Lithium cell with iron disulfide cathode
    8.
    发明申请
    Lithium cell with iron disulfide cathode 审中-公开
    锂电池与二硫化铁阴极

    公开(公告)号:US20100203370A1

    公开(公告)日:2010-08-12

    申请号:US12378255

    申请日:2009-02-12

    IPC分类号: H01M6/10 H01M6/16 H01M2/02

    摘要: A primary cell having an anode comprising lithium or lithium alloy and a cathode comprising iron disulfide (FeS2) and carbon particles. The electrolyte comprises a lithium salt preferably lithium iodide (LiI) dissolved in an organic solvent mixture. The solvent mixture preferably comprises dioxolane and dimethoxyethane. The electrolyte typically contains between about 100 and 2000 parts by weight water per million parts by weight (ppm) electrolyte therein. The anode may be lithium metal or preferably is a lithium alloy. A cathode slurry is prepared comprising iron disulfide powder, carbon, binder, and a liquid solvent. The mixture is coated onto a conductive substrate and solvent evaporated leaving a dry cathode coating on the substrate. The anode and cathode can be spirally wound with separator therebetween and inserted into the cell casing with electrolyte then added.

    摘要翻译: 具有包含锂或锂合金的阳极和包含二硫化铁(FeS 2)和碳颗粒的阴极的初级电池。 电解质包含溶解在有机溶剂混合物中的锂盐,优选碘化锂(LiI)。 溶剂混合物优选包括二氧戊环和二甲氧基乙烷。 电解液通常含有每百万重量份(ppm)电解质中约100至2000重量份的水。 阳极可以是锂金属,或者优选是锂合金。 制备包含二硫化铁粉末,碳,粘合剂和液体溶剂的阴极浆料。 将混合物涂覆到导电基材上,并蒸发溶剂,在基材上留下干燥的阴极涂层。 阳极和阴极可以用分离器螺旋卷绕并插入电池壳体中,然后加入电解质。

    Lithium cell
    9.
    发明申请
    Lithium cell 有权
    锂电池

    公开(公告)号:US20090208849A1

    公开(公告)日:2009-08-20

    申请号:US12069953

    申请日:2008-02-14

    IPC分类号: H01M6/16 H01M4/82

    摘要: A primary cell having an anode comprising lithium or lithium alloy and a cathode comprising iron disulfide (FeS2) and carbon particles. The electrolyte comprises a lithium salt preferably lithium iodide (LiI) dissolved in an organic solvent mixture. The solvent mixture preferably comprises dioxolane, dimethoxyethane and sulfolane. The electrolyte typically contains between about 100 and 2000 parts by weight water per million parts by weight (ppm) electrolyte therein. A cathode slurry is prepared comprising iron disulfide powder, carbon, binder, and a liquid solvent. The mixture is coated onto a conductive substrate and solvent evaporated leaving a dry cathode coating on the substrate. The anode and cathode can be spirally wound with separator therebetween and inserted into the cell casing with electrolyte then added.

    摘要翻译: 具有包含锂或锂合金的阳极和包含二硫化铁(FeS 2)和碳颗粒的阴极的初级电池。 电解质包含溶解在有机溶剂混合物中的锂盐,优选碘化锂(LiI)。 溶剂混合物优选包括二氧戊环,二甲氧基乙烷和环丁砜。 电解液通常含有每百万重量份(ppm)电解质中约100至2000重量份的水。 制备包含二硫化铁粉末,碳,粘合剂和液体溶剂的阴极浆料。 将混合物涂覆到导电基材上,并蒸发溶剂,在基材上留下干燥的阴极涂层。 阳极和阴极可以用分离器螺旋卷绕并插入电池壳体中,然后加入电解质。