Abstract:
In an embodiment, a dielectric substrate comprises an unsintered polytetrafluoroethylene; and a high dielectric constant filler, wherein the dielectric constant of the high dielectric constant filler is greater than or equal to 35; wherein the dielectric substrate has a specific gravity of greater than or equal to 90% of a calculated theoretical density of the dielectric substrate, wherein the theoretical specific gravity is calculated based on a measured specific gravity of the high dielectric constant filler, the specific gravity of the unsintered polytetrafluoroethylene, and the relative weight fractions of the unsintered polytetrafluoroethylene and the high dielectric constant filler; and wherein the dielectric substrate has a dielectric constant of greater than or equal to 11.5 as determined at a frequency of 10 GHz.
Abstract:
A method of making a dielectric, Dk, electromagnetic, EM, structure, includes: providing a first mold portion comprising substantially identical ones of a first plurality of recesses arranged in an array; filling the first plurality of recesses with a curable first Dk composition having a first average dielectric constant greater than that of air after full cure; placing a substrate on top of and across multiple ones of the first plurality of recesses filled with the first Dk composition, and at least partially curing the curable first Dk composition; and, removing the substrate with the at least partially cured first Dk composition from the first mold portion, resulting in an assembly having the substrate and a plurality of Dk forms including the at least partially cured first Dk composition, each of the plurality of Dk forms having a three dimensional, 3D, shape defined by corresponding ones of the first plurality of recesses.
Abstract:
Disclosed herein is a hexaferrite composite comprising polytetrafluoroethylene; and greater than or equal to 40 vol %, or 40 to 90 vol % a plurality of Co2Z hexaferrite particles based on the total volume of the polytetrafluoroethylene and the plurality of Co2Z hexaferrite particles on a void-free basis; wherein the hexaferrite composite has a porosity of greater than or equal to 10 vol % based on the total volume of the hexaferrite composite; wherein the hexaferrite composite has a permeability of greater than or equal to 2.5 and a ratio of the permeability to the permittivity of greater than or equal to 0.4, both determined at 500 MHz.
Abstract:
Disclosed herein is a hexaferrite composite comprising polytetrafluoroethylene; and greater than or equal to 40 vol %, or 40 to 90 vol % a plurality of Co2Z hexaferrite particles based on the total volume of the polytetrafluoroethylene and the plurality of Co2Z hexaferrite particles on a void-free basis; wherein the hexaferrite composite has a porosity of greater than or equal to 10 vol % based on the total volume of the hexaferrite composite; wherein the hexaferrite composite has a permeability of greater than or equal to 2.5 and a ratio of the permeability to the permittivity of greater than or equal to 0.4, both determined at 500 MHz.
Abstract:
In an embodiment, a magneto-dielectric substrate comprises a dielectric polymer matrix; and a plurality of hexaferrite particles dispersed in the polymer matrix in an amount and of a type effective to provide a magneto-dielectric substrate having a magnetic constant of greater than or equal to 2.5 from 0 to 500 MHz, or 3 to 8 from 0 to 500 MHz; a magnetic loss of less than or equal to 0.1 from 0 to 500 MHz, or 0.001 to 0.05 over 0 to 500 MHz; and a dielectric constant of 1.5 to 8 or 2.5 to 8 from 0 to 500 MHz.
Abstract:
In an aspect, a Co2Y-type ferrite includes oxides of at least Ba, La, Co, Me, Fe, and optionally Ca; wherein Me is at least Ni and optionally one or more of Zn, Cu, Mn, or Mg. A composite can include the Co2Y-type ferrite and a polymer. An article can include the Co2Y-type ferrite.
Abstract:
In an embodiment, a magneto-dielectric substrate comprises a dielectric polymer matrix; and a plurality of hexaferrite particles dispersed in the dielectric polymer matrix in amount and of a type effective to provide the magneto-dielectric substrate with a magnetic constant of less than or equal to 3.5 from 500 MHz to 1 GHz, or 3 to 8 from 500 MHz to 1 GHz, and a magnetic loss of less than or equal to 0.1 from 0 to 1 GHz, or 0.001 to 0.07 over 0 to 1 GHz.
Abstract:
In an embodiment, a magneto-dielectric substrate comprises a dielectric polymer matrix; and a plurality of hexaferrite particles dispersed in the polymer matrix in an amount and of a type effective to provide a magneto-dielectric substrate having a magnetic constant of greater than or equal to 2.5 from 0 to 500 MHz, or 3 to 8 from 0 to 500 MHz; a magnetic loss of less than or equal to 0.1 from 0 to 500 MHz, or 0.001 to 0.05 over 0 to 500 MHz; and a dielectric constant of 1.5 to 8 or 2.5 to 8 from 0 to 500 MHz.
Abstract:
A method of making a dielectric, Dk, electromagnetic, EM, structure, includes: providing a first mold portion comprising substantially identical ones of a first plurality of recesses arranged in an array; filling the first plurality of recesses with a curable first Dk composition having a first average dielectric constant greater than that of air after full cure; placing a substrate on top of and across multiple ones of the first plurality of recesses filled with the first Dk composition, and at least partially curing the curable first Dk composition; and, removing the substrate with the at least partially cured first Dk composition from the first mold portion, resulting in an assembly having the substrate and a plurality of Dk forms including the at least partially cured first Dk composition, each of the plurality of Dk forms having a three dimensional, 3D, shape defined by corresponding ones of the first plurality of recesses.