内的预定温度,随后在预定温度下进行第二次热氯化反应。
-
公开(公告)号:US12104004B2
公开(公告)日:2024-10-01
申请号:US17437303
申请日:2020-03-27
IPC分类号: C08F8/22 , C08F114/06
CPC分类号: C08F8/22 , C08F114/06
摘要: The present invention provides a chlorinated polyvinyl chloride that enables excellent continuous productivity in molding and that enables a molded article to have both processability and unevenness-preventing properties. Provided is a chlorinated polyvinyl chloride having an endothermic peak start temperature (L) and an endothermic peak end temperature (H) that satisfy the following expression (1) in endothermic peak measurement using a differential scanning calorimeter (DSC): 41° C.≤H−L≤98° C. (1).
-
公开(公告)号:US09346901B2
公开(公告)日:2016-05-24
申请号:US14361791
申请日:2012-11-30
发明人: Masatoshi Harada
IPC分类号: C08F8/22 , C08F14/06 , C08F114/06
CPC分类号: C08F114/06 , C08F8/22 , C08F14/06
摘要: Chlorinated vinyl chloride resin may be produced through a heat chlorination reaction of an aqueous suspension of vinyl chloride resin in a hermetically sealable reaction vessel, the method including carrying out a first heat chlorination reaction while raising the temperature of an aqueous suspension of a vinyl chloride resin powder to a predetermined temperature within the range of 85° C. to 95° C., and subsequently carrying out a second heat chlorination reaction at the predetermined temperature.
摘要翻译: 氯化氯乙烯树脂可以通过氯乙烯树脂的水性悬浮液在可密封的反应容器中的热氯化反应来制备,该方法包括进行第一热氯化反应同时提高氯乙烯树脂的水悬浮液的温度 粉末至85℃至95℃范围内的预定温度,随后在预定温度下进行第二次热氯化反应。
-
-