公开(公告)号:US10815155B2
公开(公告)日:2020-10-27
申请号:US16124913
申请日:2018-09-07
Applicant: AGC CERAMICS CO., LTD.
Inventor: Kenji Matano , Nobuo Tomura
IPC: C04B35/484 , C03B5/43 , C04B35/05 , C04B35/48 , F27D1/00 , C04B35/66 , C04B35/657
Abstract: To provide a high-zirconia electrocast refractory in which occurrence of cracks in manufacture and occurrence of cracks in use as a furnace material is further reduced while maintaining extremely high corrosion resistance to molten glass. The high-zirconia electrocast refractory contains 96.7 to 98.5 mass % of ZrO2, 0.8 to 2.7 mass % of SiO2, 0 to 0.2 mass % of Na2O, 0.21 to 1 mass % of K2O, 0.1 to 0.4 mass % of Al2O3, and does not substantially contain B2O3, in terms of oxide, as a chemical composition, wherein contents of the Na2O and the K2O satisfy a relation of following Formula (1) 0.15 mass %≤CK2O/2+CNa2O≤0.6 mass % (1) where CK2O is the content of K2O and CNa2O is the content of Na2O, and each of the contents is expressed by mass % in the refractory.
-
公开(公告)号:US20190077714A1
公开(公告)日:2019-03-14
申请号:US16124913
申请日:2018-09-07
Applicant: AGC Ceramics Co., Ltd.
Inventor: Kenji Matano , Nobuo Tomura
IPC: C04B35/484 , C03B5/43
CPC classification number: C04B35/484 , C03B5/43 , C04B35/05 , C04B35/48 , C04B35/657 , C04B35/66 , C04B2235/3201 , C04B2235/3217 , C04B2235/3418 , C04B2235/6565 , C04B2235/72 , C04B2235/96 , C04B2235/9607 , C04B2235/9669 , F27D1/0006
Abstract: To provide a high-zirconia electrocast refractory in which occurrence of cracks in manufacture and occurrence of cracks in use as a furnace material is further reduced while maintaining extremely high corrosion resistance to molten glass. The high-zirconia electrocast refractory contains 96.7 to 98.5 mass % of ZrO2, 0.8 to 2.7 mass % of SiO2, 0 to 0.2 mass % of Na2O, 0.21 to 1 mass % of K2O, 0.1 to 0.4 mass % of Al2O3, and does not substantially contain B2O3, in terms of oxide, as a chemical composition, wherein contents of the Na2O and the K2O satisfy a relation of following Formula (1) 0.15 mass %≤CK2O/2+CNa2O≤0.6 mass % (1) where CK2O is the content of K2O and CNa2O is the content of Na2O, and each of the contents is expressed by mass % in the refractory.
-