公开(公告)号:US09605090B2
公开(公告)日:2017-03-28
申请号:US14416179
申请日:2013-07-22
发明人: Noriyuki Takahashi , Yasuo Saitoh
IPC分类号: B01J21/16 , C08F4/58 , B01J37/06 , B01J35/00 , C10G45/68 , B01J35/10 , B01J35/02 , B01J20/12 , C10G45/04
CPC分类号: C08F4/58 , B01J20/12 , B01J21/16 , B01J35/002 , B01J35/02 , B01J35/10 , B01J37/06 , C10G45/04 , C10G45/68
摘要: An activated clay for treating aromatic hydrocarbons, containing montmorillonite in an amount of not less than 34% by mass, having an SiO2/Al2O3 mol ratio in a range of 3.8 to 8.0, and desorbing ammonia in an amount in a range of 0.11 to 0.20 mmols/g as measured by the ammonia TPD method with the heat of adsorption in a range of 128 to 148 kJ/mol. The activated clay comprises an acid-treated product of smectite clay, imposes no limitation on the area where the starting clay is produced, and features long catalytic life free of dispersion in the properties.
-
公开(公告)号:US20150203603A1
公开(公告)日:2015-07-23
申请号:US14416179
申请日:2013-07-22
发明人: Noriyuki Takahashi , Yasuo Saitoh
IPC分类号: C08F4/58
CPC分类号: C08F4/58 , B01J20/12 , B01J21/16 , B01J35/002 , B01J35/02 , B01J35/10 , B01J37/06 , C10G45/04 , C10G45/68
摘要: An activated clay for treating aromatic hydrocarbons, containing montmorillonite in an amount of not less than 34% by mass, having an SiO2/Al2O3 mol ratio in a range of 3.8 to 8.0, and desorbing ammonia in an amount in a range of 0.11 to 0.20 mmols/g as measured by the ammonia TPD method with the heat of adsorption in a range of 128 to 148 kJ/mol. The activated clay comprises an acid-treated product of smectite clay, imposes no limitation on the area where the starting clay is produced, and features long catalytic life free of dispersion in the properties.
摘要翻译: 一种用于处理芳族烃的活性粘土,其含有不少于34质量%的具有SiO 2 / Al 2 O 3摩尔比在3.8至8.0的范围内的蒙脱石,并且以0.11至0.20的范围解吸氨 通过氨TPD法测得的吸附热量在128〜148kJ / mol的范围内。 活性白土包括蒙脱石粘土的酸处理产物,对起始粘土的生产区域没有限制,并具有长的催化剂寿命,不具有分散性。
-