摘要:
The invention relates to high magnetic induction oriented silicon steel and a preparation method thereof. The oriented silicon steel comprises the following chemical elements by weight percent: 0.035-0.120% of C, 2.9-4.5% of Si, 0.05-0.20% of Mn, 0.005-0.050% of P, 0.005-0.012% of S, 0.015-0.035% of Als, 0.001-0.010% of N, 0.05-0.30% of Cr, 0.005-0.090% of Sn, not more than 0.0100% of V, not more than 0.0100% of Ti, at least one of trace elements of Sb, Bi, Nb and Mo, and the balance of Fe and other inevitable impurities, wherein Sb+Bi+Nb+Mo is 0.0015-0.0250% and (Sb/121.8+Bi/209.0+Nb/92.9+Mo/95.9)/(Ti/47.9+V/50.9) ranges from 0.1 to 15.
摘要:
The invention relates to high magnetic induction oriented silicon steel and a preparation method thereof. The oriented silicon steel comprises the following chemical elements by weight percent: 0.035-0.120% of C, 2.9-4.5% of Si, 0.05-0.20% of Mn, 0.005-0.050% of P, 0.005-0.012% of S, 0.015-0.035% of Als, 0.001-0.010% of N, 0.05-0.30% of Cr, 0.005-0.090% of Sn, not more than 0.0100% of V, not more than 0.0100% of Ti, at least one of trace elements of Sb, Bi, Ni and Mo, and the balance of Fe and other inevitable impurities, wherein Sb+Bi+Nb+Mo is 0.0015-0.0250% and (Sb/121.8+Bi/209.0+Nb/92.9+Mo/95.9)/(Ti/47.9+V/50.9) ranges from 0.1 to 15.
摘要翻译:本发明涉及高磁感应定向硅钢及其制备方法。 取向硅钢按重量百分比计含有以下化学元素:C:0.035-0.120%,Si:2.9-4.5%,Mn:0.05-0.20%,P:0.005-0.050%,S:0.005-0.012% 0.035%的Al,0.001-0.010%的N,0.05-0.30%的Cr,0.005-0.090%的Sn,不大于0.0100%的V,不大于0.0100%的Ti,Sb中的至少一种微量元素 ,Bi,Ni和Mo,余量为Fe等不可避免的杂质,其中Sb + Bi + Nb + Mo为0.0015〜0.0250%,(Sb / 121.8 + Bi / 209.0 + Nb / 92.9 + Mo / 95.9)/( Ti / 47.9 + V / 50.9)为0.1〜15。