公开(公告)号:US20220267880A1
公开(公告)日:2022-08-25
申请号:US17739385
申请日:2022-05-09
摘要: A method for producing a high temperature component includes a shaping step of shaping a powder compact of a desired high temperature component shape using a specific powder shaping method, from an alloy powder of γ′ precipitation strengthening-type Ni-based alloy, and a crystal grain coarsening step of coarsening a crystal grain size of the powder compact by heat treatment, wherein the powder compact contains 0.002% or more and 0.07% or less of C, and 5.40% or more and 8.40% or less of Al+Ti by mass percentage.
-
公开(公告)号:US20230313693A1
公开(公告)日:2023-10-05
申请号:US18199165
申请日:2023-05-18
IPC分类号: F01D5/28 , B23K26/342
CPC分类号: F01D5/288 , B23K26/342 , F05D2240/307 , F05D2230/31 , F05D2230/90 , F05D2300/611 , B23K2101/001
摘要: A rotor assembly component which is a component of a gas turbine engine is provided with a rotor assembly component body made from a metal, and a hard particle layer including a mass of hard particles and a matrix material, with the hard particles being made from a material harder than a material forming the rotor assembly component body. The matrix material is made solely from the material forming the rotor assembly component body. The hard particle layer is supported directly on a surface of the rotor assembly component body.
-
公开(公告)号:US20240009736A1
公开(公告)日:2024-01-11
申请号:US18025557
申请日:2021-09-10
CPC分类号: B22F10/28 , B22F10/64 , C22C19/056 , C22C19/057 , C22F1/10 , B33Y10/00
摘要: A shaped article production method includes: fabricating an intermediate article by powder bed fusion using a powder of a gamma prime precipitation strengthening Ni-based alloy; and heat-treating the intermediate article. The Ni-based alloy contains, in percent by mass, 7.0 to 17.0% Cr, 7.0 to 12.0% Co, 5.0 to 8.0% Al+Ti, 2.0 to 12.0% W, 1.5 to 4.4% Nb+Ta, 2.3% or less Mo, 0.3% or less C, 2.0% or less Hf, and 0.2% or less Zr. The fabricating the intermediate article includes applying a laser beam to a layer (3) of the powder along scan lines (4) parallel to one another. In applying the laser beam, a value obtained by dividing a pitch between the scan lines (4) by a laser spot diameter is in the range of 0.6 to 1.1.
-
公开(公告)号:US20240149339A1
公开(公告)日:2024-05-09
申请号:US18280980
申请日:2022-03-07
IPC分类号: B22F7/06 , B22F3/10 , B22F3/16 , B22F3/22 , B22F7/00 , B23K1/00 , B23K1/19 , B23K35/30 , B32B15/01 , C22C19/05
CPC分类号: B22F7/06 , B22F3/10 , B22F3/16 , B22F3/225 , B22F7/008 , B23K1/0008 , B23K1/19 , B23K35/304 , B32B15/01 , C22C19/055 , B22F2301/15 , B22F2998/10 , B22F2999/00
摘要: A first pre-sintered body composed of a powder made of a first Ni-based alloy is prepared, and a second pre-sintered body composed of a powder made of a second Ni-based alloy is prepared. Subsequently, the first and second pre-sintered bodies are positioned to face each other across a predetermined gap, and a joining material made of a Ni-based alloy having a lower liquidus temperature than the first and second Ni-based alloys is placed in a space that adjoins the first and second pre-sintered bodies and to which the gap opens. After the placing of the joining material, the first and second pre-sintered bodies are heated to melt the joining material, fill the gap with the molten joining material, and subsequently turn the first and second pre-sintered bodies into first and second sintered bodies, respectively.
-
公开(公告)号:US20200087754A1
公开(公告)日:2020-03-19
申请号:US16616285
申请日:2018-05-11
摘要: A method for producing a high temperature component includes a shaping step of shaping a powder compact of a desired high temperature component shape using a specific powder shaping method, from an alloy powder of γ′ precipitation strengthening-type Ni-based alloy, and a crystal grain coarsening step of coarsening a crystal grain size of the powder compact by heat treatment, wherein the powder compact contains 0.002% or more and 0.07% or less of C, and 5.40% or more and 8.40% or less of Al+Ti by mass percentage.
-
-
-
-