STEEL AND METHOD OF PRODUCING SAME

    公开(公告)号:US20220275489A1

    公开(公告)日:2022-09-01

    申请号:US17635377

    申请日:2020-08-18

    摘要: The steel of the present disclosure contains, in mass %, C: 0.100% to 0.700%, Si: 0.05% to 1.00%, Mn: 20.0% to 40.0%, P: ≤0.030%, S: ≤0.0050%, Al: 0.01% to 5.00%, Cr: 0.5% to 7.0%, N: 0.0050% to 0.0500%, O: ≤0.0050%, Ti: ≤0.005%, Nb: ≤0.005%, and at least one selected from Ca: 0.0005% to 0.0100%, Mg: 0.0005% to 0.0100%, and REM: 0.0010% to 0.0200%, and has a microstructure with austenite as matrix, where an average grain size is 50 μm or less, a cleanliness of sulfide inclusion is less than 1.0%, a yield strength is 400 MPa or more, and a percent brittle fracture after a Charpy impact test at −269° C. is less than 5%.

    HIGH-Mn STEEL AND METHOD OF PRODUCING SAME

    公开(公告)号:US20210301378A1

    公开(公告)日:2021-09-30

    申请号:US17264295

    申请日:2019-07-31

    摘要: Provided is a high-Mn steel having excellent low-temperature toughness and excellent surface characteristics. A high-Mn steel comprises: a chemical composition containing, in mass %, C: 0.100 to 0.700%, Si: 0.05 to 1.00%, Mn: 20.0 to 35.0%, P: ≤0.030%, S: ≤0.0070%, Al: 0.010 to 0.070%, Cr: 0.50 to 5.00%, N: 0.0050 to 0.0500%, O: ≤0.0050%, Ti: ≤0.005%, and Nb: ≤0.005%, with a balance consisting of Fe and inevitable impurities; and a microstructure having austenite as a matrix, wherein in the microstructure, a Mn concentration of a Mn-concentrated portion is 38.0% or less, and an average KAM value is 0.3 or more, yield stress is 400 MPa or more, absorbed energy vE−196 in a Charpy impact test at −196° C. is 100 J or more, and percent brittle fracture is less than 10%.

    SUBMERGED ARC WELDED JOINT
    7.
    发明公开

    公开(公告)号:US20240051070A1

    公开(公告)日:2024-02-15

    申请号:US18277833

    申请日:2022-02-28

    IPC分类号: B23K35/30 B23K9/18

    摘要: A submerged arc welded joint in a high-Mn content steel material that can be formed with reduced occurrence of hot cracking during the welding process and has high strength and excellent cryogenic impact toughness. In the welded joint, the high-Mn content steel material has a chemical composition including, by mass %, C: 0.10 to 0.80%, Si: 0.05 to 1.00%, Mn: 18.0 to 30.0%, P: 0.030% or less, S: 0.0070% or less, Al: 0.010 to 0.070%, Cr: 2.5 to 7.0%, N: 0.0050 to 0.0500%, and O: 0.0050% or less, the balance being Fe and incidental impurities, and a weld metal has a chemical composition including C: 0.10 to 0.80%, Si: 0.05 to 1.00%, Mn: 15.0 to 30.0%, P: 0.030% or less, S: 0.030% or less, Al: 0.100% or less, Cr: 6.0 to 14.0%, and N: 0.100% or less, the balance being Fe and incidental impurities.