METHOD OF MAKING A CEMENTED CARBIDE POWDER WITH LOW SINTERING SHRINKAGE AND THE POWDER OBTAINED
    1.
    发明申请
    METHOD OF MAKING A CEMENTED CARBIDE POWDER WITH LOW SINTERING SHRINKAGE AND THE POWDER OBTAINED 审中-公开
    制造具有低烧结收缩率的粉末碳化硅粉末和获得的粉末的方法

    公开(公告)号:US20100260641A1

    公开(公告)日:2010-10-14

    申请号:US12680264

    申请日:2008-09-24

    Applicant: Jan Qvick

    Inventor: Jan Qvick

    Abstract: A method of making cemented carbide powder with low sintering shrinkage including WC and 4-15 wt-% Co and up to 20 wt-% cubic carbide forming elements from the Groups 4 and 5 of the Periodic Table of the Elements by the powder metallurgical techniques wet milling, pressing and sintering. According to the method wet milling is performed in a rotating ball mill with a ratio between the weight of milling bodies and powder of 2-5. The milling bodies are shaped either as spheres or cylinders with semi-spherical end surfaces. The spherical bodies have a diameter of 10 to 15 mm and the cylindrical bodies have a diameter and height of 10 to 15 mm. The composition of the milling bodies is WC with 6 to 10 wt-% Co. A powder made according to the method is described.

    Abstract translation: 通过粉末冶金技术制造具有低烧结收缩率的硬质合金粉末的方法,其包括WC和4-15重量%Co以及元素周期表第4和5组中至多20重量%的立方碳化物形成元素 湿磨,压制和烧结。 根据该方法,在旋转式球磨机中进行湿法研磨,研磨体重量与粉末重量之间的比例为2-5。 碾磨体成形为具有半球形端面的球体或圆柱体。 球体的直径为10〜15mm,圆柱体的直径和高度为10〜15mm。 研磨体的组成为6〜10重量%的WC。根据该方法制造的粉末进行了说明。

    FINE GRAINED CEMENTED CARBIDE POWDER MIXTURE WITH LOW SINTERING SHRINKAGE AND METHOD OF MAKING THE SAME
    3.
    发明申请
    FINE GRAINED CEMENTED CARBIDE POWDER MIXTURE WITH LOW SINTERING SHRINKAGE AND METHOD OF MAKING THE SAME 审中-公开
    具有低烧结收缩率的精细粉碎的碳化硅粉末混合物及其制备方法

    公开(公告)号:US20110271605A1

    公开(公告)日:2011-11-10

    申请号:US13145117

    申请日:2010-02-16

    Applicant: Jan Qvick

    Inventor: Jan Qvick

    CPC classification number: C22C29/08

    Abstract: A fine grained cemented carbide powder mixture for cutting tool inserts for metal machining includes WC-powder with a Scott density of 2.75-3.75 g/cm3 and a compacting density after dry pressing at 100 MPa within 8.8-9.8 g/cm3. The sintering shrinkage of the fine grained cemented carbide powder mixture is 16.8 to 17.9% at a compacting pressure of 150 MPa. A method of making the powder mixture is also described.

    Abstract translation: 用于金属加工的切削工具刀片的细粒硬质合金粉末混合物包括Scott密度为2.75-3.75g / cm 3的WC粉末和在8.8MPa至9.8g / cm 3的100MPa下干压后的压实密度。 在150MPa的压实压力下,细晶粒硬质合金粉末混合物的烧结收缩率为16.8〜17.9%。 还描述了制备粉末混合物的方法。

    Cemented carbide with binder phase enriched surface zone
    4.
    发明授权
    Cemented carbide with binder phase enriched surface zone 失效
    具有粘结相富集表面区的硬质合金

    公开(公告)号:US06913843B2

    公开(公告)日:2005-07-05

    申请号:US10846641

    申请日:2004-05-17

    Abstract: A cutting tool insert has a cemented carbide substrate and a coating. The cemented carbide substrate includes 73-93 wt % WC, 4-12 wt % binder phase, and cubic carbide phase with a binder phase enriched surface zone essentially free of cubic carbide phase. The cubic carbide phase includes elements from the groups IVB and VB, with the Ta content on a level corresponding to a technical impurity. Inserts according to the invention exhibit favorable edge strength and thermal shock resistance.

    Abstract translation: 切削刀具刀片具有硬质合金基底和涂层。 硬质合金基体包括73-93重量%的WC,4-12重量%的粘结相和具有基本上不含立方晶碳相的粘结相富集表面区的立方碳化物相。 立方晶碳相包括来自IVB和VB族的元素,其Ta含量对应于技术杂质。 根据本发明的插入件显示出有利的边缘强度和耐热冲击性。

    Method of making submicron cemented carbide cutting tool inserts
    6.
    发明授权
    Method of making submicron cemented carbide cutting tool inserts 失效
    制造亚微米硬质合金刀具刀片的方法

    公开(公告)号:US06336951B1

    公开(公告)日:2002-01-08

    申请号:US09252976

    申请日:1999-02-19

    Abstract: An improved method of making submicron cemented carbide bodies include wet milling powders of WC and Co and grain growth inhibitors to a slurry, drying the slurry to a powder, uniaxial pressing of the powder to form bodies of a desired shape, and sintering. WC powder is provided with an FSSS grain size, dwc, of less than 1 &mgr;m and a Co powder with an FSSS grain size, dco, such that the ratio dwc/dco is 0.75-1.5.

    Abstract translation: 制造亚微米硬质合金体的改进方法包括WC和Co的湿磨粉末和浆料的晶粒生长抑制剂,将浆料干燥成粉末,单轴压制粉末以形成所需形状的体并进行烧结。 WC粉末具有小于1um的FSSS粒度dwc和具有FSSS晶粒尺寸dco的Co粉末,使得dwc / dco的比例为0.75-1.5。