Polyester-polycarbonate blends useful for extrusion blow-molding

    公开(公告)号:US07345104B2

    公开(公告)日:2008-03-18

    申请号:US10982305

    申请日:2004-11-05

    IPC分类号: C08L69/00 C08L67/02

    摘要: Blends of polycarbonate and copolyester that are capable of being extrusion blow-molded are described. The blends preferably comprise (I) about 1 to 99% by weight of a linear or branched polycarbonate and (II) about 1 to 99% by weight of a mixture of (i) about 40 to 100% by weight of a first copolyester and (ii) about 0 to 60% by weight of a second copolyester. The first copolyester preferably comprises (A) diacid residues comprising terephthalic acid residues, (B) diol residues comprising about 45 to 75 mole percent of 1,4-cyclohexanedimethanol (CHDM) residues and about 25 to 55 mole percent of ethylene glycol residues, and (C) about 0.05 to 1.0 mole percent of the residue of a trifunctional monomer. The optional second copolyester preferably comprises (A) diacid residues comprising terephthalic acid residues and (B) diol residues comprising about 52 to 90 mole percent of CHDM residues and about 10 to 48 mole percent of ethylene glycol residues. Preferably, the average amount of CHDM residues in the copolyester mixture II ranges from 52 to 75 mole percent. It has been surprisingly found that the presence of the trifunctional residues in the first copolyester can impart sufficient melt strength for the blends to be extrusion blow-molded. Containers and shaped articles made from the blends as well as a method of making the articles are also described.

    Copolyesters and blends with improved recyclability, processes for their manufacture, and articles prepared therefrom
    6.
    发明授权
    Copolyesters and blends with improved recyclability, processes for their manufacture, and articles prepared therefrom 有权
    具有改善的可回收性的共聚酯和共混物,其制造方法和由其制备的制品

    公开(公告)号:US08980389B2

    公开(公告)日:2015-03-17

    申请号:US12255237

    申请日:2008-10-21

    摘要: Described as one aspect of the invention are extrusion blow molded articles comprising at least one polyester which comprises: (a) a dicarboxylic acid component comprising: (i) about 90 to about 100 mole % of terephthalic acid residues; (ii) about 0 to about 10 mole % of aromatic and/or aliphatic dicarboxylic acid residues having up to 20 carbon atoms; and (b) a glycol component comprising: (i) about 42 to about 60 mole % ethylene glycol residues; and (ii) about 40 to about 58 mole % residues of 1,4-cyclohexanedimethanol; wherein the total mole % of the dicarboxylic acid component is 100 mole %, and wherein the total mole % of the glycol component is 100 mole %; and wherein the inherent viscosity of the polyester is from 0.50 to 1.0 dL/g as determined in 60/40 (wt/wt) phenol/tetrachloroethane at a concentration of 0.25 g/50 ml at 25° C.

    摘要翻译: 描述为本发明的一个方面的是包含至少一种聚酯的挤出吹塑制品,其包含:(a)二羧酸组分,其包含:(i)约90至约100摩尔%的对苯二甲酸残基; (ii)约0至约10摩尔%的具有至多20个碳原子的芳族和/或脂族二羧酸残基; 和(b)二元醇组分,其包含:(i)约42至约60摩尔%的乙二醇残基; 和(ii)1,4-环己烷二甲醇的约40至约58摩尔%的残余物; 其中二羧酸组分的总摩尔%为100摩尔%,其中二醇组分的总摩尔%为100摩尔%; 并且其中在25℃下浓度为0.25g / 50ml的60/40(wt / wt)苯酚/四氯乙烷中测定的聚酯的特性粘度为0.50至1.0dL / g。

    COPOLYESTERS AND BLENDS WITH IMPROVED RECYCLABILITY, PROCESSES FOR THEIR MANUFACTURE, AND ARTICLES PREPARED THEREFROM
    9.
    发明申请
    COPOLYESTERS AND BLENDS WITH IMPROVED RECYCLABILITY, PROCESSES FOR THEIR MANUFACTURE, AND ARTICLES PREPARED THEREFROM 有权
    具有改进可回收性的共聚物和共混物,其制备方法及其制备的制品

    公开(公告)号:US20090181196A1

    公开(公告)日:2009-07-16

    申请号:US12255237

    申请日:2008-10-21

    摘要: Described as one aspect of the invention are extrusion blow molded articles comprising at least one polyester which comprises: (a) a dicarboxylic acid component comprising: (i) about 90 to about 100 mole % of terephthalic acid residues; (ii) about 0 to about 10 mole % of aromatic and/or aliphatic dicarboxylic acid residues having up to 20 carbon atoms; and (b) a glycol component comprising: (i) about 42 to about 60 mole % ethylene glycol residues; and (ii) about 40 to about 58 mole % residues of 1,4-cyclohexanedimethanol; wherein the total mole % of the dicarboxylic acid component is 100 mole %, and wherein the total mole % of the glycol component is 100 mole %; and wherein the inherent viscosity of the polyester is from 0.50 to 1.0 dL/g as determined in 60/40 (wt/wt) phenol/tetrachloroethane at a concentration of 0.25 g/50 ml at 25° C.

    摘要翻译: 描述为本发明的一个方面的是包含至少一种聚酯的挤出吹塑制品,其包含:(a)二羧酸组分,其包含:(i)约90至约100摩尔%的对苯二甲酸残基; (ii)约0至约10摩尔%的具有至多20个碳原子的芳族和/或脂族二羧酸残基; 和(b)二元醇组分,其包含:(i)约42至约60摩尔%的乙二醇残基; 和(ii)1,4-环己烷二甲醇的约40至约58摩尔%的残余物; 其中二羧酸组分的总摩尔%为100摩尔%,其中二醇组分的总摩尔%为100摩尔%; 并且其中在25℃下浓度为0.25g / 50ml的60/40(wt / wt)苯酚/四氯乙烷中测定的聚酯的特性粘度为0.50至1.0dL / g。

    Polyester-polycarbonate blends useful for extrusion blow-molding
    10.
    发明授权
    Polyester-polycarbonate blends useful for extrusion blow-molding 有权
    用于挤出吹塑的聚酯 - 聚碳酸酯共混物

    公开(公告)号:US07342059B2

    公开(公告)日:2008-03-11

    申请号:US10737513

    申请日:2003-12-16

    IPC分类号: C08L69/00 C08L67/02

    摘要: Blends of polycarbonate and copolyester that are capable of being extrusion blow-molded are described. The blends preferably comprise (I) about 1 to 99% by weight of a linear or branched polycarbonate and (II) about 1 to 99% by weight of a mixture of (i) about 40 to 100% by weight of a first copolyester and (ii) about 0 to 60% by weight of a second copolyester. The first copolyester preferably comprises (A) diacid residues comprising terephthalic acid residues, (B) diol residues comprising about 45 to 75 mole percent of 1,4-cyclohexanedimethanol (CHDM) residues and about 25 to 55 mole percent of ethylene glycol residues, and (C) about 0.05 to 1.0 mole percent of the residue of a trifunctional monomer. The optional second copolyester preferably comprises (A) diacid residues comprising terephthalic acid residues and (B) diol residues comprising about 52 to 90 mole percent of CHDM residues and about 10 to 48 mole percent of ethylene glycol residues. Preferably, the average amount of CHDM residues in the copolyester mixture II ranges from 52 to 75 mole percent. It has been surprisingly found that the presence of the trifunctional residues in the first copolyester can impart sufficient melt strength for the blends to be extrusion blow-molded. Containers and shaped articles made from the blends as well as a method of making the articles are also described.

    摘要翻译: 描述了能够挤出吹塑成型的聚碳酸酯和共聚酯的共混物。 共混物优选包含(I)约1至99重量%的直链或支链聚碳酸酯和(II)约1至99重量%的(i)约40至100重量%的第一共聚酯和 (ii)约0至60重量%的第二共聚酯。 第一共聚酯优选包含(A)包含对苯二甲酸残基的二酸残基,(B)包含约45至75摩尔%的1,4-环己烷二甲醇(CHDM)残基和约25至55摩尔%乙二醇残基的二醇残基,以及 (C)约0.05〜1.0摩尔%的三官能单体残基。 任选的第二共聚酯优选包含(A)包含对苯二甲酸残基的二酸残基和包含约52至90摩尔%CHDM残基和约10至48摩尔%乙二醇残基的(B)二醇残基。 优选地,共聚酯混合物II中CHDM残基的平均量为52至75摩尔%。 已经令人惊奇地发现,第一共聚酯中三官能残基的存在可赋予共混物足够的熔体强度以进行挤出吹塑。 还描述了由共混物制成的容器和成型制品以及制造制品的方法。