摘要:
There is provided a dielectric ceramic composition including: a major component (a barium titanate-based base material); and a minor component, wherein in an XRD analysis of a sintered body obtained by sintering the dielectric ceramic composition, when a (110) peak of BaTiO3 is set as 1.00, a ratio of a peak of pyrochlore (RE2Ti2O7) at about 30.5 degrees with respect to the (110) peak of BaTiO3 satisfies 0.02 or less, where RE is at least one of Y, Dy, Ho, Sm, Gd, Er, La, Ce, Nd, Tb, and Pr.
摘要翻译:提供了一种介电陶瓷组合物,其包括:主要成分(钛酸钡基基材); 和次要组分,其中在通过烧结介电陶瓷组合物获得的烧结体的XRD分析中,当BaTiO 3的(110)峰值设定为1.00时,烧绿石的峰值(RE 2 Ti 2 O 7)与约30.5度的比例与 相对于BaTiO 3的(110)峰满足0.02以下,其中RE为Y,Dy,Ho,Sm,Gd,Er,La,Ce,Nd,Tb和Pr中的至少一种。
摘要:
A manufacturing method of a dielectric ceramic composition includes attaching a reactive functional group to a surface of a base material powder particle of a perovskite structure.
摘要:
A method of producing a core-shell particle includes introducing a barium titanate-based base powder and an additive to a reactor, and exposing the barium titanate-based base powder and the additive to a thermal plasma torch to obtain core-shell particles including a core portion having barium titanate (BaTiO3) and a shell portion including the additive and formed on a surface of the core portion.
摘要:
There is provided a dielectric ceramic composition including: a major component (a barium titanate-based base material); and a minor component, wherein the dielectric ceramic composition is sintered to form a sintered body having a fine structure, the fine structure includes first crystal grains in which a Ca content is lower than 2.5 mol % and second crystal grains in which a Ca content is between 2.5 mol % to 13.5 mol %, and the second crystal grains have a cross-sectional area ratio of 30% to 80% on the basis of 100% of an overall cross-sectional area of the fine structure.
摘要:
A dielectric material includes a barium titanate based base material main ingredient and an accessory ingredient. In a fine sintered structure of the dielectric material, crystal grains in which a content of Ca is less than 2.5 mol % are first crystal grains, crystal grains in which the content of Ca is 4.0 to 12.0 mol % are second crystal grains, and a ratio of an average size of the first crystal grains to an average size of the second crystal grains is in a range of 1.6 to 2.2.
摘要:
A dielectric ceramic composition contains a base material main ingredient and an accessory ingredient. The base material main ingredient includes a first base material main ingredient containing BaTiO3 and a second base material main ingredient containing (Na1-yKy)NbO3. The base material main ingredient is represented by (1−x)BaTiO3-x(Na1-yKy)NbO3, in which x and y satisfy 0.005≦x≦0.5 and 0.3≦y≦1.0, respectively.
摘要:
A multilayer electronic component includes a body including a dielectric layer and an internal electrode; and an external electrode disposed on the body, wherein the dielectric layer includes a plurality of dielectric grains, and wherein the plurality of dielectric grains include one or more first dielectric grains in which a sum of lengths of defects in a dielectric grain is 150 nm or more.
摘要:
There is provided a dielectric ceramic composition including a base powder, wherein the base powder includes: a first major component represented by BaTiO3, a second major component represented by (Na, K)NbO3, and a third major component represented by (Bi, Na)TiO3. The base powder is represented by xBaTiO3-y(Na, K)NbO3-z(Bi, Na)TiO3, where x+y+z=1, and x, y, and z are represented by mol, and x, y and z satisfy 0.5≦x≦0.97, 0.01≦y≦0.48, and 0.02≦z≦0.2, respectively. In certain embodiments, the base powder is be represented by xBaTiO3-y(Na0.5K0.5)NbO3-z(Bi0.5Na0.5)TiO3.
摘要:
There is provided a dielectric ceramic composition including: a major component (a barium titanate-based base material); and a minor component, wherein the dielectric ceramic composition is sintered to form a sintered body having a fine structure, the fine structure includes first crystal grains in which a Ca content is lower than 2.5 mol % and second crystal grains in which a Ca content is between 2.5 mol % to 13.5 mol %, and the second crystal grains have a cross-sectional area ratio of 30% to 80% on the basis of 100% of an overall cross-sectional area of the fine structure.