    摘要: Rolled articles such as hot rolled or cold rolled and annealed sheet and/or strip include effective amounts of vanadium in low carbon steels to produce an improved bake hardenable product especially adapted for automotive use. The use of vanadium in the alloy steel chemistry controls bake hardenability, permits solution annealing at lower temperatures in its manufacturing sequence and specifies a composition range which is more easily cast within desired limits and causes less variation in final mechanical properties.

    摘要翻译: 诸如热轧或冷轧和退火的板材和/或带材的轧制制品包括有效量的低碳钢中的钒以产生特别适用于汽车应用的改进的可烘烤硬化产品。 合金钢化学中钒的使用控制烘烤淬透性,允许在其制造顺序中在较低温度下进行固溶退火,并且指定更容易在期望的范围内铸造的组成范围并且导致最终机械性能的较小变化。

    Bake hardenable vanadium containing steel and method thereof
    2.
    发明授权
    Bake hardenable vanadium containing steel and method thereof 失效
    烘烤可硬化含钒钢及其方法

    公开(公告)号:US5656102A

    公开(公告)日:1997-08-12

    申请号:US607893

    申请日:1996-02-27

    CPC分类号: C22C38/12

    摘要: Rolled articles such as hot rolled or cold rolled and annealed sheet and/or strip include effective amounts of vanadium in low carbon steels to produce an improved bake hardenable product especially adapted for automotive use. The use of vanadium in the alloy steel chemistry controls bake hardenability, permits solution annealing at lower temperatures in its manufacturing sequence and specifies a composition range which is more easily cast within desired limits and causes less variation in final mechanical properties. Controlling the vanadium to carbon ratio to maintain a value of about 10 or greater also improves aging resistance.

    摘要翻译: 诸如热轧或冷轧和退火的板材和/或带材的轧制制品包括有效量的低碳钢中的钒以产生特别适用于汽车应用的改进的可烘烤硬化产品。 合金钢化学中钒的使用控制烘烤淬透性,允许在其制造顺序中在较低温度下进行固溶退火,并且指定更容易在期望的范围内铸造的组成范围并且导致最终机械性能的较小变化。 控制钒与碳之比保持约10或更大的值也可改善耐老化性。

    Method of determining slope angles of impression walls and depths of
impressions on an embossed sheet surface
    3.
    发明授权
    Method of determining slope angles of impression walls and depths of impressions on an embossed sheet surface 失效
    确定压印壁的倾斜角度和压花片表面上的印模深度的方法

    公开(公告)号:US5780726A

    公开(公告)日:1998-07-14

    申请号:US697562

    申请日:1996-08-28

    IPC分类号: B21B1/22 B21B27/00 G01N33/20

    摘要: An embossed cold rolled metal (e.g. steel) sheet for use in manufacturing appliances and method of making same wherein the surface attributes of the embossed sheet are optimized to improve corrosion resistance of the painted product, promote uniform paint coverage of the sheet surface, reduce paint consumption, enable repainting without loss of pattern crispness, and provide consistent and aesthetically pleasing appearance of the painted sheet. The embossed sheet has a plurality of plateaus and impressions defined therein in a manner such that the arithmetic average surface roughness (Ra) of the plateaus is from about 50 to 100 microinches, the maximum impression depths over a given area are from about 0.0025 to 0.0032 inches, the impression walls define maximum slopes of from about 8-17 degrees, and there are no sharp corners or ridges at the transition points between plateaus and impressions.

    摘要翻译: 用于制造电器的压花冷轧金属(例如钢)片及其制造方法,其中压花片的表面特性被优化以改善涂漆产品的耐腐蚀性,促进片材表面的均匀涂料覆盖,减少涂料 消耗,不会损失图案的脆性,并提供一致和美观的外观。 压纹片材具有多个平台和印模,其方式使得平台的算术平均表面粗糙度(Ra)为约50至100微英寸,给定面积上的最大印模深度为约0.0025至0.0032 英寸,印象墙定义了大约8-17度的最大斜率,在平台和印象之间的过渡点没有尖角或脊。

    Embossed cold rolled steel with improved corrosion resistance,
paintability, and appearance
    4.
    发明授权
    Embossed cold rolled steel with improved corrosion resistance, paintability, and appearance 失效
    压花冷轧钢,具有改善的耐腐蚀性,可涂漆性和外观

    公开(公告)号:US5552235A

    公开(公告)日:1996-09-03

    申请号:US409219

    申请日:1995-03-23

    IPC分类号: B21B1/22 B21B27/00 B32B15/18

    摘要: An embossed cold rolled metal (e.g. steel) sheet for use in manufacturing appliances and method of making same wherein the surface attributes of the embossed sheet are optimized to improve corrosion resistance of the painted product, promote uniform paint coverage of the sheet surface, reduce paint consumption, enable repainting without loss of pattern crispness, and provide consistent and aesthetically pleasing appearance of the painted sheet. The embossed sheet has a plurality of plateaus and impressions defined therein in a manner such that the arithmetic average surface roughness (Ra) of the plateaus is from about 50 to 100 microinches, the maximum impression depths over a given area are from about 0.0025 to 0.0032 inches, the impression walls define maximum slopes of from about 8-17 degrees, and there are no sharp corners or ridges at the transition points between plateaus and impressions.

    摘要翻译: 用于制造电器的压花冷轧金属(例如钢)片及其制造方法,其中压花片的表面特性被优化以改善涂漆产品的耐腐蚀性,促进片材表面的均匀涂料覆盖,减少涂料 消耗,不会损失图案的脆性,并提供一致和美观的外观。 压纹片材具有多个平台和印模,其方式使得平台的算术平均表面粗糙度(Ra)为约50至100微英寸,给定面积上的最大印模深度为约0.0025至0.0032 英寸,印象墙定义了大约8-17度的最大斜率,在平台和印象之间的过渡点没有尖角或脊。