公开(公告)号:US10259927B2
公开(公告)日:2019-04-16
申请号:US15129737
申请日:2015-03-23
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Rick Robert Emilie Bercx , Hendrik Kormelink
Abstract: The present invention relates to a polymer composition having low sensory impression of smell comprising a polypropylene and a calcium salt of phosphoric acid, wherein in said polymer composition the amount of said calcium salt of phosphoric acid is preferably such to accomplish a sensory impression of smell measured according to VDA 270 of at most 4.0.
-
公开(公告)号:US20240035203A1
公开(公告)日:2024-02-01
申请号:US18266106
申请日:2021-12-07
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Abderrahman Meddad , Fahad Al-Mutairy , Henrica Norberta Alberta Maria Steenbakkers-Menting , Hendrik Kormelink , Tinashe Victor Mandishonha Ndoro , Gert Boven , Ronald Julianus Peter Schipper , Marco Dohmen
CPC classification number: D01D5/0985 , D01F6/06
Abstract: A melt-blown web contains melt-blown fibers obtained by a) melt-mixing a propylene-based polymer, a first peroxide and a second peroxide at temperatures between 180° C. and 240° C., preferably between 200° C. and 220° C., wherein the first peroxide has a half-life time of 1 hour at a first temperature T1/2 1 and the second peroxide has a half-life time of 1 hour at a second temperature T1/2 2, wherein T1/2 2 is higher than T1/2 1 and b) processing the composition obtained by step a) by a melt-blown process at temperatures between 240° C. and 300° C., preferably between 245° C. and 280° C., to provide the melt-blown fibers.
-
公开(公告)号:US20170137597A1
公开(公告)日:2017-05-18
申请号:US15129737
申请日:2015-03-23
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Rick Robert Emilie Bercx , Hendrik Kormelink
CPC classification number: C08K3/32 , B60R13/02 , C08K3/346 , C08K7/14 , C08K2003/325 , C08K2201/007 , C08L23/06 , C08L23/12 , C08L23/16 , C08L2205/025 , C08L2205/035 , G01N33/442
Abstract: The present invention relates to a polymer composition having low sensory impression of smell comprising a polypropylene and a calcium salt of phosphoric acid, wherein in said polymer composition the amount of said calcium salt of phosphoric acid is preferably such to accomplish a sensory impression of smell measured according to VDA 270 of at most 4.0.
-
-