公开(公告)号:US20140323365A1
公开(公告)日:2014-10-30
申请号:US14360643
申请日:2012-12-14
申请人: Chad Henry Kamann , Robert A. Green
发明人: Chad Henry Kamann , Robert A. Green
CPC分类号: D01F6/92 , A01G13/0275 , C08L67/04 , C09K8/44 , C09K8/467 , C09K8/56 , C09K8/62 , C09K8/70 , C09K8/80 , C09K2208/08 , D01F6/625 , D10B2331/041 , D10B2505/18 , E21B43/26
摘要: Polylactide fibers are made from a blend of polylactides. One of the polylactides has a ratio of R-lactic and S-lactic units from 8:92 to 92:8. The second polylactide has a ratio of the R-lactic and S-lactic units of >97:3 or
摘要翻译: 聚丙交酯纤维由聚丙交酯的共混物制成。 一种聚丙交酯的R-乳酸和S-乳酸单元的比例为8:92至92:8。 第二聚丙交酯的R-乳酸和S-乳酸单位的比例> 97:3或<3:97。 混合物中R-乳酸单元与S-乳酸单元的比例为7:93至25:75或75:25至93:7。 聚丙交酯纤维在纤维中含有每克聚丙交酯树脂至少5焦耳的聚丙交酯微晶。
-
公开(公告)号:US09404032B2
公开(公告)日:2016-08-02
申请号:US14360643
申请日:2012-12-14
申请人: Chad Henry Kamann , Robert A. Green
发明人: Chad Henry Kamann , Robert A. Green
IPC分类号: C09K8/60 , C09K8/62 , C09K8/70 , D01F6/62 , D01F6/92 , A01G13/00 , C09K8/467 , C09K8/80 , C08L67/04 , C09K8/56 , E21B43/26
CPC分类号: D01F6/92 , A01G13/0275 , C08L67/04 , C09K8/44 , C09K8/467 , C09K8/56 , C09K8/62 , C09K8/70 , C09K8/80 , C09K2208/08 , D01F6/625 , D10B2331/041 , D10B2505/18 , E21B43/26
摘要: Polylactide fibers are made from a blend of polylactides. One of the polylactides has a ratio of R-lactic and S-lactic units from 8:92 to 92:8. The second polylactide has a ratio of the R-lactic and S-lactic units of >97:3 or
摘要翻译: 聚丙交酯纤维由聚丙交酯的共混物制成。 一种聚丙交酯的R-乳酸和S-乳酸单元的比例为8:92至92:8。 第二聚丙交酯的R-乳酸和S-乳酸单位的比例> 97:3或<3:97。 混合物中R-乳酸单元与S-乳酸单元的比例为7:93至25:75或75:25至93:7。 聚丙交酯纤维在纤维中含有每克聚丙交酯树脂至少5焦耳的聚丙交酯微晶。
-
公开(公告)号:US20100308494A1
公开(公告)日:2010-12-09
申请号:US12679365
申请日:2008-09-26
IPC分类号: B29C47/08
摘要: PLA stereocomplex fibers are made by separately melting a high-D PLA starting resin and a high-L starting resin, mixing the melts and spinning the molten mixture. Subsequent heat treatment introduces high-melting “stereocomplex” crystallinity into the fibers. The process can form fibers having a high content of “stereocomplex” crystallites that have a high melting temperature. As a result, the fibers have excellent thermal resistance. The process is also easily adaptable to commercial melt spinning operations.
摘要翻译: PLA立体复合纤维通过分开熔融高D PLA起始树脂和高-L起始树脂,混合熔体并纺丝熔融混合物而制成。 随后的热处理将高熔点的“立体复合物”结晶引入纤维中。 该方法可以形成具有高含量的具有高熔点的“立体络合物”晶体的纤维。 结果,纤维具有优异的耐热性。 该方法也易于适应商业熔融纺丝操作。
-
公开(公告)号:US08377353B2
公开(公告)日:2013-02-19
申请号:US12679373
申请日:2008-09-26
CPC分类号: D01F6/92 , D01F6/625 , D01F8/14 , Y10T428/1352 , Y10T428/2929
摘要: Conjugate fibers are prepared in which at least one segment is a mixture of a high-D PLA resin and a high-L PLA resin. These segments have crystallites having a crystalline melting temperature of at least 200° C. At least one other segment is a high-D PLA resin or a high-L PLA resin. The conjugate fibers may be, for example, bicomponent, multi-component, islands-in-the-sea or sheath-and-core types. Specialty fibers of various types can be made through further downstream processing of these conjugate fibers.
摘要翻译: 制备共轭纤维,其中至少一个片段是高D PLA树脂和高-L PLA树脂的混合物。 这些段具有结晶熔融温度至少为200℃的微晶。至少另一个区段是高D PLA树脂或高-L PLA树脂。 复合纤维可以是例如双组分,多组分,海岛或鞘和核型。 各种类型的特种纤维可以通过这些共轭纤维的进一步下游加工制成。
-
公开(公告)号:US08182725B2
公开(公告)日:2012-05-22
申请号:US12679365
申请日:2008-09-26
摘要: PLA stereocomplex fibers are made by separately melting a high-D PLA starting resin and a high-L starting resin, mixing the melts and spinning the molten mixture. Subsequent heat treatment introduces high-melting “stereocomplex” crystallinity into the fibers. The process can form fibers having a high content of “stereocomplex” crystallites that have a high melting temperature. As a result, the fibers have excellent thermal resistance. The process is also easily adaptable to commercial melt spinning operations.
摘要翻译: PLA立体复合纤维通过分开熔融高D PLA起始树脂和高-L起始树脂,混合熔体并纺丝熔融混合物而制成。 随后的热处理将高熔点的“立体复合物”结晶引入纤维中。 该方法可以形成具有高含量的具有高熔点的“立体络合物”晶体的纤维。 结果,纤维具有优异的耐热性。 该方法也易于适应商业熔融纺丝操作。
-
公开(公告)号:US20100221471A1
公开(公告)日:2010-09-02
申请号:US12679373
申请日:2008-09-26
CPC分类号: D01F6/92 , D01F6/625 , D01F8/14 , Y10T428/1352 , Y10T428/2929
摘要: Conjugate fibers are prepared in which at least one segment is a mixture of a high-D PLA resin and a high-L PLA resin. These segments have crystallites having a crystalline melting temperature of at least 200° C. At least one other segment is a high-D PLA resin or a high-L PLA resin. The conjugate fibers may be, for example, bicomponent, multi-component, islands-in-the-sea or sheath-and-core types. Specialty fibers of various types can be made through further downstream processing of these conjugate fibers.
摘要翻译: 制备共轭纤维,其中至少一个片段是高D PLA树脂和高-L PLA树脂的混合物。 这些段具有结晶熔融温度至少为200℃的微晶。至少另一个区段是高D PLA树脂或高-L PLA树脂。 复合纤维可以是例如双组分,多组分,海岛或鞘和核型。 各种类型的特种纤维可以通过这些共轭纤维的进一步下游加工制成。
-
-
-
-
-