摘要:
The present invention relates to oxide luminescent materials activated by trivalent thulium and their preparations. The luminescent materials are the compounds with the following general formula: (RE1-xTmx)2O3, wherein a range of x is 0
摘要:
A green light-emitting glass and the method of preparing the same are provided. The components with parts by mole of the green light-emitting glass are alkali oxide 25-40, Y2O3 0.01-15, SiO2 40-70, Tb2O3 0.01-15. The method of preparing the glass includes mixing alkali salt with Y2O3, SiO2 and Tb4O7, firing the mixture at 1200° C.-1500° C. for 1-5 hours, cooling the precursor to the room temperature and annealing the precursor in a reducing atmosphere at 600° C.-1200° C. for 1-20 hours. A green light-emitting glass with good transparence, high uniformity, easily being made into big bulk and high stability is provided. The process of capsulation of parts by using the glass is simple. And a method of preparing the glass with simple process and low cost is provided.
摘要翻译:提供绿色发光玻璃及其制备方法。 具有摩尔比的绿色发光玻璃的组分是碱金属氧化物25-40,Y2O3 0.01-15,SiO2 40-70,Tb2O3 0.01-15。 制备玻璃的方法包括将碱金属盐与Y 2 O 3,SiO 2和Tb 4 O 7混合,将混合物在1200℃-1500℃下烧制1-5小时,将前体冷却至室温,并在还原 气氛在600℃-1200℃下保持1-20小时。 提供透明性好,均匀性好,容易制成大体积,高稳定性的绿色发光玻璃。 通过使用玻璃来封装部件的过程很简单。 并提供了一种以简单的工艺和低成本制备玻璃的方法。
摘要:
A silicate fluorescent material is provided. The general chemical formula of the luminescent material is Ln2SiO5:Tb, M, wherein Ln represents at least one of the elements selected from Y, Gd, La or Lu, M represents at least one of the nanoparticles selected from Ag, Au, Os, Ir, Pt, Ru, Rh or Pd, the mole ratio of Tb to Ln is greater than 0 but not greater than 0.25. The porous glass containing metal nanoparticles is prepared by introducing metal nano ions into the porous glass and extracting the uniformly dispersed metal nanoparticles from the porous glass via a chemical reduction method. A silicate fluorescent material with enhanced luminescence is obtained by substituting SiO2 which is the raw material in the process for preparing the silicate fluorescent material via the conventional high temperature solid phase sintering with the porous glass containing metal nanoparticles. The performance of the silicate fluorescent material is better and the light emitting efficiency of the silicate fluorescent material is higher compared with the conventional silicate fluorescent material.
摘要:
Disclosed is a strontium cerate luminescent material having a chemical formula of Sr2CeO4:xM and comprising the luminescent material Sr2CeO4 and metal nanoparticle M, and the preparation method thereof, where M is at least one of Ag, Au, Pt and Pd, and x is a molar ratio of M to the luminescent material Sr2CeO4 and 0
摘要:
A luminescent material and a preparation method thereof are provided. The said luminescent material is represented by the following chemical formula: Ln2−EuxSn2O7, wherein Ln is selected from one of Gd, Y and La, 0.1≦x≦1.5. The said luminescent material has good electrical performance, anti-electron bombardment and stable luminescent property. It is appropriate to be used in field emission light-emitting devices. The said preparation method has simple technique, no pollution, manageable process conditions, low preparation temperature and low equipment requirement, and is beneficial to industry production.
摘要:
A rare earth elements doping on yttrium oxide luminescent thin film containing conductive oxides and preparation methods thereof are provided. The said luminescent thin film is consisted of Y2O3:Re, Zn1-xAlxO, wherein 0
摘要翻译:提供掺杂在含氧化钇的发光薄膜上的稀土元素及其制备方法。 所述发光薄膜由Y 2 O 3:Re,Zn 1-x Al x O组成,其中0
摘要:
The present invention relates to a white light luminescent device based on purple light LED. The white light luminescent device includes a housing, a support plate, at least one purple light LED semiconductor light source, and a piece of high silica luminescent glass. The support plate is received in the housing. The at least one purple light LED semiconductor light source is positioned on the support plate. The piece of high silica luminescent glass doped with Eu ions is opposite to the purple light LED semiconductor light source. One surface of the high silica luminescent glass away from the purple light LED semiconductor light source is coated with a phosphor layer formed with a selection from a mixture of yellow phosphor and red phosphor, a mixture of green phosphor and red phosphor, and yellow phosphor.
摘要:
A luminescent glass comprises glass matrix. Said glass matrix comprises a glass part and a complex part of glass and fluorescent powder, which is embedded in said glass part. Said complex part of glass and fluorescent powder comprises glass material and fluorescent powder dispersed in said glass material. Said fluorescent powder is long after-glow fluorescent powder. A method for producing the luminescent glass and a luminescent device comprising the luminescent glass are also provided. The luminescent glass and the luminescent device have good luminescence reliability, high luminescence stability and long service life. The method can be carried out at a relatively low temperature.
摘要:
A semiconductor light emitting package includes a substrate, an encapsulating material, a semiconductor light emitting chip disposed on the substrate, wires; and an integrated glass-fluorescent powder compound light-emitting structure. The encapsulating material and the integrated glass-fluorescent powder compound light-emitting structure are packaged on the semiconductor light emitting chip, the integrated glass-fluorescent powder compound light-emitting structure is coated on the encapsulating material. The semiconductor light-emitting package has a large light-emitting area, high uniformity which can effectively avoid “halo” phenomenon, and long working life. The present invention also relates to a method for manufacturing semiconductor light emitting package, which can be implemented at low temperature and improve the reliability and the stability of the light-emitting property of the compound light-emitting structure.
摘要:
A luminescent element includes a luminescent glass and a metal layer with a metal microstructure formed on a surface of the luminescent glass; wherein the luminescent glass has a chemical composition: bY2O3.cAl2O3.dB2O3.yTb2O3, wherein bY2O3.cAl2O3.dB2O3.yTb2O3. A preparation method of a luminescent element and a luminescence method are also provided. The luminescent element has good luminescence homogeneity, high luminescence efficiency, good luminescence stability and simple structure, and can be used in luminescent device with ultrahigh brightness.