公开(公告)号:US20230374333A1
公开(公告)日:2023-11-23
申请号:US18031057
申请日:2021-10-08
申请人: Resonac Corporation
发明人: Atsushi SUGAWARA , Jun KONISHI
IPC分类号: C09D133/08 , H01M50/434 , H01M50/42 , H01M50/423 , H01M50/429 , H01M50/451 , H01M4/62 , H01M4/13
CPC分类号: C09D133/08 , H01M50/434 , H01M50/42 , H01M50/423 , H01M50/4295 , H01M50/451 , H01M4/622 , H01M4/13
摘要: A coating composition can be applied with excellent high-speed coating properties and surface smoothness in a paint, an ink, and an adhesive which mainly contain polymers, or is a coating liquid for a positive electrode, a negative electrode, a separator, and the like of a lithium-ion secondary battery. The coating composition contains a filler, a binder, a thickener, and a solvent, wherein an aspect ratio of the filler is 2 or more, the binder is at least one selected from a diene rubber and a (meth)acrylate polymer, a viscosity of the coating composition is 1.0×106 Pa·s or less as measured at a shear rate of 0.01/s, and the following thixotropy index (TI) is 1.1×106 or more: [thixotropy index (TI)]=[viscosity of the coating composition as measured at a shear rate of 0.01/s]/[viscosity of the coating composition as measured at a shear rate of 10000/s].
-
2.
公开(公告)号:US20230348735A1
公开(公告)日:2023-11-02
申请号:US18025715
申请日:2021-09-14
申请人: Resonac Corporation
发明人: Jun KONISHI , Atsushi SUGAWARA
IPC分类号: C09D7/43 , C09D7/20 , C09D7/65 , C09D7/61 , H01M10/0525 , H01M50/417 , H01M4/62 , H01M50/457
CPC分类号: C09D7/43 , C09D7/20 , C09D7/65 , C09D7/61 , H01M10/0525 , H01M50/417 , H01M4/622 , H01M50/457
摘要: Provided is a coating liquid composition that is less likely to deform even when heat is applied to a coating liquid for a paint mainly containing a polymer, an ink, an adhesive, and an anode, a cathode, or a separator of a lithium ion battery, for example. The coating liquid composition includes a filler, a solvent, a dispersant, and a thickener. When the coating liquid composition is applied to a substrate to form a coating film having a thickness of 0.5 to 20 μm, the coating film has a shrinkage rate of 20.0% or less when heating at 200° C. for 15 minutes.
-
公开(公告)号:US20230374334A1
公开(公告)日:2023-11-23
申请号:US18031274
申请日:2021-10-08
申请人: Resonac Corporation
发明人: Atsushi SUGAWARA , Jun KONISHI
IPC分类号: C09D133/08 , C09D7/61 , H01M50/451 , H01M50/446 , H01M50/42 , H01M50/423 , H01M50/434 , H01M4/62 , H01M4/13
CPC分类号: C09D133/08 , C09D7/61 , H01M50/451 , H01M50/446 , H01M50/42 , H01M50/423 , H01M50/434 , H01M4/622 , H01M4/13
摘要: Provided is a composition capable of forming an easy-drying coating on an application surface in a paint, an ink, and an adhesive which mainly contain polymers, or a coating liquid for a positive electrode, a negative electrode, a separator, and the like of a lithium-ion secondary battery. The coating composition containing a filler, a binder, a thickener, and a solvent, wherein the binder is at least one selected from a diene rubber and a (meth)acrylate polymer; a viscosity of the coating composition is 1.0×106 Pa·s or less as measured at a shear rate of 0.01/s; and the following thixotropy index (TI) is 1.1×106 or more: [thixotropy index (TI)]=[viscosity of the coating composition as measured at a shear rate of 0.01/s]/[viscosity of the coating composition as measured at a shear rate of 10000/s].
-
4.
公开(公告)号:US20230352798A1
公开(公告)日:2023-11-02
申请号:US18025737
申请日:2021-09-14
申请人: Resonac Corporation
发明人: Jun KONISHI , Atsushi SUGAWARA
IPC分类号: H01M50/451 , C09D133/04 , C09D5/02 , C09D5/24 , C09D7/20 , C09D7/44 , C09D7/45 , C09D7/65 , C09D7/61 , C09D7/63 , H01M50/417 , H01M50/434 , H01M50/42 , H01M50/423 , H01M50/429 , H01M50/489 , H01M50/457 , H01M4/62
CPC分类号: H01M50/451 , C09D133/04 , C09D5/022 , C09D5/24 , C09D7/20 , C09D7/44 , C09D7/45 , C09D7/65 , C09D7/61 , C09D7/63 , H01M50/417 , H01M50/434 , H01M50/42 , H01M50/423 , H01M50/4295 , H01M50/489 , H01M50/457 , H01M4/622
摘要: Provided is a composition that can form a coating film having excellent surface smoothness and high heat deformation resistance in a coating liquid for a paint mainly containing a polymer, an ink, an adhesive, and an anode, a cathode, or a separator of a lithium ion battery, for example. A coating liquid composition includes a filler, a solvent, a dispersant, and a thickener. When the coating liquid composition is applied to a substrate to form a coating film having a thickness of 0.5 to 20 μm, the coating film has a shrinkage rate of 15.0% or less after heating at 170° C. for 15 minutes.
-
-
-