Abstract:
A sintered product made from a starting batch containing 5 to 50% zircon and having the following average chemical composition, in weight percentages on the basis of the oxides and for a total of 100%: silica and zirconia, the zirconia content (ZrO2) being at least 64%, at least 0.2% of a dopant selected from V2O5, Nb2O5, Ta2O5, and mixtures thereof, optionally, a stabilizer selected from Y2O3, MgO, CaO, CeO2, and mixtures thereof, at a content of 6% or less, “other oxides” at a content of 6.7% or less.
Abstract:
Sintered product produced from a starting charge containing 75 to 99% zircon, and having the following average chemical composition by weight, the percentages by weight being based on the oxides: 60%
Abstract:
A sintered product having an average chemical composition such that, in weight percentages on the basis of the oxides: Cr2O3=80.0-99.0%; 0.5%≦TiO2≦9.0%; 0.2%≦MgO≦3.0%; and ZrO2≦5.0%, provided that the ratio of TiO2/MgO is between 1.5 and 9.0 and the molar ratio TiO2/Cr2O3 is less than 0.12.
Abstract:
Sintered product produced from a starting charge containing 75 to 99% zircon, and having the following average chemical composition by weight, the percentages by weight being based on the oxides: 60%
Abstract:
The present invention relates to a sintered product elaborated from a starting charge containing 75-99% of zircon, in mass percentage based on the oxides and having the following average weight chemical composition, in mass percentages based on the oxides 60%≦ZrO2≦72.8%, 27%≦SiO2≦36%, 0.1%≦B2O3+GeO2+P2O5+Sb2O3+Nb2O5+Ta2O5+V2O5, 0.1%≦ZnO+PbO+CdO, B2O3+GeO2+P2O5+Sb2O3+Nb2O5+Ta2O5+V2O5+ZnO+PbO+CdO≦5%, 0%≦Al2O3+TiO2+MgO+Fe2O3+NiO+MnO2+CoO+CuO≦5%, other oxides: ≦1.5%, for a total of 100%. Notably used in a glass furnace.
Abstract:
The present invention relates to a sintered product elaborated from a starting charge containing 75-99% of zircon, in mass percentage based on the oxides and having the following average weight chemical composition, in mass percentages based on the oxides 60%≦ZrO2≦72.8%, 27%≦SiO2≦36%, 0.1%≦B2O3+GeO2+P2O5+Sb2O3+Nb2O5+Ta2O5+V2O5, 0.1%≦ZnO+PbO+CdO, B2O3+GeO2+P2O5+Sb2O3+Nb2O5+Ta2O5+V2O5+ZnO+PbO+CdO≦5% 0% ≦Al2O3+TiO2+MgO+Fe2O3+NiO+MnO2+CoO+CuO≦5%, other oxides: ≦1.5%, for a total of 100%. Notably used in a glass furnace.
Abstract:
The invention provides a sintered product presenting an apparent density greater than 4.00 g/cm3 and having the following mean chemical composition, as a percentage by weight based on the oxides and for a total of 100%:Al2O2: complement to 100%16%≦Cr2O3≦29.5%TiO2 in a quantity such that the Cr2O3/TiO2 weight ratio is greater than 16 and less than 35, other species: ≦1%Application as an electrode bushing block.
Abstract translation:本发明提供具有大于4.00g / cm 3的表观密度并具有以下平均化学组成的烧结产品,其占氧化物的重量百分比,总计100%:Al 2 O 2:补充至100%16%< ; Cr2O3和NlE; 29.5%的TiO 2,其量使得Cr 2 O 3 / TiO 2重量比大于16且小于35,其它物质:≦̸ 1%用作电极套管块。
Abstract:
The invention provides a sintered product presenting an apparent density greater than 4.00 g/cm3 and having the following mean chemical composition, as a percentage by weight based on the oxides and for a total of 100%: Al2O2: complement to 100% 16%≦Cr2O3≦29.5% TiO2 in a quantity such that the Cr2O3/TiO2 weight ratio is greater than 16 and less than 35, other species: ≦1% Application as an electrode bushing block.