Double-blown PET bottle shaped container having essentially no residual
stress and superior heat resistance
    1.
    发明授权
    Double-blown PET bottle shaped container having essentially no residual stress and superior heat resistance 失效
    基本上没有残余应力和优异的耐热性的双吹PET瓶形容器

    公开(公告)号:US5562960A

    公开(公告)日:1996-10-08

    申请号:US327893

    申请日:1994-10-24

    摘要: A biaxially oriented polyethylene terephthalate resin bottle-shaped container, and method of blow-molding the same, is disclosed. The method comprises the steps of heating the body portion of a preform at 90.degree. C. to 130.degree. C., biaxial-orientation blow-molding the preform in a primary blowing mold heated at 110.degree. C. to 230.degree. C. to form a primary intermediate molded bottle-shaped piece, heating the primary intermediate molded bottle-shaped piece at 130.degree. C. to 255.degree. C. or at a temperature which is at least 20.degree. C. greater than the primary blowing mold temperature to form a secondary intermediate molded bottle-shaped piece, and blow-molding the secondary intermediate molded bottle-shaped piece in a secondary blowing mold heated at 100.degree. C. to 150.degree. C. to form a bottle-shaped container. The temperature of the secondary blowing mold is several degrees greater than the maximum temperature the molded bottle-shaped container will be subjected to during use. The bottle-shaped container of the present invention has no stress remaining from biaxial orientation blow-molding and has a high heat resistance temperature value.

    摘要翻译: 公开了一种双轴取向的聚对苯二甲酸乙二醇酯树脂瓶形容器及其吹塑方法。 该方法包括以下步骤:将预制件的主体部分在90℃至130℃加热,双轴取向吹塑预成型体,在加热至110℃至230℃的初级吹塑模具中形成 初级中间成型瓶形件,在130℃至255℃或比初级吹塑模具温度高至少20℃的温度下加热初级中间成型瓶形件,以形成 二次中间成型的瓶形件,并将二次中间成型的瓶形件吹塑到加热至100℃至150℃的二次吹塑模具中以形成瓶形容器。 二次吹塑模具的温度比成型瓶形容器在使用过程中经受的最高温度大几度。 本发明的瓶状容器在双轴取向吹塑成型中没有应力残留,耐热温度高。

    Method of blow-molding biaxially oriented polyethylene terephthalate
resin bottle-shaped container
    2.
    发明授权
    Method of blow-molding biaxially oriented polyethylene terephthalate resin bottle-shaped container 失效
    双轴取向聚对苯二甲酸乙二醇酯树脂瓶形容器吹塑方法

    公开(公告)号:US5510079A

    公开(公告)日:1996-04-23

    申请号:US472922

    申请日:1995-06-07

    摘要: A method of blow-molding a biaxially-oriented polyethylene terephthalate resin bottle-shaped container having high heat resistance and substantially no residual stress is disclosed. The method comprises the steps of: providing a preform with a neck and a body; heating the preform to an orienting temperature; first biaxial-orientation blow-molding the preform in a first mold which is at a first temperature to biaxially stretch the preform to form a primary intermediate molded bottle-shaped piece that is larger than the bottle-shaped container and having an area magnification of at least 5 times the preform, the biaxial stretching creating residual stress in the primary intermediate molded bottle-shaped piece; causing thermal contraction of the primary intermediate molded bottle-shaped piece by heating the primary intermediate molded bottle-shaped piece to a temperature higher than the first temperature to form a secondary intermediate molded bottle-shaped piece and to eliminate residual stress caused by the first blow-molding; and second blow-molding the secondary intermediate molded bottle-shaped piece in a second mold to form the bottle-shaped container, wherein orientation magnification of the secondary intermediate molded bottle-shaped piece is small compared to orientation magnification of the primary intermediate molded bottle-shaped piece and substantially no stress is created during the second blow-molding.

    摘要翻译: 公开了一种吹塑成型具有高耐热性且基本上没有残余应力的双轴取向聚对苯二甲酸乙二醇酯树脂瓶形容器的方法。 该方法包括以下步骤:为颈部和身体提供预型件; 将预成型件加热到定向温度; 在第一模具中将第一双轴取向吹塑成型坯,该第一模具处于第一温度以双轴拉伸预型件,以形成大于瓶形容器的大于瓶形容器的初级中间成型瓶形件,并具有面积放大倍数 至少是预制件的5倍,双轴拉伸在初级中间成型瓶形件中产生残余应力; 通过将初级中间成型瓶形件加热到高于第一温度的温度来引起初级中间成型瓶形件的热收缩,以形成第二中间成型瓶形件,并消除由第一次吹塑引起的残余应力 模具 将第二中间成型瓶状件在第二模具中吹塑成型以形成瓶形容器,其中二次中间成型瓶形件的取向倍率与初级中间成型瓶形件的取向放大率相比较小, 并且在第二次吹塑成型期间基本上没有产生应力。

    Double-blown pet bottle shaped container having essentially no residual
stress and superior heat resistance
    4.
    发明授权
    Double-blown pet bottle shaped container having essentially no residual stress and superior heat resistance 失效
    双吹宠物瓶形容器基本上没有残余应力和优异的耐热性

    公开(公告)号:US5928742A

    公开(公告)日:1999-07-27

    申请号:US980019

    申请日:1997-11-26

    摘要: A biaxially oriented polyethylene terephthalate resin bottle-shaped container, and method of blow-molding the same, is disclosed. The method comprises the steps of heating the body portion of a preform at 90.degree. to 130.degree. C., biaxial-orientation blow-molding the preform in a primary blowing mold heated at 110 to 230.degree. C. to form a primary intermediate molded bottle-shaped piece, heating the primary intermediate molded bottle-shaped piece at 130 to 255.degree. C. or at a temperature which is at least 20.degree. C. greater than the primary blowing mold temperature to form a secondary intermediate molded bottle-shaped piece, and blow-molding the secondary intermediate molded bottle-shaped piece in a secondary blowing mold heated at 100.degree. to 150.degree. C. to form a bottle-shaped container. The temperature of the secondary blowing mold is several degrees greater than the maximum temperature the molded bottle-shaped container will be subjected to during use. The bottle-shaped container of the present invention has no stress remaining from biaxial orientation blow-molding and has a high heat resistance temperature value.

    摘要翻译: 公开了一种双轴取向的聚对苯二甲酸乙二醇酯树脂瓶形容器及其吹塑方法。 该方法包括以下步骤:将预制件的主体部分在90°至130℃加热,双轴取向吹塑成型预成型件,该模具加热至110-230℃,以形成初级中间模塑瓶 在130-255℃或比初级吹塑模具温度高至少20℃的温度下加热初级中间模塑瓶形件以形成二次中间成型瓶形件, 并将二次中间成型的瓶形件吹塑在加热至100-150℃的二次吹塑模具中以形成瓶形容器。 二次吹塑模具的温度比成型瓶形容器在使用过程中经受的最高温度大几度。 本发明的瓶状容器在双轴取向吹塑成型中没有应力残留,耐热温度高。

    Intermediate product capable of being formed into a biaxially oriented
polyethylene terephthalate resin bottle-shaped container and method of
blow-molding the same
    5.
    发明授权
    Intermediate product capable of being formed into a biaxially oriented polyethylene terephthalate resin bottle-shaped container and method of blow-molding the same 失效
    能够形成双轴取向的聚对苯二甲酸乙二醇酯树脂瓶形容器的中间产物及其吹塑成型方法

    公开(公告)号:US5747130A

    公开(公告)日:1998-05-05

    申请号:US683431

    申请日:1996-07-18

    摘要: A biaxially oriented polyethylene terephthalate resin bottle-shaped container, and method of blow-molding the same, is disclosed. The method comprises the steps of heating the body portion of a preform at 90.degree. to 130.degree. C., biaxial-orientation blow-molding the preform in a primary blowing mold heated at 110.degree. to 230.degree. C. to form a primary intermediate molded bottle-shaped piece, heating the primary intermediate molded bottle-shaped piece at 130.degree. to 255.degree. C. or at a temperature which is at least 20.degree. C. greater than the primary blowing mold temperature to form a secondary intermediate molded bottle-shaped piece, and blow-molding the secondary intermediate molded bottle-shaped piece in a secondary blowing mold heated at 100.degree. to 150.degree. C. to form a bottle-shaped container. The temperature of the secondary blowing mold is several degrees greater than the maximum temperature the molded bottle-shaped container will be subjected to during use. The bottle-shaped container of the present invention has no stress remaining from biaxial orientation blow-molding and has a high heat resistance temperature value.

    摘要翻译: 公开了一种双轴取向的聚对苯二甲酸乙二醇酯树脂瓶形容器及其吹塑方法。 该方法包括以下步骤:将预成型体的主体部分加热到90℃至130℃,双轴取向吹塑成型预成型坯,在初始吹塑模具中加热至110℃至230℃,以形成初级中间成型 瓶形件,将初级中间成型瓶形件在130℃至255℃或在比初始吹塑模具温度高至少20℃的温度下加热以形成二次中间成型瓶形 将二次中间成型的瓶状件吹塑成加热至100-150℃的二次吹塑成型体,形成瓶状容器。 二次吹塑模具的温度比成型瓶形容器在使用过程中经受的最高温度大几度。 本发明的瓶状容器在双轴取向吹塑成型中没有应力残留,耐热温度高。

    Method of blow-molding biaxially-oriented polyethylene terephthalate
resin bottle-shaped container
    6.
    发明授权
    Method of blow-molding biaxially-oriented polyethylene terephthalate resin bottle-shaped container 失效
    双轴取向聚对苯二甲酸乙二醇酯树脂瓶形容器吹塑方法

    公开(公告)号:US5445784A

    公开(公告)日:1995-08-29

    申请号:US327894

    申请日:1994-10-24

    摘要: A biaxially oriented polyethylene terephthalate resin bottle-shaped container, and method of blow molding the same by heating the body portion of a preform at 90.degree. C. to 130.degree. C., biaxial-orientation blow-molding the preform in a primary blowing mold heated at 110.degree. C. to 230.degree. C. to form a primary intermediate molded bottle-shaped piece, heating the primary intermediate molded bottle-shaped piece at 130.degree. C. to 255.degree. C. or at a temperature which is 20.degree. C. or higher than the primary blowing mold temperature to form a secondary intermediate molded bottle-shaped piece, and blow-molding the secondary intermediate molded bottle-shaped piece in a secondary blowing mold heated at 100.degree. C. to 150.degree. C. to form a bottle-shaped container. The temperature of the secondary blowing mold is several degrees greater than the maximum temperature the molded bottle-shaped container will be subjected to during use. The bottle-shaped container has no stress remaining from biaxial orientation blow-molding and has a high heat resistance temperature value.

    摘要翻译: 双轴取向的聚对苯二甲酸乙二醇酯树脂瓶形容器,以及通过在90℃至130℃下加热预成型体的主体部分来吹塑成型方法,在一次吹塑模具中双轴取向吹塑预制件 加热至110℃至230℃,形成初级中间成型瓶形件,将初级中间成型瓶形件加热至130℃至255℃或温度为20℃ 或高于初级吹塑模具温度,以形成二次中间成型瓶形件,并将二次中间成型的瓶形件吹塑到加热至100℃至150℃的二次吹塑模具中以形成 一个瓶形容器。 二次吹塑模具的温度比成型瓶形容器在使用过程中经受的最高温度大几度。 瓶形容器从双轴取向吹塑成型中没有应力残留,并且具有高的耐热温度值。

    Biaxial orientation blow molding process
    9.
    发明授权
    Biaxial orientation blow molding process 有权
    双轴取向吹塑成型工艺

    公开(公告)号:US07316798B2

    公开(公告)日:2008-01-08

    申请号:US10495866

    申请日:2003-01-22

    IPC分类号: B29C49/18

    摘要: The double blow molding process comprises a primary blow molding step of biaxially drawing and blow molding the preform into a primary intermediate product, a step of heating the primary intermediate product to shrink-mold it into the secondary intermediate product, and a secondary blow molding step of molding the secondary intermediate product into a bottle. This double blow molding process is characterized in that, just before the secondary blow molding step, the secondary intermediate product on standby is maintained at a temperature at least 40° C. or 50° C. higher than the mold temperature used in said secondary blow molding step. From such a temperature, it is possible to determine the double blow molding conditions, which can correspond to the levels of heat resistance required for the bottles, and to provide, with high productivity, the bottles having necessary levels of heat resistance.

    摘要翻译: 双吹模法包括将预成型坯双轴拉伸和吹塑成初级中间产品的一次吹塑成型步骤,加热初级中间产品以将其收缩成二次中间产品的步骤和二次吹塑步骤 将次级中间产品模制成瓶子。 这种双吹模法的特征在于,在二次吹塑步骤之前,备用的二次中间产品保持在比所述二次吹塑中使用的模具温度高至少40℃或50℃的温度 成型步骤。 从这样的温度,可以确定双重吹塑条件,其可以对应于瓶子所需的耐热水平,并且以高生产率提供具有必要的耐热水平的瓶子。