公开(公告)号:US20180222291A1
公开(公告)日:2018-08-09
申请号:US15948067
申请日:2018-04-09
CPC分类号: B60J1/006 , C03C17/009 , C03C17/28 , C03C2217/445 , C03C2217/475 , C03C2217/48 , E05F11/38 , E05F11/385 , E05F11/445 , E05F11/535 , E05Y2600/526
摘要: A glass article which has: a glass plate having a contour shape having an upper edge and a lower edge; a functional film formed on at least one of principal surfaces of the glass plate; and a holder having a recessed portion into which the lower edge of the glass plate is fitted, wherein the functional film has a first coverage area and a second coverage area, the second coverage area being formed in a manner to cover the principal surface, the first coverage area being formed on a lower side of the second coverage area, and a maximum film thickness of the first coverage area being smaller than a maximum film thickness of the second coverage area, and the holder is provided on a lower edge side of the glass plate, within the first coverage area of functional film, via an adhesive in the recessed portion.
-
2.
公开(公告)号:US20160362332A1
公开(公告)日:2016-12-15
申请号:US15244523
申请日:2016-08-23
IPC分类号: C03C17/25 , C09D183/06 , C09D163/00 , C09D1/00 , C09D5/32
CPC分类号: C03C17/25 , C03C2217/213 , C03C2218/113 , C08G77/16 , C08G77/80 , C09D1/00 , C09D5/32 , C09D7/40 , C09D163/00 , C09D183/04 , C09D183/06 , C23C18/1212 , C23C18/1245 , C23C18/1254 , C23C18/1275 , C23C18/1283 , C25B1/00
摘要: There are provide a liquid composition for forming a silicon oxide-based cured coating film by the sol-gel method, the liquid composition having excellent storage stability and being capable of forming a coating film excellent in durability, in particular, alkali resistance even after long-term storage. A liquid composition applied on a surface of a substrate and cured by heating to form a coating film, contains: a matrix component containing a hydrolyzable silicon compound whose content is 20 to 60 mass % as a SiO2 content when silicon atoms contained in the matrix component are converted into SiO2 to the total solid content amount in the liquid composition; a functional component containing an ultraviolet absorbent and an infrared absorbent; water; and an acid thermally decomposing at 80° C. or higher and a temperature of the heating or lower, wherein a pH increases between before and after the thermal decomposition of the acid.
摘要翻译: 提供了通过溶胶 - 凝胶法形成氧化硅类固化涂膜的液体组合物,该液体组合物具有优异的储存稳定性,并且能够即使在长时间后形成耐久性,特别是耐碱性优异的涂膜 -term存储。 涂布在基材表面上并通过加热固化以形成涂膜的液体组合物包含:当基质组分中含有硅原子时,含有含量为20至60质量%的可水解硅化合物的基质组分作为SiO 2含量 在液体组合物中转化为SiO 2至总固体含量; 含有紫外线吸收剂和红外线吸收剂的功能性成分; 水; 和在80℃以上的热分解和加热温度以下的酸,其中在酸的热分解之前和之后pH增加。
-