Abstract:
A sintered electroconductive oxide having a perovskite oxide type crystal structure represented by a compositional formula: M1aM2bMncAldCreOf wherein M1 represents at least one element selected from group 3 elements; and M2 represents at least one element selected from among Mg, Ca, Sr and Ba, wherein element M1 predominantly includes at least one element selected from Nd, Pr and Sm, and a, b, c, d, e and f satisfy the following relationships: 0.6005≦a
Abstract:
In a manufacturing method for a thermistor element (3) including: a thermistor portion (49) which is a sintered body formed from a thermistor material; and a pair of electrode wires (25) which are embedded in the thermistor portion (49) and at least one end portion of each of the electrode wires projects at an outer side of the thermistor portion (49), the resistance value of the thermistor element (3) is adjusted by performing a removal processing of removing a part of the thermistor portion (49).